Bending Strength of Wetly and Dryly Ground Y-TZP

Specimens of tetragonal zirconia containing 3mol% Y2O3 were ground wetly and dryly with a grinding wheel of grain size 200/230. The residual stress and the monoclinic content were measured by the X-ray diffraction method. The monoclinic content on the surface ground wetly with enough coolant was rai...