Calcium phosphate cement to prepare Sr-containing biomaterials

A new route, based on the use of ionic calcium phosphate cements, has been developed to synthesize calcium strontium hydroxyapatite. Cements were prepared from tetracalcium phosphate, alpha -tricalcium phosphate, phosphoric acid, strontium nitrate and water and were then mixed and shaped. Cements wi...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Key engineering materials 2001-01, Vol.192-195, p.235-238
Hauptverfasser: Leroux, L, Freche, M, Lacout, J L
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 238
container_issue
container_start_page 235
container_title Key engineering materials
container_volume 192-195
creator Leroux, L
Freche, M
Lacout, J L
description A new route, based on the use of ionic calcium phosphate cements, has been developed to synthesize calcium strontium hydroxyapatite. Cements were prepared from tetracalcium phosphate, alpha -tricalcium phosphate, phosphoric acid, strontium nitrate and water and were then mixed and shaped. Cements with various amounts of strontium (0 to 4.3 wt%) were prepared. All the materials obtained were coherent and solid. Mixed hydroxyapatite was obtained at low temperatures. Mixed calcium strontium apatite was obtained after heating. This original method can be of interest for the preparation of biomaterials because strontium plays a part in the mineralisation of bone. The steady release of strontium was studied and can lead to a better osteointegration of the biomaterial.
format Article
fullrecord <record><control><sourceid>proquest</sourceid><recordid>TN_cdi_proquest_miscellaneous_21457901</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>526449</sourcerecordid><originalsourceid>FETCH-LOGICAL-p99t-e2ee7def2f0f458c7c4b4c6ddb77d50316c4be1272959af40975d1e29991b1603</originalsourceid><addsrcrecordid>eNotj81qxCAYRV20MNNp38FVd4IajXFTKKF_MNBFZz8Y_ZyxJGrVvH8D7erA5XK49wbtGWUd0QPvd-iu1m9KOzYwuUdPo5ltWBecr6nmq2mALSwQG24J5wLZFMBfhdgUmwkxxAueQlq2Xglmrvfo1m-Ah38e0On15TS-k-Pn28f4fCRZ60aAAygHnnvqhRyssmIStnduUsrJbUq_BcC44lpq4wXVSjoGXGvNJtbT7oAe_7S5pJ8VajsvoVqYZxMhrfXMmZBKbxd_AY-IRYE</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>21457901</pqid></control><display><type>article</type><title>Calcium phosphate cement to prepare Sr-containing biomaterials</title><source>Scientific.net Journals</source><creator>Leroux, L ; Freche, M ; Lacout, J L</creator><creatorcontrib>Leroux, L ; Freche, M ; Lacout, J L</creatorcontrib><description>A new route, based on the use of ionic calcium phosphate cements, has been developed to synthesize calcium strontium hydroxyapatite. Cements were prepared from tetracalcium phosphate, alpha -tricalcium phosphate, phosphoric acid, strontium nitrate and water and were then mixed and shaped. Cements with various amounts of strontium (0 to 4.3 wt%) were prepared. All the materials obtained were coherent and solid. Mixed hydroxyapatite was obtained at low temperatures. Mixed calcium strontium apatite was obtained after heating. This original method can be of interest for the preparation of biomaterials because strontium plays a part in the mineralisation of bone. The steady release of strontium was studied and can lead to a better osteointegration of the biomaterial.</description><identifier>ISSN: 1013-9826</identifier><language>eng</language><subject>Biomaterials ; Bone ; Heating ; Hydroxyapatite ; Infrared spectroscopy ; Nitrates ; Phosphoric acid ; Strontium ; Synthesis (chemical) ; Water</subject><ispartof>Key engineering materials, 2001-01, Vol.192-195, p.235-238</ispartof><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,776,780</link.rule.ids></links><search><creatorcontrib>Leroux, L</creatorcontrib><creatorcontrib>Freche, M</creatorcontrib><creatorcontrib>Lacout, J L</creatorcontrib><title>Calcium phosphate cement to prepare Sr-containing biomaterials</title><title>Key engineering materials</title><description>A new route, based on the use of ionic calcium phosphate cements, has been developed to synthesize calcium strontium hydroxyapatite. Cements were prepared from tetracalcium phosphate, alpha -tricalcium phosphate, phosphoric acid, strontium nitrate and water and were then mixed and shaped. Cements with various amounts of strontium (0 to 4.3 wt%) were prepared. All the materials obtained were coherent and solid. Mixed hydroxyapatite was obtained at low temperatures. Mixed calcium strontium apatite was obtained after heating. This original method can be of interest for the preparation of biomaterials because strontium plays a part in the mineralisation of bone. The steady release of strontium was studied and can lead to a better osteointegration of the biomaterial.