The autoacceleration of polypropylene thermo-oxidation in reduced coordinates: effect of the oxidation temperature and of polyolefin structure

Polypropylene samples ranging from highly isotactic (100% by FTIR) to fairly isotactic (76.6% by FTIR) have been thermo-oxidised in the temperature interval 80–150°C and the chemiluminescence emission along the induction and autoacceleration stages has been recorded. Of these oxidation curves, some...