Hydrothermal synthesis and characterisation of BaTiO3 fine powders : precursors, polymorphism and properties

The influence of TiO2 (anatase) and H2TiO3 (beta-titanic acid) precursors on the purity and particle size of BaTiO3 powders prepared via hydrothermal synthesis is discussed. Amorphous H2TiO3 was found to be an excellent Ti-precursor material and offers several advantages over crystalline anatase. Ph...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of material chemistry 1999, Vol.9 (1), p.83-91
Hauptverfasser: CLARK, L. J, TAKEUCHI, T, OHTORI, N, SINCLAIR, D. C
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 91
container_issue 1
container_start_page 83
container_title Journal of material chemistry
container_volume 9
creator CLARK, L. J
TAKEUCHI, T
OHTORI, N
SINCLAIR, D. C
description The influence of TiO2 (anatase) and H2TiO3 (beta-titanic acid) precursors on the purity and particle size of BaTiO3 powders prepared via hydrothermal synthesis is discussed. Amorphous H2TiO3 was found to be an excellent Ti-precursor material and offers several advantages over crystalline anatase. Phase pure powders which have small particle sizes (about 40-80 nm) and narrow size distributions can be prepared at 180 C after 24 h using H2TiO3 as a precursor material. Although the initial reaction is very fast, about 90% yield after 8-10 h, extended reaction periods at 180 C are required in order to drive the reaction to completion. Lowering the temperature from 180 to 85 C produces powders with even smaller particle sizes; however, very long reaction periods are required, e.g. over 72 h, to ensure complete reaction. Raman spectra of as-prepared and heat treated (1000 C) powders with average particle sizes as small as about 20-40 nm indicate asymmetry within the TiO6 octahedra of the BaTiO3 lattice. These results contradict the widely cited "critical" particle size theory for the stabilisation of the cubic polymorph, at least for sizes greater than about 20-40 nm. As-prepared powders contain many defects, primarily in the form of lattice OH- ions. Preliminary ac impedance spectroscopy data on samples heat treated to remove lattice OH- ions show these materials to be modest proton conductors. 54 refs.
doi_str_mv 10.1039/a805756g
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_26977954</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>26977954</sourcerecordid><originalsourceid>FETCH-LOGICAL-c305t-70b78ba39617326cadfc113a0e7e6be9dbadf6aa964a9e5e2d9f196bcbb99133</originalsourceid><addsrcrecordid>eNpFkE1LxDAURYMoOI6CPyELERdWk0mTTNyp-AWCm9mX1_TVibRNzesg_fdWZ8TVu1wO58Fl7FSKKymUu4al0Fab9z02k8rkmdZC7rOZcNplLl8sD9kR0YcQUlqjZ6x5HqsUhzWmFhpOYzdFCsShq7hfQwI_YAoEQ4gdjzW_g1V4U7wOHfI-flWYiN_wPqHfJIqJLqe2GduY-nWg9lfTp9hjGgLSMTuooSE82d05Wz0-rO6fs9e3p5f729fMK6GHzIrSLktQzkirFsZDVXspFQi0aEp0VTk1BsCZHBxqXFSuls6Uviydk0rN2flWO33-3CANRRvIY9NAh3FDxcI4a53OJ_BiC_oUiRLWRZ9CC2kspCh-1iz-1pzQs50TyENTJ-h8oH_eWLnMrfoGn6x3Bw</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>26977954</pqid></control><display><type>article</type><title>Hydrothermal synthesis and characterisation of BaTiO3 fine powders : precursors, polymorphism and properties</title><source>Royal Society of Chemistry Journals Archive (1841-2007)</source><source>Royal Society Of Chemistry Journals 2008-</source><creator>CLARK, L. J ; TAKEUCHI, T ; OHTORI, N ; SINCLAIR, D. C</creator><contributor>WCA</contributor><creatorcontrib>CLARK, L. J ; TAKEUCHI, T ; OHTORI, N ; SINCLAIR, D. C ; WCA</creatorcontrib><description>The influence of TiO2 (anatase) and H2TiO3 (beta-titanic acid) precursors on the purity and particle size of BaTiO3 powders prepared via hydrothermal synthesis is discussed. Amorphous H2TiO3 was found to be an excellent Ti-precursor material and offers several advantages over crystalline anatase. Phase pure powders which have small particle sizes (about 40-80 nm) and narrow size distributions can be prepared at 180 C after 24 h using H2TiO3 as a precursor material. Although the initial reaction is very fast, about 90% yield after 8-10 h, extended reaction periods at 180 C are required in order to drive the reaction to completion. Lowering the temperature from 180 to 85 C produces powders with even smaller particle sizes; however, very long reaction periods are required, e.g. over 72 h, to ensure complete reaction. Raman spectra of as-prepared and heat treated (1000 C) powders with average particle sizes as small as about 20-40 nm indicate asymmetry within the TiO6 octahedra of the BaTiO3 lattice. These results contradict the widely cited "critical" particle size theory for the stabilisation of the cubic polymorph, at least for sizes greater than about 20-40 nm. As-prepared powders contain many defects, primarily in the form of lattice OH- ions. Preliminary ac impedance spectroscopy data on samples heat treated to remove lattice OH- ions show these materials to be modest proton conductors. 