</description><subject>Biomaterials</subject><subject>Bone</subject><subject>Heating</subject><subject>Hydroxyapatite</subject><subject>Infrared spectroscopy</subject><subject>Nitrates</subject><subject>Phosphoric acid</subject><subject>Strontium</subject><subject>Synthesis (chemical)</subject><subject>Water</subject><issn>1013-9826</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2001</creationdate><recordtype>article</recordtype><sourceid/><recordid>eNotj81qxCAYRV20MNNp38FVd4IajXFTKKF_MNBFZz8Y_ZyxJGrVvH8D7erA5XK49wbtGWUd0QPvd-iu1m9KOzYwuUdPo5ltWBecr6nmq2mALSwQG24J5wLZFMBfhdgUmwkxxAueQlq2Xglmrvfo1m-Ah38e0On15TS-k-Pn28f4fCRZ60aAAygHnnvqhRyssmIStnduUsrJbUq_BcC44lpq4wXVSjoGXGvNJtbT7oAe_7S5pJ8VajsvoVqYZxMhrfXMmZBKbxd_AY-IRYE</recordid><startdate>20010101</startdate><enddate>20010101</enddate><creator>Leroux, L</creator><creator>Freche, M</creator><creator>Lacout, J L</creator><scope/></search><sort><creationdate>20010101</creationdate><title>Calcium phosphate cement to prepare Sr-containing biomaterials</title><author>Leroux, L ; Freche, M ; Lacout, J L</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-p99t-e2ee7def2f0f458c7c4b4c6ddb77d50316c4be1272959af40975d1e29991b1603</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2001</creationdate><topic>Biomaterials</topic><topic>Bone</topic><topic>Heating</topic><topic>Hydroxyapatite</topic><topic>Infrared spectroscopy</topic><topic>Nitrates</topic><topic>Phosphoric acid</topic><topic>Strontium</topic><topic>Synthesis (chemical)</topic><topic>Water</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Leroux, L</creatorcontrib><creatorcontrib>Freche, M</creatorcontrib><creatorcontrib>Lacout, J L</creatorcontrib><jtitle>Key engineering materials</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Leroux, L</au><au>Freche, M</au><au>Lacout, J L</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Calcium phosphate cement to prepare Sr-containing biomaterials</atitle><jtitle>Key engineering materials</jtitle><date>2001-01-01</date><risdate>2001</risdate><volume>192-195</volume><spage>235</spage><epage>238</epage><pages>235-238</pages><issn>1013-9826</issn><abstract>A new route, based on the use of ionic calcium phosphate cements, has been developed to synthesize calcium strontium hydroxyapatite. Cements were prepared from tetracalcium phosphate, alpha -tricalcium phosphate, phosphoric acid, strontium nitrate and water and were then mixed and shaped. Cements with various amounts of strontium (0 to 4.3 wt%) were prepared. All the materials obtained were coherent and solid. Mixed hydroxyapatite was obtained at low temperatures. Mixed calcium strontium apatite was obtained after heating. This original method can be of interest for the preparation of biomaterials because strontium plays a part in the mineralisation of bone. The steady release of strontium was studied and can lead to a better osteointegration of the biomaterial.</abstract><tpages>4</tpages></addata></record>
fulltext fulltext
identifier ISSN: 1013-9826
ispartof Key engineering materials, 2001-01, Vol.192-195, p.235-238
issn 1013-9826
language eng
recordid cdi_proquest_miscellaneous_21457901
source Scientific.net Journals
subjects Biomaterials
Bone
Heating
Hydroxyapatite
Infrared spectroscopy
Nitrates
Phosphoric acid
Strontium
Synthesis (chemical)
Water
title Calcium phosphate cement to prepare Sr-containing biomaterials
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-11T08%3A15%3A59IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Calcium%20phosphate%20cement%20to%20prepare%20Sr-containing%20biomaterials&rft.jtitle=Key%20engineering%20materials&rft.au=Leroux,%20L&rft.date=2001-01-01&rft.volume=192-195&rft.spage=235&rft.epage=238&rft.pages=235-238&rft.issn=1013-9826&rft_id=info:doi/&rft_dat=%3Cproquest%3E526449%3C/proquest%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=21457901&rft_id=info:pmid/&rfr_iscdi=true