Study of damping capacity of Fe–5.4Al–0.05Ti alloy

The damping capacity of a Fe–5.4Al–0.05Ti (wt.%) alloy in structural states was measured using forced bending subresonance vibrations and analysed with an emphasis on grain size and cooling rate effects. Annealing of a cold rolled sheet at higher temperatures or longer times enhances the damping cap...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of alloys and compounds 2015-12, Vol.653, p.460-467
Hauptverfasser: Emdadi, Aliakbar, Nartey, Martinson A., Xu, Yong-gang, Golovin, Igor S.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The damping capacity of a Fe–5.4Al–0.05Ti (wt.%) alloy in structural states was measured using forced bending subresonance vibrations and analysed with an emphasis on grain size and cooling rate effects. Annealing of a cold rolled sheet at higher temperatures or longer times enhances the damping capacity, which mainly corresponds to pinning effects of grain boundaries against domain wall motion. The damping capacity of a single crystalline Fe–Al sample is nearly five times larger than that of a polycrystalline sample reflecting a strong negative role of grain boundaries on the damping capacity. Air cooling of the sample leads to higher damping as compared to water quenching and furnace cooling due to lower local internal stresses in the former case and preventing of ordering in the latter case. Magnetic domains are more regular and finer in the air cooled sample. Local internal stresses imposed on the samples during water quenching, mechanical cleaning of the sample surface, and a static stress lessen the damping capacity due to a pinning effect of magnetic domain wall displacements. The results indicate that heat treatment of the rolled sheet has a significant effect on the damping capacity of specimens. •Study of magnetomechanical damping capacity of ferromagnetic Fe–Al–Ti sheet at different annealing and testing conditions.•Effect of cooling rate on magnetic domain structure and related damping properties.•Influence of local internal stress, static pre-stress, and grain size on damping capacity.
ISSN:0925-8388