Nickel sulfide hollow whisker formation
Hollow, high-aspect-ratio nickel sulfide whiskers were formed during aqueous corrosion experiments at 250°C by the U. S. Department of Energy. The whiskers grew radially from Teflon thread at the waterline in acidic sodium sulfate solutions containing chloride additions. The hollow morphology is con...
Gespeichert in:
Veröffentlicht in: | Materials Characterization 1997-02, Vol.38 (2), p.67-73 |
---|---|
Hauptverfasser: | , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Hollow, high-aspect-ratio nickel sulfide whiskers were formed during aqueous corrosion experiments at 250°C by the U. S. Department of Energy. The whiskers grew radially from Teflon thread at the waterline in acidic sodium sulfate solutions containing chloride additions. The hollow morphology is consistent with that reported for the mineral millerite found in nature in hematite cavities. The data suggest that iron and chloride impurities are necessary for the observed whisker structure. |
---|---|
ISSN: | 1044-5803 1873-4189 |
DOI: | 10.1016/S1044-5803(97)80025-3 |