Study of the deformation and damage mechanisms of a 9Cr-ODS steel: Microstructure evolution and fracture characteristics

In this study, the tensile properties of a tempered martensitic 9Cr oxide dispersion strengthened (ODS) steel are investigated. The tensile tests were performed in the temperature range of 25°C to 800°C at a nominal strain rate of 10−3s−1. At room temperature, the material exhibited high yield stren...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials science & engineering. A, Structural materials : properties, microstructure and processing Structural materials : properties, microstructure and processing, 2016-03, Vol.658, p.123-134
Hauptverfasser: Chauhan, Ankur, Litvinov, Dimitri, de Carlan, Yann, Aktaa, Jarir
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 134
container_issue
container_start_page 123
container_title Materials science & engineering. A, Structural materials : properties, microstructure and processing
container_volume 658
creator Chauhan, Ankur
Litvinov, Dimitri
de Carlan, Yann
Aktaa, Jarir
description In this study, the tensile properties of a tempered martensitic 9Cr oxide dispersion strengthened (ODS) steel are investigated. The tensile tests were performed in the temperature range of 25°C to 800°C at a nominal strain rate of 10−3s−1. At room temperature, the material exhibited high yield strength and ultimate tensile strength of 929 and 1052MPa, respectively. A decrease in strength was observed with increase in temperature down up to 156MPa of ultimate tensile strength at 800°C. The total elongation-to-failure that was 7.6% at 25°C increased sharply with increase in temperature and reached a maximum of 38.4% at 700°C. In order to compare the influence of heat treatment the tensile tests were also performed on specimens when in a ferritic state. Interestingly, at elevated temperatures both states presented a similar trend of strength and elongation. Transmission electron microscopy after deformation revealed a modification of the deformation mechanism with the temperature. The dislocation activity that was homogeneously distributed at room temperature was localized close to grain boundaries at elevated temperatures. A strong particle–dislocation interaction was observed at all testing temperatures. Orowan mechanism is supposed to govern particle–dislocation interaction at moderate temperatures. At elevated temperatures, an attractive particle–dislocation interaction phenomenon called interfacial pinning was identified. The additional microstructural evolution that includes reduced dislocation density, the transformation of lath structure into coarse equiaxed grains and the M23C6 carbide coarsening, resulted in a loss of strength at elevated temperatures. Fracture surface investigation at room temperature revealed intragranular fracture with dimples. As the temperature increased, the fracture surface formed with a shear-lip zone at the outer periphery and dimples that were larger and deeper in comparison to the ones formed at lower temperatures. These observations are associated with the increased ductility. A change in fracture mechanism from intragranular to intergranular fracture was observed at 650°C. This change became fully apparent at 800°C where it is associated with a reduced ductility. The change in damage mechanism is due to the modification of the deformation mechanism. In comparison to other commercial, as well as experimental, ODS steels, the material offers an excellent compromise between strength and ductility.
doi_str_mv 10.1016/j.msea.2016.01.109
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_1793281470</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0921509316301071</els_id><sourcerecordid>1793281470</sourcerecordid><originalsourceid>FETCH-LOGICAL-c333t-bc8854562ac3ab9ea03ae57d18f9ff3ff2d1be2bc0f8cf8064d0ccb9628e853a3</originalsourceid><addsrcrecordid>eNp9UEtLAzEYDKJgrf4BTzl62Zps9pGIF6lPqPRQPYds8sWm7EOTbLH_3l1WPHqaYZgZmEHokpIFJbS43i2aAGqRDnxB6KCJIzSjvGRJJlhxjGZEpDTJiWCn6CyEHSGEZiSfoe9N7M0BdxbHLWADtvONiq5rsWoNNqpRH4Ab0FvVutCE0aiwWPpkfb_BIQLUN_jVad-F6Hsdew8Y9l3d_1VYryZ5qBgpeBei0-EcnVhVB7j4xTl6f3x4Wz4nq_XTy_JulWjGWEwqzXme5UWqNFOVAEWYgrw0lFthLbM2NbSCtNLEcm05KTJDtK5EkXLgOVNsjq6m3k_fffUQomxc0FDXqoWuD5KWgqWcZiUZrOlkHecED1Z-etcof5CUyPFmuZPjzXK8WRI6aGII3U4hGEbsHXgZtINWg3EedJSmc__FfwADuYj1</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1793281470</pqid></control><display><type>article</type><title>Study of the deformation and damage mechanisms of a 9Cr-ODS steel: Microstructure evolution and fracture characteristics</title><source>Access via ScienceDirect (Elsevier)</source><creator>Chauhan, Ankur ; Litvinov, Dimitri ; de Carlan, Yann ; Aktaa, Jarir</creator><creatorcontrib>Chauhan, Ankur ; Litvinov, Dimitri ; de Carlan, Yann ; Aktaa, Jarir</creatorcontrib><description>In this study, the tensile properties of a tempered martensitic 9Cr oxide dispersion strengthened (ODS) steel are investigated. The tensile tests were performed in the temperature range of 25°C to 800°C at a nominal strain rate of 10−3s−1. At room temperature, the material exhibited high yield strength and ultimate tensile strength of 929 and 1052MPa, respectively. A decrease in strength was observed with increase in temperature down up to 156MPa of ultimate tensile strength at 800°C. The total elongation-to-failure that was 7.6% at 25°C increased sharply with increase in temperature and reached a maximum of 38.4% at 700°C. In order to compare the influence of heat treatment the tensile tests were also performed on specimens when in a ferritic state. Interestingly, at elevated temperatures both states presented a similar trend of strength and elongation. Transmission electron microscopy after deformation revealed a modification of the deformation mechanism with the temperature. The dislocation activity that was homogeneously distributed at room temperature was localized close to grain boundaries at elevated temperatures. A strong particle–dislocation interaction was observed at all testing temperatures. Orowan mechanism is supposed to govern particle–dislocation interaction at moderate temperatures. At elevated temperatures, an attractive particle–dislocation interaction phenomenon called interfacial pinning was identified. The additional microstructural evolution that includes reduced dislocation density, the transformation of lath structure into coarse equiaxed grains and the M23C6 carbide coarsening, resulted in a loss of strength at elevated temperatures. Fracture surface investigation at room temperature revealed intragranular fracture with dimples. As the temperature increased, the fracture surface formed with a shear-lip zone at the outer periphery and dimples that were larger and deeper in comparison to the ones formed at lower temperatures. These observations are associated with the increased ductility. A change in fracture mechanism from intragranular to intergranular fracture was observed at 650°C. This change became fully apparent at 800°C where it is associated with a reduced ductility. The change in damage mechanism is due to the modification of the deformation mechanism. In comparison to other commercial, as well as experimental, ODS steels, the material offers an excellent compromise between strength and ductility.</description><identifier>ISSN: 0921-5093</identifier><identifier>EISSN: 1873-4936</identifier><identifier>DOI: 10.1016/j.msea.2016.01.109</identifier><language>eng</language><publisher>Elsevier B.V</publisher><subject>Chromium steels ; Damage ; Deformation ; Dimpling ; Ductility ; Fracture mechanics ; Fracture surfaces ; High temperature ; Microstructure ; ODS steel ; Strength ; TEM ; Tempered martensite ; Tensile properties</subject><ispartof>Materials science &amp; engineering. A, Structural materials : properties, microstructure and processing, 2016-03, Vol.658, p.123-134</ispartof><rights>2016 Elsevier B.V.</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c333t-bc8854562ac3ab9ea03ae57d18f9ff3ff2d1be2bc0f8cf8064d0ccb9628e853a3</citedby><cites>FETCH-LOGICAL-c333t-bc8854562ac3ab9ea03ae57d18f9ff3ff2d1be2bc0f8cf8064d0ccb9628e853a3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://dx.doi.org/10.1016/j.msea.2016.01.109$$EHTML$$P50$$Gelsevier$$H</linktohtml><link.rule.ids>315,782,786,3552,27931,27932,46002</link.rule.ids></links><search><creatorcontrib>Chauhan, Ankur</creatorcontrib><creatorcontrib>Litvinov, Dimitri</creatorcontrib><creatorcontrib>de Carlan, Yann</creatorcontrib><creatorcontrib>Aktaa, Jarir</creatorcontrib><title>Study of the deformation and damage mechanisms of a 9Cr-ODS steel: Microstructure evolution and fracture characteristics</title><title>Materials science &amp; engineering. A, Structural materials : properties, microstructure and processing</title><description>In this study, the tensile properties of a tempered martensitic 9Cr oxide dispersion strengthened (ODS) steel are investigated. The tensile tests were performed in the temperature range of 25°C to 800°C at a nominal strain rate of 10−3s−1. At room temperature, the material exhibited high yield strength and ultimate tensile strength of 929 and 1052MPa, respectively. A decrease in strength was observed with increase in temperature down up to 156MPa of ultimate