54 refs.</description><identifier>ISSN: 0959-9428</identifier><identifier>EISSN: 1364-5501</identifier><identifier>DOI: 10.1039/a805756g</identifier><language>eng</language><publisher>Cambridge: Royal Society of Chemistry</publisher><subject>Chemistry ; Colloidal state and disperse state ; Disperse systems ; Exact sciences and technology ; General and physical chemistry ; Powders</subject><ispartof>Journal of material chemistry, 1999, Vol.9 (1), p.83-91</ispartof><rights>1999 INIST-CNRS</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c305t-70b78ba39617326cadfc113a0e7e6be9dbadf6aa964a9e5e2d9f196bcbb99133</citedby></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>309,310,314,776,780,785,786,2818,4010,4036,4037,23909,23910,25118,27900,27901,27902</link.rule.ids><backlink>$$Uhttp://pascal-francis.inist.fr/vibad/index.php?action=getRecordDetail&amp;idt=1671847$$DView record in Pascal Francis$$Hfree_for_read</backlink></links><search><contributor>WCA</contributor><creatorcontrib>CLARK, L. J</creatorcontrib><creatorcontrib>TAKEUCHI, T</creatorcontrib><creatorcontrib>OHTORI, N</creatorcontrib><creatorcontrib>SINCLAIR, D. C</creatorcontrib><title>Hydrothermal synthesis and characterisation of BaTiO3 fine powders : precursors, polymorphism and properties</title><title>Journal of material chemistry</title><description>The influence of TiO2 (anatase) and H2TiO3 (beta-titanic acid) precursors on the purity and particle size of BaTiO3 powders prepared via hydrothermal synthesis is discussed. Amorphous H2TiO3 was found to be an excellent Ti-precursor material and offers several advantages over crystalline anatase. Phase pure powders which have small particle sizes (about 40-80 nm) and narrow size distributions can be prepared at 180 C after 24 h using H2TiO3 as a precursor material. Although the initial reaction is very fast, about 90% yield after 8-10 h, extended reaction periods at 180 C are required in order to drive the reaction to completion. Lowering the temperature from 180 to 85 C produces powders with even smaller particle sizes; however, very long reaction periods are required, e.g. over 72 h, to ensure complete reaction. Raman spectra of as-prepared and heat treated (1000 C) powders with average particle sizes as small as about 20-40 nm indicate asymmetry within the TiO6 octahedra of the BaTiO3 lattice. These results contradict the widely cited "critical" particle size theory for the stabilisation of the cubic polymorph, at least for sizes greater than about 20-40 nm. As-prepared powders contain many defects, primarily in the form of lattice OH- ions. Preliminary ac impedance spectroscopy data on samples heat treated to remove lattice OH- ions show these materials to be modest proton conductors. 54 refs.</description><subject>Chemistry</subject><subject>Colloidal state and disperse state</subject><subject>Disperse systems</subject><subject>Exact sciences and technology</subject><subject>General and physical chemistry</subject><subject>Powders</subject><issn>0959-9428</issn><issn>1364-5501</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>1999</creationdate><recordtype>article</recordtype><recordid>eNpFkE1LxDAURYMoOI6CPyELERdWk0mTTNyp-AWCm9mX1_TVibRNzesg_fdWZ8TVu1wO58Fl7FSKKymUu4al0Fab9z02k8rkmdZC7rOZcNplLl8sD9kR0YcQUlqjZ6x5HqsUhzWmFhpOYzdFCsShq7hfQwI_YAoEQ4gdjzW_g1V4U7wOHfI-flWYiN_wPqHfJIqJLqe2GduY-nWg9lfTp9hjGgLSMTuooSE82d05Wz0-rO6fs9e3p5f729fMK6GHzIrSLktQzkirFsZDVXspFQi0aEp0VTk1BsCZHBxqXFSuls6Uviydk0rN2flWO33-3CANRRvIY9NAh3FDxcI4a53OJ_BiC_oUiRLWRZ9CC2kspCh-1iz-1pzQs50TyENTJ-h8oH_eWLnMrfoGn6x3Bw</recordid><startdate>1999</startdate><enddate>1999</enddate><creator>CLARK, L. J</creator><creator>TAKEUCHI, T</creator><creator>OHTORI, N</creator><creator>SINCLAIR, D. C</creator><general>Royal Society of