Crystallization and Densification of Nano-Size Amorphous Cordierite Powder Prepared by a PVA Solution-Polymerization Route

A homogeneous and stable amorphous‐type cordierite (2MgO2Al2O35SiO2) powder was prepared by a solution‐polymerization route employing a Pechini resin or a poly(vinyl alcohol) (PVA) solution as the polymeric carrier. After calcination at 800°C for 1 h under atmospheric conditions, the bulky precursor...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of the American Ceramic Society 1998-10, Vol.81 (10), p.2605-2612
Hauptverfasser: Lee, Sang-Jin, Kriven, Waltraud M.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A homogeneous and stable amorphous‐type cordierite (2MgO2Al2O35SiO2) powder was prepared by a solution‐polymerization route employing a Pechini resin or a poly(vinyl alcohol) (PVA) solution as the polymeric carrier. After calcination at 800°C for 1 h under atmospheric conditions, the bulky precursor changed into a very soft and porous powder. A 30 nm size, amorphous‐type cordierite powder was prepared by attrition milling the calcined powder, which was made using a PVA precursor solution. The nano‐size powder, which had a high specific surface area of 181 m2/g, was obtained after milling for
ISSN:0002-7820
1551-2916
DOI:10.1111/j.1151-2916.1998.tb02667.x