Processing and mechanical properties of a molybdenum silicide with the composition Mo–12Si–8.5B (at.%)
Alloys with the nominal composition Mo–12Si–8.5B (at.%) were prepared by arc-melting or powder-metallurgical processing. Cast and annealed alloys consisted of approximately 38 vol.% α-Mo in a brittle matrix of 32 vol.% Mo 3Si and 30 vol.% Mo 5SiB 2. Their flexure strengths were approximately 500 MPa...