THREE POINT BENDING TEST OF COLD FORMED SHS COLUMN TO THROUGH DIAPHRAGM WELDING CONNECTION USING 25 DEGREE NARROW GROOVE
This study presents the results of a three-point bending test performed on a cold-formed square hollow section (SHS) column to a through diaphragm welding connection using a 25 degree narrow groove. The test results are summarized as follows: The deformation capacity of a cold-formed SHS column to a...
Gespeichert in:
Veröffentlicht in: | Journal of Structural and Construction Engineering (Transactions of AIJ) 2015, Vol.80(718), pp.1991-1999 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | 1999 |
---|---|
container_issue | 718 |
container_start_page | 1991 |
container_title | Journal of Structural and Construction Engineering (Transactions of AIJ) |
container_volume | 80 |
creator | HATTORI, Kazunori MINAMI, Susumu NAKAGOMI, Tadao NISHIYAMA, Isao |
description | This study presents the results of a three-point bending test performed on a cold-formed square hollow section (SHS) column to a through diaphragm welding connection using a 25 degree narrow groove. The test results are summarized as follows: The deformation capacity of a cold-formed SHS column to a through diaphragm welding connection by using a 25 degree narrow groove is comparable to or higher than that obtained in previous tests by using a 35 degree standard groove. Relieving the stress concentration at the weld toe through grinder finishing delayed ductile crack initiation, thus improving the deformation capability of the welded connection of the cold-formed SHS column. |
doi_str_mv | 10.3130/aijs.80.1991 |
format | Article |
fullrecord | <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_1786206012</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>1786206012</sourcerecordid><originalsourceid>FETCH-LOGICAL-c2791-df1846de0b0d6233e79832ca52e2494039a556be922f188666c82e69e7c2691f3</originalsourceid><addsrcrecordid>eNo9kEtPwkAUhRujiYju_AGzdGFxHu10ZlnboW1SOqQUWU6GMiiElx1I9N_birK6r--cmxzHeURwQBCBL3q1tgMGB4hzdOX0EGPIZcgn121PPOh6GOJb587aNYTU4xT1nK8qLYUAY5kVFXgVRZwVCajEpAJyCCKZx2Aoy5GIwSSddPN0VIBKglYlp0kK4iwcp2WYjMBM5L_aSBaFiKpMFmA66RbYB7FIuidFWJZyBpJSyjdx79ws9caah7_ad6ZDUUWpm8ski8LcrXHAkbtYIubRhYFzuKCYEBNwRnCtfWywxz1IuPZ9Ojcc45ZklNKaYUO5CWpMOVqSvvN09j00-8-TsUe1XdnabDZ6Z_Ynq1DAKIYUItyiz2e0bvbWNmapDs1qq5tvhaDqAlZdwIpB1QXc4uEZX9ujfjcXWDfHVb0xFzhA7F9zudUfulFmR34AOPx6eA</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1786206012</pqid></control><display><type>article</type><title>THREE POINT BENDING TEST OF COLD FORMED SHS COLUMN TO THROUGH DIAPHRAGM WELDING CONNECTION USING 25 DEGREE NARROW GROOVE</title><source>J-STAGE Free</source><source>Open Access Journals</source><creator>HATTORI, Kazunori ; MINAMI, Susumu ; NAKAGOMI, Tadao ; NISHIYAMA, Isao</creator><creatorcontrib>HATTORI, Kazunori ; MINAMI, Susumu ; NAKAGOMI, Tadao ; NISHIYAMA, Isao</creatorcontrib><description>This study presents the results of a three-point bending test performed on a cold-formed square hollow section (SHS) column to a through diaphragm welding connection using a 25 degree narrow groove. The test results are summarized as follows: The deformation capacity of a cold-formed SHS column to a through diaphragm welding connection by using a 25 degree narrow groove is comparable to or higher than that obtained in previous tests by using a 35 degree standard groove. Relieving the stress concentration at the weld toe through grinder finishing delayed ductile crack initiation, thus improving the deformation capability of the welded connection of the cold-formed SHS column.