Development and industrial application of ultra-fast cooling technology
A new-generation TMCP(NG-TMCP) with ultra fast cooling(UFC) as core technique was suggested instead of the convention- al TMCP in which some problems are to be solved. And the ultra fast cooling technology has been successfully applied to the plate rolling production in Shouqin Metal Materials Co. L...
Gespeichert in:
Veröffentlicht in: | Science China. Technological sciences 2012-06, Vol.55 (6), p.1566-1571 |
---|---|
Hauptverfasser: | , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | 1571 |
---|---|
container_issue | 6 |
container_start_page | 1566 |
container_title | Science China. Technological sciences |
container_volume | 55 |
creator | Tian, Yong Tang, Shuai Wang, BingXing Wang, ZhaoDong Wang, GuoDong |
description | A new-generation TMCP(NG-TMCP) with ultra fast cooling(UFC) as core technique was suggested instead of the convention- al TMCP in which some problems are to be solved. And the ultra fast cooling technology has been successfully applied to the plate rolling production in Shouqin Metal Materials Co. Ltd. Industrial trials are reported for the production of X70 pipeline steels (about 70000 t) under UFC conditions. Pipeline steels with reasonably good properties have been produced on an indus- trial scale. UFC can improve the temperature uniformity, the mechanical properties and the plate profile of X70 pipeline steel. The performance features of the trial plates can meet the standard of X70 pipeline steel. Spot test results have shown that the qualification rate of shape control, the performance and charpy impact properties for the trial plates are 95%, 97% and 98%, respectively. The impact values of X70 pipeline steel at UFC mode exceed the standard requirements of X80 pipeline steel. The productivity is enhanced because cutting quantity of head and tail of the plate is reduced. The enhancement of control ac- curacy of the red back temperatures is favorable for industrial production of X70 pipeline steel. The reduced production of the steel-making has been industrially achieved, since a new composition was designed by reducing the vanadium content to less than 0.045 wt.%. |
doi_str_mv | 10.1007/s11431-012-4744-6 |
format | Article |
fullrecord | <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_1753532845</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><cqvip_id>41802763</cqvip_id><sourcerecordid>1136381909</sourcerecordid><originalsourceid>FETCH-LOGICAL-c380t-9df67981af67312ac617359ca2e51c8f221e94d66f609cfd26869bc434434cb93</originalsourceid><addsrcrecordid>eNqFkDFPwzAQhSMEElXpD2ALG4vBZztOPKICBakSC8yW6zhpKtdO7QSp_x5XqRjhdNLd8N493Zdlt4AfAOPyMQIwCggDQaxkDPGLbAYVFwgExpdp5yVDJSVwnS1i3OFUtBIY2CxbPZtvY32_N27IlavzztVjHEKnbK763nZaDZ13uW_y0Q5BoUbFIdfe2861-WD01nnr2-NNdtUoG83iPOfZ1-vL5_INrT9W78unNdK0wgMSdcNLUYFKgwJRmkNJC6EVMQXoqiEEjGA15w3HQjc14emNjWaUpdYbQefZ_XS3D_4wmjjIfRe1sVY548cooSxoQUnFiv-lQDmtEqLTVZikOvgYg2lkH7q9CkcJWJ4QywmxTIjlCbHkyUMmT0xa15ogd34MLj3_p-nuHLT1rj0k328SgwqTklP6A-qKiKg</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1136381909</pqid></control><display><type>article</type><title>Development and industrial application of ultra-fast cooling technology</title><source>Alma/SFX Local Collection</source><source>SpringerLink Journals - AutoHoldings</source><creator>Tian, Yong ; Tang, Shuai ; Wang, BingXing ; Wang, ZhaoDong ; Wang, GuoDong</creator><creatorcontrib>Tian, Yong ; Tang, Shuai ; Wang, BingXing ; Wang, ZhaoDong ; Wang, GuoDong</creatorcontrib><description>A new-generation TMCP(NG-TMCP) with ultra fast cooling(UFC) as core technique was suggested instead of the