Experimental set-up for thermopower and resistivity measurements at 100-1300 K

In this paper we describe an experimental set-up for simultaneous measurements of thermopower and electrical resistivity at temperatures from 100K to 1300K. Optimal configuration of electrodes and original mechanical contacts of thermocouples, current leads and potential probes with the sample make...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Measurement science & technology 2001-03, Vol.12 (3), p.264-272
Hauptverfasser: Burkov, A T, Heinrich, A, Konstantinov, P P, Nakama, T, Yagasaki, K
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 272
container_issue 3
container_start_page 264
container_title Measurement science & technology
container_volume 12
creator Burkov, A T
Heinrich, A
Konstantinov, P P
Nakama, T
Yagasaki, K
description In this paper we describe an experimental set-up for simultaneous measurements of thermopower and electrical resistivity at temperatures from 100K to 1300K. Optimal configuration of electrodes and original mechanical contacts of thermocouples, current leads and potential probes with the sample make it possible to measure a large variety of materials and result in greater flexibility with respect to the sample form and dimensions. Both bulk and thin film samples with resistances in the range from 0 Omega up to 200 k Omega (1 G Omega in case of the resistivity measurement) can be investigated. Precision and high reliability of the system have been proven during more than three years of use. The resistivity and thermopower of pure Pb, Cu and Ni, and a Cr-Si thin film composite are presented as test materials to demonstrate the possibilities and accuracy of this experimental set-up.
doi_str_mv 10.1088/0957-0233/12/3/304
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_27041011</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>27041011</sourcerecordid><originalsourceid>FETCH-LOGICAL-c414t-817cecf16d2bbba634c4277afa8459b51644b30bc6f077b04b56a9681935dd793</originalsourceid><addsrcrecordid>eNp9kL1OwzAURi0EEqXwAkyekBhM740dOxlRVX5EBQvMlp04Iihpgu0AfXsSFXWpxHSXcz7pHkIuEW4QsmwBeaoYJJwvMFnwBQdxRGbIJTKZAh6T2R44JWchfACAgjyfkefVT-983bpNNA0NLrKhp1XnaXx3vu367tt5ajYl9S7UIdZfddzS1pkweDdJgZpIEYAhB6BP5-SkMk1wF393Tt7uVq_LB7Z-uX9c3q5ZIVBElqEqXFGhLBNrrZFcFCJRylQmE2luU5RCWA62kBUoZUHYVJpcZpjztCxVzufkarfb--5zcCHqtg6Faxqzcd0QdKJAICCOYLIDC9-F4F2l-_Fb47caQU_p9FRGT2U0JprrMd0oXe-kuuv3_CGn-7IaWXbI_rP9C5rYenM</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>27041011</pqid></control><display><type>article</type><title>Experimental set-up for thermopower and resistivity measurements at 100-1300 K</title><source>IOP Publishing Journals</source><source>Institute of Physics (IOP) Journals - HEAL-Link</source><creator>Burkov, A T ; Heinrich, A ; Konstantinov, P P ; Nakama, T ; Yagasaki, K</creator><creatorcontrib>Burkov, A T ; Heinrich, A ; Konstantinov, P P ; Nakama, T ; Yagasaki, K</creatorcontrib><description>In this paper we describe an experimental set-up for simultaneous measurements of thermopower and electrical resistivity at temperatures from 100K to 1300K. Optimal configuration of electrodes and original mechanical contacts of thermocouples, current leads and potential probes with the sample make it possible to measure a large variety of materials and result in greater flexibility with respect to the sample form and dimensions. Both bulk and thin film samples with resistances in the range from 0 Omega up to 200 k Omega (1 G Omega in case of the resistivity measurement) can be investigated. Precision and high reliability of the system have been proven during more than three years of use. The resistivity and thermopower of pure Pb, Cu and Ni, and a Cr-Si thin film composite are presented as test materials to demonstrate the possibilities and accuracy of this experimental set-up.</description><identifier>ISSN: 0957-0233</identifier><identifier>EISSN: 1361-6501</identifier><identifier>DOI: 10.1088/0957-0233/12/3/304</identifier><language>eng</language><publisher>IOP Publishing</publisher><ispartof>Measurement science &amp; technology, 2001-03, Vol.12 (3), p.264-272</ispartof><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c414t-817cecf16d2bbba634c4277afa8459b51644b30bc6f077b04b56a9681935dd793</citedby><cites>FETCH-LOGICAL-c414t-817cecf16d2bbba634c4277afa8459b51644b30bc6f077b04b56a9681935dd793</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktopdf>$$Uhttps://iopscience.iop.org/article/10.1088/0957-0233/12/3/304/pdf$$EPDF$$P50$$Giop$$H</linktopdf><link.rule.ids>314,780,784,27924,27925,53830,53910</link.rule.ids></links><search><creatorcontrib>Burkov, A T</creatorcontrib><creatorcontrib>Heinrich, A</creatorcontrib><creatorcontrib>Konstantinov, P P</creatorcontrib><creatorcontrib>Nakama, T</creatorcontrib><creatorcontrib>Yagasaki, K</creatorcontrib><title>Experimental set-up for thermopower and resistivity measurements at 100-1300 K</title><title>Measurement science &amp; technology</title><description>In this paper we describe an experimental set-up for simultaneous measurements of thermopower and electrical resistivity at temperatures from 100K to 1300K. Optimal configuration of electrodes and original mechanical contacts of thermocouples, current leads and potential probes with the sample make it possible to measure a large variety of materials and result in greater flexibility with respect to the sample form and dimensions. Both bulk and thin film samples with resistances in the range from 0 Omega up to 200 k Omega (1 G Omega in case of the resistivity measurement) can be investigated. Precision and high reliability of the system have been proven during more than three years of use. The resistivity and thermopower of pure Pb, Cu and Ni, and a Cr-Si thin film composite are presented as test materials to demonstrate the possibilities and accuracy of this experimental set-up.