</description><identifier>ISSN: 1340-4202</identifier><identifier>EISSN: 1881-8153</identifier><identifier>DOI: 10.3130/aijs.80.1991</identifier><language>eng ; jpn</language><publisher>Architectural Institute of Japan</publisher><subject>25 degree Narrow Groove ; Bend tests ; Cold formed SHS column ; Cold forming ; Cold working ; Columns (structural) ; Cumulative Plastic Deformation ; Cyclic Bending Loading ; Diaphragms ; Grooves ; Self-propagating synthesis ; Welded Connection ; Welding ; Welding Robot</subject><ispartof>Journal of Structural and Construction Engineering (Transactions of AIJ), 2015, Vol.80(718), pp.1991-1999</ispartof><rights>2015 Architectural Institute of Japan</rights><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c2791-df1846de0b0d6233e79832ca52e2494039a556be922f188666c82e69e7c2691f3</citedby><cites>FETCH-LOGICAL-c2791-df1846de0b0d6233e79832ca52e2494039a556be922f188666c82e69e7c2691f3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,776,780,1876,4009,27902,27903,27904</link.rule.ids></links><search><creatorcontrib>HATTORI, Kazunori</creatorcontrib><creatorcontrib>MINAMI, Susumu</creatorcontrib><creatorcontrib>NAKAGOMI, Tadao</creatorcontrib><creatorcontrib>NISHIYAMA, Isao</creatorcontrib><title>THREE POINT BENDING TEST OF COLD FORMED SHS COLUMN TO THROUGH DIAPHRAGM WELDING CONNECTION USING 25 DEGREE NARROW GROOVE</title><title>Journal of Structural and Construction Engineering (Transactions of AIJ)</title><addtitle>J. Struct. Constr. Eng.</addtitle><description>This study presents the results of a three-point bending test performed on a cold-formed square hollow section (SHS) column to a through diaphragm welding connection using a 25 degree narrow groove. The test results are summarized as follows: The deformation capacity of a cold-formed SHS column to a through diaphragm welding connection by using a 25 degree narrow groove is comparable to or higher than that obtained in previous tests by using a 35 degree standard groove. Relieving the stress concentration at the weld toe through grinder finishing delayed ductile crack initiation, thus improving the deformation capability of the welded connection of the cold-formed SHS column.</description><subject>25 degree Narrow Groove</subject><subject>Bend tests</subject><subject>Cold formed SHS column</subject><subject>Cold forming</subject><subject>Cold working</subject><subject>Columns (structural)</subject><subject>Cumulative Plastic Deformation</subject><subject>Cyclic Bending Loading</subject><subject>Diaphragms</subject><subject>Grooves</subject><subject>Self-propagating synthesis</subject><subject>Welded Connection</subject><subject>Welding</subject><subject>Welding Robot</subject><issn>1340-4202</issn><issn>1881-8153</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2015</creationdate><recordtype>article</recordtype><recordid>eNo9kEtPwkAUhRujiYju_AGzdGFxHu10ZlnboW1SOqQUWU6GMiiElx1I9N_birK6r--cmxzHeURwQBCBL3q1tgMGB4hzdOX0EGPIZcgn121PPOh6GOJb587aNYTU4xT1nK8qLYUAY5kVFXgVRZwVCajEpAJyCCKZx2Aoy5GIwSSddPN0VIBKglYlp0kK4iwcp2WYjMBM5L_aSBaFiKpMFmA66RbYB7FIuidFWJZyBpJSyjdx79ws9caah7_ad6ZDUUWpm8ski8LcrXHAkbtYIubRhYFzuKCYEBNwRnCtfWywxz1IuPZ9Ojcc45ZklNKaYUO5CWpMOVqSvvN09j00-8-TsUe1XdnabDZ6Z_Ynq1DAKIYUItyiz2e0bvbWNmapDs1qq5tvhaDqAlZdwIpB1QXc4uEZX9ujfjcXWDfHVb0xFzhA7F9zudUfulFmR34AOPx6eA</recordid><startdate>2015</startdate><enddate>2015</enddate><creator>HATTORI, Kazunori</creator><creator>MINAMI, Susumu</creator><creator>NAKAGOMI, Tadao</creator><creator>NISHIYAMA, Isao</creator><general>Architectural Institute of Japan</general><scope>AAYXX</scope><scope>CITATION</scope><scope>8FD</scope><scope>FR3</scope><scope>KR7</scope></search><sort><creationdate>2015</creationdate><title>THREE POINT BENDING TEST OF COLD FORMED SHS COLUMN TO THROUGH DIAPHRAGM WELDING CONNECTION USING 25 DEGREE NARROW GROOVE</title><author>HATTORI, Kazunori ; MINAMI, Susumu ; NAKAGOMI, Tadao ; NISHIYAMA, Isao</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c2791-df1846de0b0d6233e79832ca52e2494039a556be922f188666c82e69e7c2691f3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng ; jpn</language><creationdate>2015</creationdate><topic>25 