Utilization of volcanic ashes for the production of geopolymers cured at ambient temperature

Two types of volcanic ash were characterized (chemical and mineralogical compositions, amorphous phase composition, particle size distribution and specific surface area) and then used as raw materials for the synthesis of geopolymer cements cured at ambient temperature (24±3°C). The synthesized prod...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Cement & concrete composites 2013-04, Vol.38, p.75-81
Hauptverfasser: Tchakoute, H.K., Elimbi, A., Yanne, E., Djangang, C.N.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 81
container_issue
container_start_page 75
container_title Cement & concrete composites
container_volume 38
creator Tchakoute, H.K.
Elimbi, A.
Yanne, E.
Djangang, C.N.
description Two types of volcanic ash were characterized (chemical and mineralogical compositions, amorphous phase composition, particle size distribution and specific surface area) and then used as raw materials for the synthesis of geopolymer cements cured at ambient temperature (24±3°C). The synthesized products were characterized by determination of setting time, 28-day compressive strength, X-ray diffraction and Fourier Transform Infrared Spectroscopy. The mineralogical composition, the amorphous phase composition, the particle size distribution, the specific surface area of the volcanic ashes as well as the molar ratios of Na2O/Al2O3 of the synthesized products and of SiO2/Na2O of the alkaline solutions were the main parameters which influenced the synthesis of geopolymers with attractive characteristics at ambient curing temperature. The volcanic ash sample whose mineralogical composition contained anhydrite, low content of free CaO, low specific surface area (2.3m2/g) and synthesized products with Na2O/Al2O3 molar ratios between 1.23 and 1.44 led to long setting time (test samples could be handled easily only after 14days at ambient atmosphere of the laboratory) and low 28-day compressive strength (9–19MPa) geopolymers. Moreover, its products swelled and presented cracks resulting from the formation of ettringite. The volcanic ash sample with large (Al2O3+SiO2)% wt of amorphous phase, high specific surface area (15.7m2/g) and synthesized products with Na2O/Al2O3 molar ratios between 1.04 and 1.31 led to more effective geopolymers: setting time was between 490 and 180min and 28-day compressive strength between 23 and 50MPa at ambient curing temperature (24±3°C).
doi_str_mv 10.1016/j.cemconcomp.2013.03.010
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_1730117187</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0958946513000292</els_id><sourcerecordid>1365153912</sourcerecordid><originalsourceid>FETCH-LOGICAL-c384t-ceeb0ff2dd60256b14eafb354270ecdab62113662dfb6b6aece3ca3406c427df3</originalsourceid><addsrcrecordid>eNqFkE1rGzEQhkVJoY7b_6BjL-uMVrta-9iG5gMCudTQQ0FoR6NaZne1lWSD8-sr44YcAwMDw_MOMw9jXMBKgFA3-xXSiGHCMM6rGoRcQSkBH9hCrDtZyY38dcUWsGnX1aZR7Sd2ndIeAFTT1Qv2e5v94F9M9mHiwfFjGNBMHrlJO0rchcjzjvgcgz3gK_SHwhyG00gxcTxEstxkbsbe05R5pnGmaHKZf2YfnRkSffnfl2x79-Pn7UP19Hz_ePvtqUK5bnKFRD04V1uroG5VLxoyrpdtU3dAaE2vaiGkUrV1veqVISSJRjagsCDWySX7etlbzvx7oJT16BPSMJiJwiFp0UkQojv7eBeVqhWt3Ii6oOsLijGkFMnpOfrRxJMWoM_u9V6_uddn9xpKCSjR75cola-PnqJOWOQgWR8Js7bBv7_kH4DNlNs</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1365153912</pqid></control><display><type>article</type><title>Utilization of volcanic ashes for the production of geopolymers cured at ambient temperature</title><source>Access via ScienceDirect (Elsevier)</source><creator>Tchakoute, H.K. ; Elimbi, A. ; Yanne, E. ; Djangang, C.N.</creator><creatorcontrib>Tchakoute, H.K. ; Elimbi, A. ; Yanne, E. ; Djangang, C.N.