convention- al TMCP in which some problems are to be solved. And the ultra fast cooling technology has been successfully applied to the plate rolling production in Shouqin Metal Materials Co. Ltd. Industrial trials are reported for the production of X70 pipeline steels (about 70000 t) under UFC conditions. Pipeline steels with reasonably good properties have been produced on an indus- trial scale. UFC can improve the temperature uniformity, the mechanical properties and the plate profile of X70 pipeline steel. The performance features of the trial plates can meet the standard of X70 pipeline steel. Spot test results have shown that the qualification rate of shape control, the performance and charpy impact properties for the trial plates are 95%, 97% and 98%, respectively. The impact values of X70 pipeline steel at UFC mode exceed the standard requirements of X80 pipeline steel. The productivity is enhanced because cutting quantity of head and tail of the plate is reduced. The enhancement of control ac- curacy of the red back temperatures is favorable for industrial production of X70 pipeline steel. The reduced production of the steel-making has been industrially achieved, since a new composition was designed by reducing the vanadium content to less than 0.045 wt.%.</description><identifier>ISSN: 1674-7321</identifier><identifier>EISSN: 1869-1900</identifier><identifier>DOI: 10.1007/s11431-012-4744-6</identifier><language>eng</language><publisher>Heidelberg: SP Science China Press</publisher><subject>Cooling ; Cutting ; Engineering ; High strength low alloy steels ; Impact tests ; Iron and steel making ; Pipelines ; Steels ; X70管线钢 ; X80管线钢 ; 力学性能 ; 工业应用 ; 工业生产 ; 快速冷却技术 ; 板形控制 ; 试验报告</subject><ispartof>Science China. Technological sciences, 2012-06, Vol.55 (6), p.1566-1571</ispartof><rights>Science China Press and Springer-Verlag Berlin Heidelberg 2012</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c380t-9df67981af67312ac617359ca2e51c8f221e94d66f609cfd26869bc434434cb93</citedby><cites>FETCH-LOGICAL-c380t-9df67981af67312ac617359ca2e51c8f221e94d66f609cfd26869bc434434cb93</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Uhttp://image.cqvip.com/vip1000/qk/60110X/60110X.jpg</thumbnail><linktopdf>$$Uhttps://link.springer.com/content/pdf/10.1007/s11431-012-4744-6$$EPDF$$P50$$Gspringer$$H</linktopdf><linktohtml>$$Uhttps://link.springer.com/10.1007/s11431-012-4744-6$$EHTML$$P50$$Gspringer$$H</linktohtml><link.rule.ids>314,780,784,27924,27925,41488,42557,51319</link.rule.ids></links><search><creatorcontrib>Tian, Yong</creatorcontrib><creatorcontrib>Tang, Shuai</creatorcontrib><creatorcontrib>Wang, BingXing</creatorcontrib><creatorcontrib>Wang, ZhaoDong</creatorcontrib><creatorcontrib>Wang, GuoDong</creatorcontrib><title>Development and industrial application of ultra-fast cooling technology</title><title>Science China. Technological sciences</title><addtitle>Sci. China Technol. Sci</addtitle><addtitle>SCIENCE CHINA Technological Sciences</addtitle><description>A new-generation TMCP(NG-TMCP) with ultra fast cooling(UFC) as core technique was suggested instead of the convention- al TMCP in which some problems are to be solved. And the ultra fast cooling technology has been successfully applied to the plate rolling production in Shouqin Metal Materials Co. Ltd. Industrial trials are reported for the production of X70 pipeline steels (about 70000 t) under UFC conditions. Pipeline steels with reasonably good properties have been produced on an indus- trial scale. UFC can improve the temperature uniformity, the mechanical properties and the plate profile of X70 pipeline steel. The performance