Experimental Assessment of Residual Fatigue Life of High Pressure Pipeline Section Containing Longitudinal Cracks

Non-destructive inspection of an operated section of DN 300 high pressure gas pipeline (internal diameter 300 mm) indicated a quite frequent occurrence of longitudinal cracks of depths up to 50 % of the pipe wall thickness. As such cracks would be very dangerous from the viewpoint of further pipelin...