</creatorcontrib><description>Two types of volcanic ash were characterized (chemical and mineralogical compositions, amorphous phase composition, particle size distribution and specific surface area) and then used as raw materials for the synthesis of geopolymer cements cured at ambient temperature (24±3°C). The synthesized products were characterized by determination of setting time, 28-day compressive strength, X-ray diffraction and Fourier Transform Infrared Spectroscopy. The mineralogical composition, the amorphous phase composition, the particle size distribution, the specific surface area of the volcanic ashes as well as the molar ratios of Na2O/Al2O3 of the synthesized products and of SiO2/Na2O of the alkaline solutions were the main parameters which influenced the synthesis of geopolymers with attractive characteristics at ambient curing temperature. The volcanic ash sample whose mineralogical composition contained anhydrite, low content of free CaO, low specific surface area (2.3m2/g) and synthesized products with Na2O/Al2O3 molar ratios between 1.23 and 1.44 led to long setting time (test samples could be handled easily only after 14days at ambient atmosphere of the laboratory) and low 28-day compressive strength (9–19MPa) geopolymers. Moreover, its products swelled and presented cracks resulting from the formation of ettringite. The volcanic ash sample with large (Al2O3+SiO2)% wt of amorphous phase, high specific surface area (15.7m2/g) and synthesized products with Na2O/Al2O3 molar ratios between 1.04 and 1.31 led to more effective geopolymers: setting time was between 490 and 180min and 28-day compressive strength between 23 and 50MPa at ambient curing temperature (24±3°C).</description><identifier>ISSN: 0958-9465</identifier><identifier>EISSN: 1873-393X</identifier><identifier>DOI: 10.1016/j.cemconcomp.2013.03.010</identifier><language>eng</language><publisher>Elsevier Ltd</publisher><subject>Alkaline solution ; Aluminum oxide ; Ambient curing temperature ; Amorphous phase ; Cements ; Compressive strength ; Curing ; Geopolymer ; Phase composition ; Specific surface ; Synthesis ; Volcanic ash</subject><ispartof>Cement &amp; concrete composites, 2013-04, Vol.38, p.75-81</ispartof><rights>2013 Elsevier Ltd</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c384t-ceeb0ff2dd60256b14eafb354270ecdab62113662dfb6b6aece3ca3406c427df3</citedby><cites>FETCH-LOGICAL-c384t-ceeb0ff2dd60256b14eafb354270ecdab62113662dfb6b6aece3ca3406c427df3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://dx.doi.org/10.1016/j.cemconcomp.2013.03.010$$EHTML$$P50$$Gelsevier$$H</linktohtml><link.rule.ids>314,780,784,3550,27924,27925,45995</link.rule.ids></links><search><creatorcontrib>Tchakoute, H.K.</creatorcontrib><creatorcontrib>Elimbi, A.</creatorcontrib><creatorcontrib>Yanne, E.</creatorcontrib><creatorcontrib>Djangang, C.N.</creatorcontrib><title>Utilization of volcanic ashes for the production of geopolymers cured at ambient temperature</title><title>Cement &amp; concrete composites</title><description>Two types of volcanic ash were characterized (chemical and mineralogical compositions, amorphous phase composition, particle size distribution and specific surface area) and then used as raw materials for the synthesis of geopolymer cements cured at ambient temperature (24±3°C). The synthesized products were characterized by determination of setting time, 28-day compressive strength, X-ray diffraction and Fourier Transform Infrared Spectroscopy. The mineralogical composition, the amorphous phase composition, the particle size distribution, the specific surface area of the volcanic ashes as well as the molar ratios of Na2O/Al2O3 of the synthesized products and of SiO2/Na2O of the alkaline solutions were the main parameters which influenced the synthesis of geopolymers with attractive characteristics