Fabrication of microporous calcite block from calcium hydroxide compact under carbon dioxide atmosphere at high temperature
Effects of carbonation temperature and compacting pressure on basic properties of calcite block were studied using Ca(OH)2 compact made with 0.2-2.0 MPa and their carbonation at 200-800ºC for 1 h. Microporous calcite was obtained only when carbonated at 600ºC using Ca(OH)2 compact made with 0.2 MPa...