A critical assessment of the microstructure and mechanical properties of friction stir welded reduced activation ferritic–martensitic steel

Bead-on-plate friction stir welding was conducted on 6mm thick plate of Reduced Activation Ferritic–Martensitic Steel employing polycrystalline cubic boron nitride tool with rotational speeds of 200, 300, 500 and 700rpm and traverse speed of 30mm/min. The interface temperature between shoulder botto...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials & design 2016-02, Vol.92, p.200-212
Hauptverfasser: Manugula, Vijaya L., Rajulapati, Koteswararao V., Madhusudhan Reddy, G., Mythili, R., Bhanu Sankara Rao, K.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 212
container_issue
container_start_page 200
container_title Materials & design
container_volume 92
creator Manugula, Vijaya L.
Rajulapati, Koteswararao V.
Madhusudhan Reddy, G.
Mythili, R.
Bhanu Sankara Rao, K.
description Bead-on-plate friction stir welding was conducted on 6mm thick plate of Reduced Activation Ferritic–Martensitic Steel employing polycrystalline cubic boron nitride tool with rotational speeds of 200, 300, 500 and 700rpm and traverse speed of 30mm/min. The interface temperature between shoulder bottom and top surface of the plate was monitored by non-contact in-line thermography which served to identify the peak temperature attained in the stir zone (SZ). This temperature for 200, 300 and 500, and 700rpm was respectively below Ac1, between Ac1 and Ac3, and above Ac3. In the base metal (BM), the prior austenite grain and martensite lath boundaries were decorated with chromium and tungsten rich M23C6 precipitates while intra-lath regions revealed Ta and V rich MX type carbides. Rotational speeds greater than 300rpm led to martensite formation and simultaneous recovery, recrystallization and grain growth in SZs with wide distribution in grain size whereas SZ of 200rpm and BM possessed similar distribution. The grain boundary M23C6 dissolved and very fine needles of Fe3C precipitated in all SZs. The hardness of all SZs was unacceptably higher compared to the BM. The 200rpm weld exhibited higher impact toughness in the absence of martensite in SZ. [Display omitted] •Effects of rotational speed during friction stir welding of a ferritic–martensitic steel were investigated.•Distribution of grain size in stir zones varied as a function of rotational speed.•Grain boundary M23C6 precipitates were dissolved while Fe3C formed in stir zones at all rotational speeds.•High rotational speeds promoted martensite occurrence in the stir zones with a drastic reduction in impact toughness.•Peak temperatures below Ac1 in the stir zone enabled impact toughness matching with the base metal.
doi_str_mv 10.1016/j.matdes.2015.12.019
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_1786151331</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0264127515308807</els_id><sourcerecordid>1786151331</sourcerecordid><originalsourceid>FETCH-LOGICAL-c339t-a02c3fca75ae451a6c5f2ceb3fde4fed25c067ac9e6a546a0e9515895efadf323</originalsourceid><addsrcrecordid>eNp9kE1OHDEQhS2USExIbsDCSzbdcdnt7ukNEkLkR0LKBtZWxS4Lj_pnsN0gdrlAVtyQk-CeyTqrUqneq6r3MXYOogYB7dddPWJ2lGopQNcgawH9CdvAtlNVA333gW2EbJsKZKdP2aeUdkJI2almw_5ecRtDDhYHjilRSiNNmc-e5wfiY7BxTjkuNi-ROE6Oj2QfcDro93HeU8yB0qr3Mdgc5omnHCJ_psGR45HcYkvFMnrCw9hTPBx8-_M6Ysw0pbUrLqLhM_vocUj05V89Y_ffbu6uf1S3v77_vL66raxSfa5QSKu8xU4jNRqwtdpLS7-Vd9R4clJb0XZoe2pRNy0K6jXoba_Jo_NKqjN2cdxbIjwulLIZQ7I0DDjRvCQD3bYFDUpBkTZH6UoiRfJmH0N5_MWAMCt9szNH-malb0CaQr_YLo82KjGeAkWTbKCpsAiRbDZuDv9f8A663ZY5</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1786151331</pqid></control><display><type>article</type><title>A critical assessment of the microstructure and mechanical properties of friction stir welded reduced activation ferritic–martensitic steel</title><source>Alma/SFX Local Collection</source><creator>Manugula, Vijaya L. ; Rajulapati, Koteswararao V. ; Madhusudhan Reddy, G. ; Mythili, R. ; Bhanu Sankara Rao, K.