features of the trial plates can meet the standard of X70 pipeline steel. Spot test results have shown that the qualification rate of shape control, the performance and charpy impact properties for the trial plates are 95%, 97% and 98%, respectively. The impact values of X70 pipeline steel at UFC mode exceed the standard requirements of X80 pipeline steel. The productivity is enhanced because cutting quantity of head and tail of the plate is reduced. The enhancement of control ac- curacy of the red back temperatures is favorable for industrial production of X70 pipeline steel. The reduced production of the steel-making has been industrially achieved, since a new composition was designed by reducing the vanadium content to less than 0.045 wt.%.</description><subject>Cooling</subject><subject>Cutting</subject><subject>Engineering</subject><subject>High strength low alloy steels</subject><subject>Impact tests</subject><subject>Iron and steel making</subject><subject>Pipelines</subject><subject>Steels</subject><subject>X70管线钢</subject><subject>X80管线钢</subject><subject>力学性能</subject><subject>工业应用</subject><subject>工业生产</subject><subject>快速冷却技术</subject><subject>板形控制</subject><subject>试验报告</subject><issn>1674-7321</issn><issn>1869-1900</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2012</creationdate><recordtype>article</recordtype><recordid>eNqFkDFPwzAQhSMEElXpD2ALG4vBZztOPKICBakSC8yW6zhpKtdO7QSp_x5XqRjhdNLd8N493Zdlt4AfAOPyMQIwCggDQaxkDPGLbAYVFwgExpdp5yVDJSVwnS1i3OFUtBIY2CxbPZtvY32_N27IlavzztVjHEKnbK763nZaDZ13uW_y0Q5BoUbFIdfe2861-WD01nnr2-NNdtUoG83iPOfZ1-vL5_INrT9W78unNdK0wgMSdcNLUYFKgwJRmkNJC6EVMQXoqiEEjGA15w3HQjc14emNjWaUpdYbQefZ_XS3D_4wmjjIfRe1sVY548cooSxoQUnFiv-lQDmtEqLTVZikOvgYg2lkH7q9CkcJWJ4QywmxTIjlCbHkyUMmT0xa15ogd34MLj3_p-nuHLT1rj0k328SgwqTklP6A-qKiKg</recordid><startdate>20120601</startdate><enddate>20120601</enddate><creator>Tian, Yong</creator><creator>Tang, Shuai</creator><creator>Wang, BingXing</creator><creator>Wang, ZhaoDong</creator><creator>Wang, GuoDong</creator><general>SP Science China Press</general><scope>2RA</scope><scope>92L</scope><scope>CQIGP</scope><scope>W92</scope><scope>~WA</scope><scope>AAYXX</scope><scope>CITATION</scope><scope>7SR</scope><scope>7TB</scope><scope>8BQ</scope><scope>8FD</scope><scope>FR3</scope><scope>JG9</scope><scope>KR7</scope></search><sort><creationdate>20120601</creationdate><title>Development and industrial application of ultra-fast cooling technology</title><author>Tian, Yong ; Tang, Shuai ; Wang, BingXing ; Wang, ZhaoDong ; Wang, GuoDong</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c380t-9df67981af67312ac617359ca2e51c8f221e94d66f609cfd26869bc434434cb93</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2012</creationdate><topic>Cooling</topic><topic>Cutting</topic><topic>Engineering</topic><topic>High strength low alloy steels</topic><topic>Impact tests</topic><topic>Iron and steel making</topic><topic>Pipelines</topic><topic>Steels</topic><topic>X70管线钢</topic><topic>X80管线钢</topic><topic>力学性能</topic><topic>工业应用</topic><topic>工业生产</topic><topic>快速冷却技术</topic><topic>板形控制</topic><topic>试验报告</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Tian, Yong</creatorcontrib><creatorcontrib>Tang, Shuai</creatorcontrib><creatorcontrib>Wang, BingXing</creatorcontrib><creatorcontrib>Wang, ZhaoDong</creatorcontrib><creatorcontrib>Wang, GuoDong</creatorcontrib><collection>中文科技期刊数据库</collection><collection>中文科技期刊数据库-CALIS站点</collection><collection>中文科技期刊数据库-7.0平台</collection><collection>中文科技期刊数据库-工程技术</collection><collection>中文科技期刊数据库- 镜像站点</collection><collection>CrossRef</collection><collection>Engineered Materials