1-3 ceramic/polymer composites for high-temperature transducer applications

1‐3 ceramic/polymer composites based on high Curie temperature ferroelectric ceramic BiScO3–PbTiO3 (BSPT) were fabricated using the dice and fill method. The electromechanical coupling factor kt of BSPT composite was found to be 58% at room temperature, higher than the thickness coupling factor of m...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Physica status solidi. A, Applications and materials science Applications and materials science, 2013-09, Vol.210 (9), p.1888-1891
Hauptverfasser: Li, Lili, Zhang, Shujun, Xu, Zhuo, Geng, Xuecang, Shrout, Thomas R.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:1‐3 ceramic/polymer composites based on high Curie temperature ferroelectric ceramic BiScO3–PbTiO3 (BSPT) were fabricated using the dice and fill method. The electromechanical coupling factor kt of BSPT composite was found to be 58% at room temperature, higher than the thickness coupling factor of monolithic BSPT ∼50%. In addition, BSPT 1‐3 composite exhibits high thermal stability of electromechanical properties and low dielectric loss up to 300 °C, making it a potential candidate for broad‐bandwidth transducer applications at elevated temperatures.
ISSN:1862-6300
1862-6319
DOI:10.1002/pssa.201228787