at ambient curing temperature. The volcanic ash sample whose mineralogical composition contained anhydrite, low content of free CaO, low specific surface area (2.3m2/g) and synthesized products with Na2O/Al2O3 molar ratios between 1.23 and 1.44 led to long setting time (test samples could be handled easily only after 14days at ambient atmosphere of the laboratory) and low 28-day compressive strength (9–19MPa) geopolymers. Moreover, its products swelled and presented cracks resulting from the formation of ettringite. The volcanic ash sample with large (Al2O3+SiO2)% wt of amorphous phase, high specific surface area (15.7m2/g) and synthesized products with Na2O/Al2O3 molar ratios between 1.04 and 1.31 led to more effective geopolymers: setting time was between 490 and 180min and 28-day compressive strength between 23 and 50MPa at ambient curing temperature (24±3°C).</description><subject>Alkaline solution</subject><subject>Aluminum oxide</subject><subject>Ambient curing temperature</subject><subject>Amorphous phase</subject><subject>Cements</subject><subject>Compressive strength</subject><subject>Curing</subject><subject>Geopolymer</subject><subject>Phase composition</subject><subject>Specific surface</subject><subject>Synthesis</subject><subject>Volcanic ash</subject><issn>0958-9465</issn><issn>1873-393X</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2013</creationdate><recordtype>article</recordtype><recordid>eNqFkE1rGzEQhkVJoY7b_6BjL-uMVrta-9iG5gMCudTQQ0FoR6NaZne1lWSD8-sr44YcAwMDw_MOMw9jXMBKgFA3-xXSiGHCMM6rGoRcQSkBH9hCrDtZyY38dcUWsGnX1aZR7Sd2ndIeAFTT1Qv2e5v94F9M9mHiwfFjGNBMHrlJO0rchcjzjvgcgz3gK_SHwhyG00gxcTxEstxkbsbe05R5pnGmaHKZf2YfnRkSffnfl2x79-Pn7UP19Hz_ePvtqUK5bnKFRD04V1uroG5VLxoyrpdtU3dAaE2vaiGkUrV1veqVISSJRjagsCDWySX7etlbzvx7oJT16BPSMJiJwiFp0UkQojv7eBeVqhWt3Ii6oOsLijGkFMnpOfrRxJMWoM_u9V6_uddn9xpKCSjR75cola-PnqJOWOQgWR8Js7bBv7_kH4DNlNs</recordid><startdate>201304</startdate><enddate>201304</enddate><creator>Tchakoute, H.K.</creator><creator>Elimbi, A.</creator><creator>Yanne, E.</creator><creator>Djangang, C.N.</creator><general>Elsevier Ltd</general><scope>AAYXX</scope><scope>CITATION</scope><scope>7UA</scope><scope>C1K</scope><scope>F1W</scope><scope>H96</scope><scope>L.G</scope><scope>7QQ</scope><scope>7SR</scope><scope>8FD</scope><scope>FR3</scope><scope>JG9</scope><scope>KR7</scope></search><sort><creationdate>201304</creationdate><title>Utilization of volcanic ashes for the production of geopolymers cured at ambient temperature</title><author>Tchakoute, H.K. ; Elimbi, A. ; Yanne, E. ; Djangang, C.N.</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c384t-ceeb0ff2dd60256b14eafb354270ecdab62113662dfb6b6aece3ca3406c427df3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2013</creationdate><topic>Alkaline solution</topic><topic>Aluminum oxide</topic><topic>Ambient curing temperature</topic><topic>Amorphous phase</topic><topic>Cements</topic><topic>Compressive strength</topic><topic>Curing</topic><topic>Geopolymer</topic><topic>Phase composition</topic><topic>Specific surface</topic><topic>Synthesis</topic><topic>Volcanic ash</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Tchakoute, H.K.</creatorcontrib><creatorcontrib>Elimbi, A.</creatorcontrib><creatorcontrib>Yanne, E.</creatorcontrib><creatorcontrib>Djangang, C.N.</creatorcontrib><collection>CrossRef</collection><collection>Water Resources Abstracts</collection><collection>Environmental Sciences and Pollution Management</collection><collection>ASFA: Aquatic Sciences and Fisheries Abstracts</collection><collection>Aquatic Science &amp; Fisheries Abstracts (ASFA) 2: Ocean Technology, Policy &amp; Non-Living Resources</collection><collection>Aquatic Science &amp; Fisheries Abstracts (ASFA) Professional</collection><collection>Ceramic Abstracts</collection><collection>Engineered Materials Abstracts</collection><collection>Technology Research Database</collection><collection>Engineering Research Database</collection><collection>Materials Research Database</collection><collection>Civil Engineering Abstracts</collection><jtitle>Cement &amp; concrete composites</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Tchakoute, H.K.