Abstracts</collection><collection>Mechanical & Transportation Engineering Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Engineering Research Database</collection><collection>Materials Research Database</collection><collection>Civil Engineering Abstracts</collection><jtitle>Science China. Technological sciences</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Tian, Yong</au><au>Tang, Shuai</au><au>Wang, BingXing</au><au>Wang, ZhaoDong</au><au>Wang, GuoDong</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Development and industrial application of ultra-fast cooling technology</atitle><jtitle>Science China. Technological sciences</jtitle><stitle>Sci. China Technol. Sci</stitle><addtitle>SCIENCE CHINA Technological Sciences</addtitle><date>2012-06-01</date><risdate>2012</risdate><volume>55</volume><issue>6</issue><spage>1566</spage><epage>1571</epage><pages>1566-1571</pages><issn>1674-7321</issn><eissn>1869-1900</eissn><abstract>A new-generation TMCP(NG-TMCP) with ultra fast cooling(UFC) as core technique was suggested instead of the convention- al TMCP in which some problems are to be solved. And the ultra fast cooling technology has been successfully applied to the plate rolling production in Shouqin Metal Materials Co. Ltd. Industrial trials are reported for the production of X70 pipeline steels (about 70000 t) under UFC conditions. Pipeline steels with reasonably good properties have been produced on an indus- trial scale. UFC can improve the temperature uniformity, the mechanical properties and the plate profile of X70 pipeline steel. The performance features of the trial plates can meet the standard of X70 pipeline steel. Spot test results have shown that the qualification rate of shape control, the performance and charpy impact properties for the trial plates are 95%, 97% and 98%, respectively. The impact values of X70 pipeline steel at UFC mode exceed the standard requirements of X80 pipeline steel. The productivity is enhanced because cutting quantity of head and tail of the plate is reduced. The enhancement of control ac- curacy of the red back temperatures is favorable for industrial production of X70 pipeline steel. The reduced production of the steel-making has been industrially achieved, since a new composition was designed by reducing the vanadium content to less than 0.045 wt.%.</abstract><cop>Heidelberg</cop><pub>SP Science China Press</pub><doi>10.1007/s11431-012-4744-6</doi><tpages>6</tpages></addata></record> |
fulltext | fulltext |
identifier | ISSN: 1674-7321 |
ispartof | Science China. Technological sciences, 2012-06, Vol.55 (6), p.1566-1571 |
issn | 1674-7321 1869-1900 |
language | eng |
recordid | cdi_proquest_miscellaneous_1753532845 |
source | Alma/SFX Local Collection; SpringerLink Journals - AutoHoldings |
subjects | Cooling Cutting Engineering High strength low alloy steels Impact tests Iron and steel making Pipelines Steels X70管线钢 X80管线钢 力学性能 工业应用 工业生产 快速冷却技术 板形控制 试验报告 |
title | Development and industrial application of ultra-fast cooling technology |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-05T18%3A46%3A08IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Development%20and%20industrial%20application%20of%20ultra-fast%20cooling%20technology&rft.jtitle=Science%20China.%20Technological%20sciences&rft.au=Tian,%20Yong&rft.date=2012-06-01&rft.volume=55&rft.issue=6&rft.spage=1566&rft.epage=1571&rft.pages=1566-1571&rft.issn=1674-7321&rft.eissn=1869-1900&rft_id=info:doi/10.1007/s11431-012-4744-6&rft_dat=%3Cproquest_cross%3E1136381909%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=1136381909&rft_id=info:pmid/&rft_cqvip_id=41802763&rfr_iscdi=true |