Micro-mechanisms and compressive strength of Geopolymer-Portland cementitious system under various curing temperatures

The excellent strength of low calcium fly ash-based geopolymer paste (GP) can only be attained when high heat curing (60–90 °C) is applied. To achieve reasonable strength in ambient curing temperature (20 ± 2 °C), an inclusion of OPC to GP (GeoPC system), has been studied to accelerate (C,N)-A-S-H f...