tensile strength at 800°C. The total elongation-to-failure that was 7.6% at 25°C increased sharply with increase in temperature and reached a maximum of 38.4% at 700°C. In order to compare the influence of heat treatment the tensile tests were also performed on specimens when in a ferritic state. Interestingly, at elevated temperatures both states presented a similar trend of strength and elongation. Transmission electron microscopy after deformation revealed a modification of the deformation mechanism with the temperature. The dislocation activity that was homogeneously distributed at room temperature was localized close to grain boundaries at elevated temperatures. A strong particle–dislocation interaction was observed at all testing temperatures. Orowan mechanism is supposed to govern particle–dislocation interaction at moderate temperatures. At elevated temperatures, an attractive particle–dislocation interaction phenomenon called interfacial pinning was identified. The additional microstructural evolution that includes reduced dislocation density, the transformation of lath structure into coarse equiaxed grains and the M23C6 carbide coarsening, resulted in a loss of strength at elevated temperatures. Fracture surface investigation at room temperature revealed intragranular fracture with dimples. As the temperature increased, the fracture surface formed with a shear-lip zone at the outer periphery and dimples that were larger and deeper in comparison to the ones formed at lower temperatures. These observations are associated with the increased ductility. A change in fracture mechanism from intragranular to intergranular fracture was observed at 650°C. This change became fully apparent at 800°C where it is associated with a reduced ductility. The change in damage mechanism is due to the modification of the deformation mechanism. In comparison to other commercial, as well as experimental, ODS steels, the material offers an excellent compromise between strength and ductility.</description><subject>Chromium steels</subject><subject>Damage</subject><subject>Deformation</subject><subject>Dimpling</subject><subject>Ductility</subject><subject>Fracture mechanics</subject><subject>Fracture surfaces</subject><subject>High temperature</subject><subject>Microstructure</subject><subject>ODS steel</subject><subject>Strength</subject><subject>TEM</subject><subject>Tempered martensite</subject><subject>Tensile properties</subject><issn>0921-5093</issn><issn>1873-4936</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2016</creationdate><recordtype>article</recordtype><recordid>eNp9UEtLAzEYDKJgrf4BTzl62Zps9pGIF6lPqPRQPYds8sWm7EOTbLH_3l1WPHqaYZgZmEHokpIFJbS43i2aAGqRDnxB6KCJIzSjvGRJJlhxjGZEpDTJiWCn6CyEHSGEZiSfoe9N7M0BdxbHLWADtvONiq5rsWoNNqpRH4Ab0FvVutCE0aiwWPpkfb_BIQLUN_jVad-F6Hsdew8Y9l3d_1VYryZ5qBgpeBei0-EcnVhVB7j4xTl6f3x4Wz4nq_XTy_JulWjGWEwqzXme5UWqNFOVAEWYgrw0lFthLbM2NbSCtNLEcm05KTJDtK5EkXLgOVNsjq6m3k_fffUQomxc0FDXqoWuD5KWgqWcZiUZrOlkHecED1Z-etcof5CUyPFmuZPjzXK8WRI6aGII3U4hGEbsHXgZtINWg3EedJSmc__FfwADuYj1</recordid><startdate>20160321</startdate><enddate>20160321</enddate><creator>Chauhan, Ankur</creator><creator>Litvinov, Dimitri</creator><creator>de Carlan, Yann</creator><creator>Aktaa, Jarir</creator><general>Elsevier B.V</general><scope>AAYXX</scope><scope>CITATION</scope><scope>7SR</scope><scope>8BQ</scope><scope>8FD</scope><scope>JG9</scope></search><sort><creationdate>20160321</creationdate><title>Study of the deformation and damage mechanisms of a 9Cr-ODS steel: Microstructure evolution and fracture characteristics</title><author>Chauhan, Ankur ; Litvinov, Dimitri ; de Carlan, Yann ; Aktaa, Jarir</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c333t-bc8854562ac3ab9ea03ae57d18f9ff3ff2d1be2bc0f8cf8064d0ccb9628e853a3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2016</creationdate><topic>Chromium steels</topic><topic>Damage</topic><topic>Deformation</topic><topic>Dimpling</topic><topic>Ductility</topic><topic>Fracture mechanics</topic><topic>Fracture surfaces</topic><topic>High temperature</topic><topic>Microstructure</topic><topic>ODS steel</topic><topic>Strength</topic><topic>TEM</topic><topic>Tempered martensite</topic><topic>Tensile properties</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Chauhan, Ankur</creatorcontrib><creatorcontrib>Litvinov, Dimitri</creatorcontrib><creatorcontrib>de Carlan, Yann</creatorcontrib><creatorcontrib>Aktaa, Jarir</creatorcontrib><collection>CrossRef</collection><collection>Engineered Materials Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><jtitle>Materials science &amp; engineering. A, Structural