Precision of different fatigue methods for predicting glass-ceramic failure
This study aimed to characterize the fatigue behavior using two fatigue methods, boundary and staircase, and to predict the probability of failure (P ) of zirconia-reinforced lithium silicate glass-ceramic (ZLS). Bar-shaped specimens of ZLS (18 ×4 ×1.2 mm) were fabricated. Thirty specimens were subj...
Gespeichert in:
Veröffentlicht in: | Journal of the mechanical behavior of biomedical materials 2018-12, Vol.88, p.497-503 |
---|---|
Hauptverfasser: | , , , , |
Format: | Artikel |
Sprache: | eng |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | This study aimed to characterize the fatigue behavior using two fatigue methods, boundary and staircase, and to predict the probability of failure (P
) of zirconia-reinforced lithium silicate glass-ceramic (ZLS). Bar-shaped specimens of ZLS (18 ×4 ×1.2 mm) were fabricated. Thirty specimens were subjected to a three-point flexural strength test using a universal testing machine with 0.5 mm/min crosshead speed, in 37 °C distilled water. Flexural strength data were analyzed with Weibull statistics. Eighty-six bars were subjected to cyclic fatigue using boundary and staircase methods. Fatigue tests were performed in a pneumatic cycling machine (2 Hz, 37 °C distilled water) for 10 ³ and 10
cycles. Fatigue data were analyzed using an inverse power law relationship and log normal-lifetime distribution. Fracture toughness (K
) was determined using V-notched specimens (18 ×4 ×3 mm) and the short beam toughness method (n = 7). Vickers hardness (VH) was evaluated (4.9 N, 20 s). Fractographic and EDS analyses were also performed. ZLS showed a characteristic strength of 197 MPa, Weibull modulus of 4, VH of 6.67 GPa and K
of 1.93 MPa m
. After 10
cycles, for both methods, there was a degradation of 78% of the initial strength. There was no significant degradation when the number of cycles increased from 10
to 10
. Both methods resulted in similar P
and precision at 40 MPa (~50% P
). Yet, staircase shows good accuracy and precision in predicting the stress amplitude for a P
near 50%; while boundary is also effective for P
lower than 50%. The fatigue methods evaluated show similar accuracy and precision for predicting the P
of a glass-ceramic when simulations were made in the range of stress levels and lifetimes used in the fatigue tests. |
---|---|
ISSN: | 1751-6161 1878-0180 |
DOI: | 10.1016/j.jmbbm.2018.09.004 |