Formation Mechanism of Sliver-type Surface Defect with Oxide Scale on Sheet and Coil

Laboratory rolling test of continuously cast steel slab with artificial defects was conducted to determine the origin of sliver-type surface defects with oxide scale on sheet and coil. The results obtained are summarized as follows: (1) The surface crack and pinhole could be the origins of sliver-ty...