</description><issn>0957-0233</issn><issn>1361-6501</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2001</creationdate><recordtype>article</recordtype><recordid>eNp9kL1OwzAURi0EEqXwAkyekBhM740dOxlRVX5EBQvMlp04Iihpgu0AfXsSFXWpxHSXcz7pHkIuEW4QsmwBeaoYJJwvMFnwBQdxRGbIJTKZAh6T2R44JWchfACAgjyfkefVT-983bpNNA0NLrKhp1XnaXx3vu367tt5ajYl9S7UIdZfddzS1pkweDdJgZpIEYAhB6BP5-SkMk1wF393Tt7uVq_LB7Z-uX9c3q5ZIVBElqEqXFGhLBNrrZFcFCJRylQmE2luU5RCWA62kBUoZUHYVJpcZpjztCxVzufkarfb--5zcCHqtg6Faxqzcd0QdKJAICCOYLIDC9-F4F2l-_Fb47caQU_p9FRGT2U0JprrMd0oXe-kuuv3_CGn-7IaWXbI_rP9C5rYenM</recordid><startdate>20010301</startdate><enddate>20010301</enddate><creator>Burkov, A T</creator><creator>Heinrich, A</creator><creator>Konstantinov, P P</creator><creator>Nakama, T</creator><creator>Yagasaki, K</creator><general>IOP Publishing</general><scope>AAYXX</scope><scope>CITATION</scope><scope>8BQ</scope><scope>8FD</scope><scope>F28</scope><scope>FR3</scope><scope>H8D</scope><scope>JG9</scope><scope>L7M</scope></search><sort><creationdate>20010301</creationdate><title>Experimental set-up for thermopower and resistivity measurements at 100-1300 K</title><author>Burkov, A T ; Heinrich, A ; Konstantinov, P P ; Nakama, T ; Yagasaki, K</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c414t-817cecf16d2bbba634c4277afa8459b51644b30bc6f077b04b56a9681935dd793</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2001</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Burkov, A T</creatorcontrib><creatorcontrib>Heinrich, A</creatorcontrib><creatorcontrib>Konstantinov, P P</creatorcontrib><creatorcontrib>Nakama, T</creatorcontrib><creatorcontrib>Yagasaki, K</creatorcontrib><collection>CrossRef</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>ANTE: Abstracts in New Technology &amp; Engineering</collection><collection>Engineering Research Database</collection><collection>Aerospace Database</collection><collection>Materials Research Database</collection><collection>Advanced Technologies Database with Aerospace</collection><jtitle>Measurement science &amp; technology</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Burkov, A T</au><au>Heinrich, A</au><au>Konstantinov, P P</au><au>Nakama, T</au><au>Yagasaki, K</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Experimental set-up for thermopower and resistivity measurements at 100-1300 K</atitle><jtitle>Measurement science &amp; technology</jtitle><date>2001-03-01</date><risdate>2001</risdate><volume>12</volume><issue>3</issue><spage>264</spage><epage>272</epage><pages>264-272</pages><issn>0957-0233</issn><eissn>1361-6501</eissn><abstract>In this paper we describe an experimental set-up for simultaneous measurements of thermopower and electrical resistivity at temperatures from 100K to 1300K. Optimal configuration of electrodes and original mechanical contacts of thermocouples, current leads and potential probes with the sample make it possible to measure a large variety of materials and result in greater flexibility with respect to the sample form and dimensions. Both bulk and thin film samples with resistances in the range from 0 Omega up to 200 k Omega (1 G Omega in case of the resistivity measurement) can be investigated. Precision and high reliability of the system have been proven during more than three years of use. The resistivity and thermopower of pure Pb, Cu and Ni, and a Cr-Si thin film composite are presented as test materials to demonstrate the possibilities and accuracy of this experimental set-up.</abstract><pub>IOP Publishing</pub><doi>10.1088/0957-0233/12/3/304</doi><tpages>9</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0957-0233
ispartof Measurement science & technology, 2001-03, Vol.12 (3), p.264-272
issn 0957-0233
1361-6501
language eng
recordid cdi_proquest_miscellaneous_27041011
source IOP Publishing Journals; Institute of Physics (IOP) Journals - HEAL-Link
title Experimental set-up for thermopower and resistivity measurements at 100-1300 K
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-20T06%3A10%3A40IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Experimental%20set-up%20for%20thermopower%20and%20resistivity%20measurements%20at%20100-1300%20K&rft.jtitle=Measurement%20science%20&%20technology&rft.au=Burkov,%20A%20T&rft.date=2001-03-01&rft.volume=12&rft.issue=3&rft.spage=264&rft.epage=272&rft.pages=264-272&rft.issn=0957-0233&rft.eissn=1361-6501&rft_id=info:doi/10.1088/0957-0233/12/3/304&rft_dat=%3Cproquest_cross%3E27041011%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=27041011&rft_id=info:pmid/&rfr_iscdi=true