materials : properties, microstructure and processing</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Chauhan, Ankur</au><au>Litvinov, Dimitri</au><au>de Carlan, Yann</au><au>Aktaa, Jarir</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Study of the deformation and damage mechanisms of a 9Cr-ODS steel: Microstructure evolution and fracture characteristics</atitle><jtitle>Materials science &amp; engineering. A, Structural materials : properties, microstructure and processing</jtitle><date>2016-03-21</date><risdate>2016</risdate><volume>658</volume><spage>123</spage><epage>134</epage><pages>123-134</pages><issn>0921-5093</issn><eissn>1873-4936</eissn><abstract>In this study, the tensile properties of a tempered martensitic 9Cr oxide dispersion strengthened (ODS) steel are investigated. The tensile tests were performed in the temperature range of 25°C to 800°C at a nominal strain rate of 10−3s−1. At room temperature, the material exhibited high yield strength and ultimate tensile strength of 929 and 1052MPa, respectively. A decrease in strength was observed with increase in temperature down up to 156MPa of ultimate tensile strength at 800°C. The total elongation-to-failure that was 7.6% at 25°C increased sharply with increase in temperature and reached a maximum of 38.4% at 700°C. In order to compare the influence of heat treatment the tensile tests were also performed on specimens when in a ferritic state. Interestingly, at elevated temperatures both states presented a similar trend of strength and elongation. Transmission electron microscopy after deformation revealed a modification of the deformation mechanism with the temperature. The dislocation activity that was homogeneously distributed at room temperature was localized close to grain boundaries at elevated temperatures. A strong particle–dislocation interaction was observed at all testing temperatures. Orowan mechanism is supposed to govern particle–dislocation interaction at moderate temperatures. At elevated temperatures, an attractive particle–dislocation interaction phenomenon called interfacial pinning was identified. The additional microstructural evolution that includes reduced dislocation density, the transformation of lath structure into coarse equiaxed grains and the M23C6 carbide coarsening, resulted in a loss of strength at elevated temperatures. Fracture surface investigation at room temperature revealed intragranular fracture with dimples. As the temperature increased, the fracture surface formed with a shear-lip zone at the outer periphery and dimples that were larger and deeper in comparison to the ones formed at lower temperatures. These observations are associated with the increased ductility. A change in fracture mechanism from intragranular to intergranular fracture was observed at 650°C. This change became fully apparent at 800°C where it is associated with a reduced ductility. The change in damage mechanism is due to the modification of the deformation mechanism. In comparison to other commercial, as well as experimental, ODS steels, the material offers an excellent compromise between strength and ductility.</abstract><pub>Elsevier B.V</pub><doi>10.1016/j.msea.2016.01.109</doi><tpages>12</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0921-5093
ispartof Materials science & engineering. A, Structural materials : properties, microstructure and processing, 2016-03, Vol.658, p.123-134
issn 0921-5093
1873-4936
language eng
recordid cdi_proquest_miscellaneous_1793281470
source Access via ScienceDirect (Elsevier)
subjects Chromium steels
Damage
Deformation
Dimpling
Ductility
Fracture mechanics
Fracture surfaces
High temperature
Microstructure
ODS steel
Strength
TEM
Tempered martensite
Tensile properties
title Study of the deformation and damage mechanisms of a 9Cr-ODS steel: Microstructure evolution and fracture characteristics
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-04T08%3A57%3A22IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Study%20of%20the%20deformation%20and%20damage%20mechanisms%20of%20a%209Cr-ODS%20steel:%20Microstructure%20evolution%20and%20fracture%20characteristics&rft.jtitle=Materials%20science%20&%20engineering.%20A,%20Structural%20materials%20:%20properties,%20microstructure%20and%20processing&rft.au=Chauhan,%20Ankur&rft.date=2016-03-21&rft.volume=658&rft.spage=123&rft.epage=134&rft.pages=123-134&rft.issn=0921-5093&rft.eissn=1873-4936&rft_id=info:doi/10.1016/j.msea.2016.01.109&rft_dat=%3Cproquest_cross%3E1793281470%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=1793281470&rft_id=info:pmid/&rft_els_id=S0921509316301071&rfr_iscdi=true