</creator><creatorcontrib>Manugula, Vijaya L. ; Rajulapati, Koteswararao V. ; Madhusudhan Reddy, G. ; Mythili, R. ; Bhanu Sankara Rao, K.</creatorcontrib><description>Bead-on-plate friction stir welding was conducted on 6mm thick plate of Reduced Activation Ferritic–Martensitic Steel employing polycrystalline cubic boron nitride tool with rotational speeds of 200, 300, 500 and 700rpm and traverse speed of 30mm/min. The interface temperature between shoulder bottom and top surface of the plate was monitored by non-contact in-line thermography which served to identify the peak temperature attained in the stir zone (SZ). This temperature for 200, 300 and 500, and 700rpm was respectively below Ac1, between Ac1 and Ac3, and above Ac3. In the base metal (BM), the prior austenite grain and martensite lath boundaries were decorated with chromium and tungsten rich M23C6 precipitates while intra-lath regions revealed Ta and V rich MX type carbides. Rotational speeds greater than 300rpm led to martensite formation and simultaneous recovery, recrystallization and grain growth in SZs with wide distribution in grain size whereas SZ of 200rpm and BM possessed similar distribution. The grain boundary M23C6 dissolved and very fine needles of Fe3C precipitated in all SZs. The hardness of all SZs was unacceptably higher compared to the BM. The 200rpm weld exhibited higher impact toughness in the absence of martensite in SZ. [Display omitted] •Effects of rotational speed during friction stir welding of a ferritic–martensitic steel were investigated.•Distribution of grain size in stir zones varied as a function of rotational speed.•Grain boundary M23C6 precipitates were dissolved while Fe3C formed in stir zones at all rotational speeds.•High rotational speeds promoted martensite occurrence in the stir zones with a drastic reduction in impact toughness.•Peak temperatures below Ac1 in the stir zone enabled impact toughness matching with the base metal.</description><identifier>ISSN: 0264-1275</identifier><identifier>EISSN: 1873-4197</identifier><identifier>DOI: 10.1016/j.matdes.2015.12.019</identifier><language>eng</language><publisher>Elsevier Ltd</publisher><subject>Activation ; Friction stir welding ; Hardness ; Interface temperature ; Martensite ; Mechanical properties ; Microstructure ; Needles ; RAFM steel ; Rotational ; Steels ; Stir zone ; Tungsten</subject><ispartof>Materials &amp; design, 2016-02, Vol.92, p.200-212</ispartof><rights>2015 Elsevier Ltd</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c339t-a02c3fca75ae451a6c5f2ceb3fde4fed25c067ac9e6a546a0e9515895efadf323</citedby><cites>FETCH-LOGICAL-c339t-a02c3fca75ae451a6c5f2ceb3fde4fed25c067ac9e6a546a0e9515895efadf323</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,776,780,27901,27902</link.rule.ids></links><search><creatorcontrib>Manugula, Vijaya L.</creatorcontrib><creatorcontrib>Rajulapati, Koteswararao V.</creatorcontrib><creatorcontrib>Madhusudhan Reddy, G.</creatorcontrib><creatorcontrib>Mythili, R.</creatorcontrib><creatorcontrib>Bhanu Sankara Rao, K.</creatorcontrib><title>A critical assessment of the microstructure and mechanical properties of friction stir welded reduced activation ferritic–martensitic steel</title><title>Materials &amp; design</title><description>Bead-on-plate friction stir welding was conducted on 6mm thick plate of Reduced Activation Ferritic–Martensitic Steel employing polycrystalline cubic boron nitride tool with rotational speeds of 200, 300, 500 and 700rpm and traverse speed of 30mm/min. The interface temperature between shoulder bottom and top surface of the plate was monitored by non-contact in-line thermography which served to identify the peak temperature attained in the stir zone (SZ). This temperature for 200, 300 and 500, and 700rpm was