Chemistry</general><scope>IQODW</scope><scope>AAYXX</scope><scope>CITATION</scope><scope>7QQ</scope><scope>8FD</scope><scope>JG9</scope></search><sort><creationdate>1999</creationdate><title>Hydrothermal synthesis and characterisation of BaTiO3 fine powders : precursors, polymorphism and properties</title><author>CLARK, L. J ; TAKEUCHI, T ; OHTORI, N ; SINCLAIR, D. C</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c305t-70b78ba39617326cadfc113a0e7e6be9dbadf6aa964a9e5e2d9f196bcbb99133</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>1999</creationdate><topic>Chemistry</topic><topic>Colloidal state and disperse state</topic><topic>Disperse systems</topic><topic>Exact sciences and technology</topic><topic>General and physical chemistry</topic><topic>Powders</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>CLARK, L. J</creatorcontrib><creatorcontrib>TAKEUCHI, T</creatorcontrib><creatorcontrib>OHTORI, N</creatorcontrib><creatorcontrib>SINCLAIR, D. C</creatorcontrib><collection>Pascal-Francis</collection><collection>CrossRef</collection><collection>Ceramic Abstracts</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><jtitle>Journal of material chemistry</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>CLARK, L. J</au><au>TAKEUCHI, T</au><au>OHTORI, N</au><au>SINCLAIR, D. C</au><au>WCA</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Hydrothermal synthesis and characterisation of BaTiO3 fine powders : precursors, polymorphism and properties</atitle><jtitle>Journal of material chemistry</jtitle><date>1999</date><risdate>1999</risdate><volume>9</volume><issue>1</issue><spage>83</spage><epage>91</epage><pages>83-91</pages><issn>0959-9428</issn><eissn>1364-5501</eissn><abstract>The influence of TiO2 (anatase) and H2TiO3 (beta-titanic acid) precursors on the purity and particle size of BaTiO3 powders prepared via hydrothermal synthesis is discussed. Amorphous H2TiO3 was found to be an excellent Ti-precursor material and offers several advantages over crystalline anatase. Phase pure powders which have small particle sizes (about 40-80 nm) and narrow size distributions can be prepared at 180 C after 24 h using H2TiO3 as a precursor material. Although the initial reaction is very fast, about 90% yield after 8-10 h, extended reaction periods at 180 C are required in order to drive the reaction to completion. Lowering the temperature from 180 to 85 C produces powders with even smaller particle sizes; however, very long reaction periods are required, e.g. over 72 h, to ensure complete reaction. Raman spectra of as-prepared and heat treated (1000 C) powders with average particle sizes as small as about 20-40 nm indicate asymmetry within the TiO6 octahedra of the BaTiO3 lattice. These results contradict the widely cited "critical" particle size theory for the stabilisation of the cubic polymorph, at least for sizes greater than about 20-40 nm. As-prepared powders contain many defects, primarily in the form of lattice OH- ions. Preliminary ac impedance spectroscopy data on samples heat treated to remove lattice OH- ions show these materials to be modest proton conductors. 54 refs.</abstract><cop>Cambridge</cop><pub>Royal Society of Chemistry</pub><doi>10.1039/a805756g</doi><tpages>9</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0959-9428
ispartof Journal of material chemistry, 1999, Vol.9 (1), p.83-91
issn 0959-9428
1364-5501
language eng
recordid cdi_proquest_miscellaneous_26977954
source Royal Society of Chemistry Journals Archive (1841-2007); Royal Society Of Chemistry Journals 2008-
subjects Chemistry
Colloidal state and disperse state
Disperse systems
Exact sciences and technology
General and physical chemistry
Powders
title Hydrothermal synthesis and characterisation of BaTiO3 fine powders : precursors, polymorphism and properties
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-02T05%3A19%3A22IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Hydrothermal%20synthesis%20and%20characterisation%20of%20BaTiO3%20fine%20powders%20:%20precursors,%20polymorphism%20and%20properties&rft.jtitle=Journal%20of%20material%20chemistry&rft.au=CLARK,%20L.%20J&rft.date=1999&rft.volume=9&rft.issue=1&rft.spage=83&rft.epage=91&rft.pages=83-91&rft.issn=0959-9428&rft.eissn=1364-5501&rft_id=info:doi/10.1039/a805756g&rft_dat=%3Cproquest_cross%3E26977954%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=26977954&rft_id=info:pmid/&rfr_iscdi=true