</au><au>Elimbi, A.</au><au>Yanne, E.</au><au>Djangang, C.N.</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Utilization of volcanic ashes for the production of geopolymers cured at ambient temperature</atitle><jtitle>Cement &amp; concrete composites</jtitle><date>2013-04</date><risdate>2013</risdate><volume>38</volume><spage>75</spage><epage>81</epage><pages>75-81</pages><issn>0958-9465</issn><eissn>1873-393X</eissn><abstract>Two types of volcanic ash were characterized (chemical and mineralogical compositions, amorphous phase composition, particle size distribution and specific surface area) and then used as raw materials for the synthesis of geopolymer cements cured at ambient temperature (24±3°C). The synthesized products were characterized by determination of setting time, 28-day compressive strength, X-ray diffraction and Fourier Transform Infrared Spectroscopy. The mineralogical composition, the amorphous phase composition, the particle size distribution, the specific surface area of the volcanic ashes as well as the molar ratios of Na2O/Al2O3 of the synthesized products and of SiO2/Na2O of the alkaline solutions were the main parameters which influenced the synthesis of geopolymers with attractive characteristics at ambient curing temperature. The volcanic ash sample whose mineralogical composition contained anhydrite, low content of free CaO, low specific surface area (2.3m2/g) and synthesized products with Na2O/Al2O3 molar ratios between 1.23 and 1.44 led to long setting time (test samples could be handled easily only after 14days at ambient atmosphere of the laboratory) and low 28-day compressive strength (9–19MPa) geopolymers. Moreover, its products swelled and presented cracks resulting from the formation of ettringite. The volcanic ash sample with large (Al2O3+SiO2)% wt of amorphous phase, high specific surface area (15.7m2/g) and synthesized products with Na2O/Al2O3 molar ratios between 1.04 and 1.31 led to more effective geopolymers: setting time was between 490 and 180min and 28-day compressive strength between 23 and 50MPa at ambient curing temperature (24±3°C).</abstract><pub>Elsevier Ltd</pub><doi>10.1016/j.cemconcomp.2013.03.010</doi><tpages>7</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0958-9465
ispartof Cement & concrete composites, 2013-04, Vol.38, p.75-81
issn 0958-9465
1873-393X
language eng
recordid cdi_proquest_miscellaneous_1730117187
source Access via ScienceDirect (Elsevier)
subjects Alkaline solution
Aluminum oxide
Ambient curing temperature
Amorphous phase
Cements
Compressive strength
Curing
Geopolymer
Phase composition
Specific surface
Synthesis
Volcanic ash
title Utilization of volcanic ashes for the production of geopolymers cured at ambient temperature
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-18T18%3A17%3A07IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Utilization%20of%20volcanic%20ashes%20for%20the%20production%20of%20geopolymers%20cured%20at%20ambient%20temperature&rft.jtitle=Cement%20&%20concrete%20composites&rft.au=Tchakoute,%20H.K.&rft.date=2013-04&rft.volume=38&rft.spage=75&rft.epage=81&rft.pages=75-81&rft.issn=0958-9465&rft.eissn=1873-393X&rft_id=info:doi/10.1016/j.cemconcomp.2013.03.010&rft_dat=%3Cproquest_cross%3E1365153912%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=1365153912&rft_id=info:pmid/&rft_els_id=S0958946513000292&rfr_iscdi=true