respectively below Ac1, between Ac1 and Ac3, and above Ac3. In the base metal (BM), the prior austenite grain and martensite lath boundaries were decorated with chromium and tungsten rich M23C6 precipitates while intra-lath regions revealed Ta and V rich MX type carbides. Rotational speeds greater than 300rpm led to martensite formation and simultaneous recovery, recrystallization and grain growth in SZs with wide distribution in grain size whereas SZ of 200rpm and BM possessed similar distribution. The grain boundary M23C6 dissolved and very fine needles of Fe3C precipitated in all SZs. The hardness of all SZs was unacceptably higher compared to the BM. The 200rpm weld exhibited higher impact toughness in the absence of martensite in SZ. [Display omitted] •Effects of rotational speed during friction stir welding of a ferritic–martensitic steel were investigated.•Distribution of grain size in stir zones varied as a function of rotational speed.•Grain boundary M23C6 precipitates were dissolved while Fe3C formed in stir zones at all rotational speeds.•High rotational speeds promoted martensite occurrence in the stir zones with a drastic reduction in impact toughness.•Peak temperatures below Ac1 in the stir zone enabled impact toughness matching with the base metal.</description><subject>Activation</subject><subject>Friction stir welding</subject><subject>Hardness</subject><subject>Interface temperature</subject><subject>Martensite</subject><subject>Mechanical properties</subject><subject>Microstructure</subject><subject>Needles</subject><subject>RAFM steel</subject><subject>Rotational</subject><subject>Steels</subject><subject>Stir zone</subject><subject>Tungsten</subject><issn>0264-1275</issn><issn>1873-4197</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2016</creationdate><recordtype>article</recordtype><recordid>eNp9kE1OHDEQhS2USExIbsDCSzbdcdnt7ukNEkLkR0LKBtZWxS4Lj_pnsN0gdrlAVtyQk-CeyTqrUqneq6r3MXYOogYB7dddPWJ2lGopQNcgawH9CdvAtlNVA333gW2EbJsKZKdP2aeUdkJI2almw_5ecRtDDhYHjilRSiNNmc-e5wfiY7BxTjkuNi-ROE6Oj2QfcDro93HeU8yB0qr3Mdgc5omnHCJ_psGR45HcYkvFMnrCw9hTPBx8-_M6Ysw0pbUrLqLhM_vocUj05V89Y_ffbu6uf1S3v77_vL66raxSfa5QSKu8xU4jNRqwtdpLS7-Vd9R4clJb0XZoe2pRNy0K6jXoba_Jo_NKqjN2cdxbIjwulLIZQ7I0DDjRvCQD3bYFDUpBkTZH6UoiRfJmH0N5_MWAMCt9szNH-malb0CaQr_YLo82KjGeAkWTbKCpsAiRbDZuDv9f8A663ZY5</recordid><startdate>20160215</startdate><enddate>20160215</enddate><creator>Manugula, Vijaya L.</creator><creator>Rajulapati, Koteswararao V.</creator><creator>Madhusudhan Reddy, G.</creator><creator>Mythili, R.</creator><creator>Bhanu Sankara Rao, K.</creator><general>Elsevier Ltd</general><scope>AAYXX</scope><scope>CITATION</scope><scope>7SR</scope><scope>8BQ</scope><scope>8FD</scope><scope>JG9</scope></search><sort><creationdate>20160215</creationdate><title>A critical assessment of the microstructure and mechanical properties of friction stir welded reduced activation ferritic–martensitic steel</title><author>Manugula, Vijaya L. ; Rajulapati, Koteswararao V. ; Madhusudhan Reddy, G. ; Mythili, R. ; Bhanu Sankara Rao, K.</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c339t-a02c3fca75ae451a6c5f2ceb3fde4fed25c067ac9e6a546a0e9515895efadf323</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2016</creationdate><topic>Activation</topic><topic>Friction stir welding</topic><topic>Hardness</topic><topic>Interface temperature</topic><topic>Martensite</topic><topic>Mechanical properties</topic><topic>Microstructure</topic><topic>Needles</topic><topic>RAFM steel</topic><topic>Rotational</topic><topic>Steels</topic><topic>Stir zone</topic><topic>Tungsten</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Manugula, Vijaya L.</creatorcontrib><creatorcontrib>Rajulapati, Koteswararao V.</creatorcontrib><creatorcontrib>Madhusudhan Reddy, G.</creatorcontrib><creatorcontrib>Mythili, R.</creatorcontrib><creatorcontrib>Bhanu Sankara Rao, K.