degree Narrow Groove</topic><topic>Bend tests</topic><topic>Cold formed SHS column</topic><topic>Cold forming</topic><topic>Cold working</topic><topic>Columns (structural)</topic><topic>Cumulative Plastic Deformation</topic><topic>Cyclic Bending Loading</topic><topic>Diaphragms</topic><topic>Grooves</topic><topic>Self-propagating synthesis</topic><topic>Welded Connection</topic><topic>Welding</topic><topic>Welding Robot</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>HATTORI, Kazunori</creatorcontrib><creatorcontrib>MINAMI, Susumu</creatorcontrib><creatorcontrib>NAKAGOMI, Tadao</creatorcontrib><creatorcontrib>NISHIYAMA, Isao</creatorcontrib><collection>CrossRef</collection><collection>Technology Research Database</collection><collection>Engineering Research Database</collection><collection>Civil Engineering Abstracts</collection><jtitle>Journal of Structural and Construction Engineering (Transactions of AIJ)</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>HATTORI, Kazunori</au><au>MINAMI, Susumu</au><au>NAKAGOMI, Tadao</au><au>NISHIYAMA, Isao</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>THREE POINT BENDING TEST OF COLD FORMED SHS COLUMN TO THROUGH DIAPHRAGM WELDING CONNECTION USING 25 DEGREE NARROW GROOVE</atitle><jtitle>Journal of Structural and Construction Engineering (Transactions of AIJ)</jtitle><addtitle>J. Struct. Constr. Eng.</addtitle><date>2015</date><risdate>2015</risdate><volume>80</volume><issue>718</issue><spage>1991</spage><epage>1999</epage><pages>1991-1999</pages><issn>1340-4202</issn><eissn>1881-8153</eissn><abstract>This study presents the results of a three-point bending test performed on a cold-formed square hollow section (SHS) column to a through diaphragm welding connection using a 25 degree narrow groove. The test results are summarized as follows: The deformation capacity of a cold-formed SHS column to a through diaphragm welding connection by using a 25 degree narrow groove is comparable to or higher than that obtained in previous tests by using a 35 degree standard groove. Relieving the stress concentration at the weld toe through grinder finishing delayed ductile crack initiation, thus improving the deformation capability of the welded connection of the cold-formed SHS column.</abstract><pub>Architectural Institute of Japan</pub><doi>10.3130/aijs.80.1991</doi><tpages>9</tpages><oa>free_for_read</oa></addata></record> |
fulltext | fulltext |
identifier | ISSN: 1340-4202 |
ispartof | Journal of Structural and Construction Engineering (Transactions of AIJ), 2015, Vol.80(718), pp.1991-1999 |
issn | 1340-4202 1881-8153 |
language | eng ; jpn |
recordid | cdi_proquest_miscellaneous_1786206012 |
source | J-STAGE Free; Open Access Journals |
subjects | 25 degree Narrow Groove Bend tests Cold formed SHS column Cold forming Cold working Columns (structural) Cumulative Plastic Deformation Cyclic Bending Loading Diaphragms Grooves Self-propagating synthesis Welded Connection Welding Welding Robot |
title | THREE POINT BENDING TEST OF COLD FORMED SHS COLUMN TO THROUGH DIAPHRAGM WELDING CONNECTION USING 25 DEGREE NARROW GROOVE |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-24T19%3A25%3A19IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=THREE%20POINT%20BENDING%20TEST%20OF%20COLD%20FORMED%20SHS%20COLUMN%20TO%20THROUGH%20DIAPHRAGM%20WELDING%20CONNECTION%20USING%2025%20DEGREE%20NARROW%20GROOVE&rft.jtitle=Journal%20of%20Structural%20and%20Construction%20Engineering%20(Transactions%20of%20AIJ)&rft.au=HATTORI,%20Kazunori&rft.date=2015&rft.volume=80&rft.issue=718&rft.spage=1991&rft.epage=1999&rft.pages=1991-1999&rft.issn=1340-4202&rft.eissn=1881-8153&rft_id=info:doi/10.3130/aijs.80.1991&rft_dat=%3Cproquest_cross%3E1786206012%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=1786206012&rft_id=info:pmid/&rfr_iscdi=true |