Interfacial effects in carbon-epoxies: Part 3 Toughness with short fibres
The work of fracture has been measured, using the Izod test, for short-fibre laminates. The fibres were 2 mm long and in one series of experiments were aligned, and in a second series of experiments they were random in the plane of the laminate. The work of fracture increased monotonically with incr...
Gespeichert in:
Veröffentlicht in: | Journal of materials science 1986-05, Vol.21 (5), p.1642-1646 |
---|---|