</creatorcontrib><collection>CrossRef</collection><collection>Engineered Materials Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><jtitle>Materials &amp; design</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Manugula, Vijaya L.</au><au>Rajulapati, Koteswararao V.</au><au>Madhusudhan Reddy, G.</au><au>Mythili, R.</au><au>Bhanu Sankara Rao, K.</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>A critical assessment of the microstructure and mechanical properties of friction stir welded reduced activation ferritic–martensitic steel</atitle><jtitle>Materials &amp; design</jtitle><date>2016-02-15</date><risdate>2016</risdate><volume>92</volume><spage>200</spage><epage>212</epage><pages>200-212</pages><issn>0264-1275</issn><eissn>1873-4197</eissn><abstract>Bead-on-plate friction stir welding was conducted on 6mm thick plate of Reduced Activation Ferritic–Martensitic Steel employing polycrystalline cubic boron nitride tool with rotational speeds of 200, 300, 500 and 700rpm and traverse speed of 30mm/min. The interface temperature between shoulder bottom and top surface of the plate was monitored by non-contact in-line thermography which served to identify the peak temperature attained in the stir zone (SZ). This temperature for 200, 300 and 500, and 700rpm was respectively below Ac1, between Ac1 and Ac3, and above Ac3. In the base metal (BM), the prior austenite grain and martensite lath boundaries were decorated with chromium and tungsten rich M23C6 precipitates while intra-lath regions revealed Ta and V rich MX type carbides. Rotational speeds greater than 300rpm led to martensite formation and simultaneous recovery, recrystallization and grain growth in SZs with wide distribution in grain size whereas SZ of 200rpm and BM possessed similar distribution. The grain boundary M23C6 dissolved and very fine needles of Fe3C precipitated in all SZs. The hardness of all SZs was unacceptably higher compared to the BM. The 200rpm weld exhibited higher impact toughness in the absence of martensite in SZ. [Display omitted] •Effects of rotational speed during friction stir welding of a ferritic–martensitic steel were investigated.•Distribution of grain size in stir zones varied as a function of rotational speed.•Grain boundary M23C6 precipitates were dissolved while Fe3C formed in stir zones at all rotational speeds.•High rotational speeds promoted martensite occurrence in the stir zones with a drastic reduction in impact toughness.•Peak temperatures below Ac1 in the stir zone enabled impact toughness matching with the base metal.</abstract><pub>Elsevier Ltd</pub><doi>10.1016/j.matdes.2015.12.019</doi><tpages>13</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0264-1275
ispartof Materials & design, 2016-02, Vol.92, p.200-212
issn 0264-1275
1873-4197
language eng
recordid cdi_proquest_miscellaneous_1786151331
source Alma/SFX Local Collection
subjects Activation
Friction stir welding
Hardness
Interface temperature
Martensite
Mechanical properties
Microstructure
Needles
RAFM steel
Rotational
Steels
Stir zone
Tungsten
title A critical assessment of the microstructure and mechanical properties of friction stir welded reduced activation ferritic–martensitic steel
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-07T02%3A33%3A10IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=A%20critical%20assessment%20of%20the%20microstructure%20and%20mechanical%20properties%20of%20friction%20stir%20welded%20reduced%20activation%20ferritic%E2%80%93martensitic%20steel&rft.jtitle=Materials%20&%20design&rft.au=Manugula,%20Vijaya%20L.&rft.date=2016-02-15&rft.volume=92&rft.spage=200&rft.epage=212&rft.pages=200-212&rft.issn=0264-1275&rft.eissn=1873-4197&rft_id=info:doi/10.1016/j.matdes.2015.12.019&rft_dat=%3Cproquest_cross%3E1786151331%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=1786151331&rft_id=info:pmid/&rft_els_id=S0264127515308807&rfr_iscdi=true