Reaction synthesis and mechanical properties of TiB2-AlN-SiC composites

TiB2-AlN-SiC (TAS) ternary composites were prepared by reactive hot pressing at 2000 C for 60 min in an Ar atmosphere using TiH2, Si, Al, B4C, BN and C as raw powders. The distributions of Al and Si were not homogeneous, which shows that, to obtain a homogeneous solid solution of AlN and SiC in the...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of the European Ceramic Society 1999-01, Vol.19 (3), p.293-298
Hauptverfasser: YUE, X. M, ZHANG, G. J, WANG, Y. M
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:TiB2-AlN-SiC (TAS) ternary composites were prepared by reactive hot pressing at 2000 C for 60 min in an Ar atmosphere using TiH2, Si, Al, B4C, BN and C as raw powders. The distributions of Al and Si were not homogeneous, which shows that, to obtain a homogeneous solid solution of AlN and SiC in the composites, temperatures higher than 2000 C or time duration longer than 60 min are needed. Fracture toughnesses of about 6.35 MPa.m1/2 and 6.49 MPa.m1/2 were obtained in samples with equal molar contents of AlN and SiC. The highest fracture strength (470 MPa) was obtained in a sample, in which the volume ratio of TiB2/(AlN + SiC) was the nearest to 1 and there was finer co-continuous microstructure. 20 refs.
ISSN:0955-2219
1873-619X
DOI:10.1016/s0955-2219(98)00150-2