Heat treatment of 6H-SiC under different gaseous environments
Silicon carbide is a useful material for the reactors in chemical processes. In recent years, microreactors have gained significant attentions due to the high demand for process miniaturization. As heat and mass-transfer are highly improved inside the gas flow channels in microreactors, any change o...
Gespeichert in:
Veröffentlicht in: | Ceramics international 2014-04, Vol.40 (3), p.4149-4154 |
---|---|
Hauptverfasser: | , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | 4154 |
---|---|
container_issue | 3 |
container_start_page | 4149 |
container_title | Ceramics international |
container_volume | 40 |
creator | Lee, Woo Jin Li, Chaoen Burke, Nick Patel, Jim Wilson, Merrill Gerdes, Karl |
description | Silicon carbide is a useful material for the reactors in chemical processes. In recent years, microreactors have gained significant attentions due to the high demand for process miniaturization. As heat and mass-transfer are highly improved inside the gas flow channels in microreactors, any change on the surface of inner channels under heating becomes critical to the performance of microreactors. To investigate the surface changes of silicon carbide during the heat treatment, 6H-SiC coupons were processed in five different gases—Ar, N2, air, 0.9% O2 in Ar and 50% H2O in air—that are commonly encountered in high temperature chemical processes. While the formation of oxide film was found to be dependent on the partial pressure of oxidizing gas, surface decomposition was found from the treatment in nitrogen environment. Characterization of the SiC surface by Raman spectroscopy and SEM–EDX revealed that a graphitic layer has formed at the oxide film/SiC interface. Crystallinity of graphitic layer at the interface seemed to be dependent on the partial pressure of oxidizing gas, which was revealed by the relationship between G peak position and R(ID/IG). The intensity ratio of FTO(0)/FTO(2/6) bands showed that stacking faults on the surface of SiC coupons were reduced after heat treatment. |
doi_str_mv | 10.1016/j.ceramint.2013.08.071 |
format | Article |
fullrecord | <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_1692380140</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0272884213010298</els_id><sourcerecordid>1541431648</sourcerecordid><originalsourceid>FETCH-LOGICAL-c415t-44f22283986b15dd99410354beaf041faa32eb65f326785cef3ac3f961ed6faf3</originalsourceid><addsrcrecordid>eNqFkE9LAzEQxYMoWKtfQfboZddM_m32IChFrVDwoJ5Dmkwkpbtbk23Bb-8u1bOXmcP83mPeI-QaaAUU1O2mcphsG7uhYhR4RXVFazghM9A1L3kj1SmZUVazUmvBzslFzhs6ChtBZ-RuiXYohjTOFruh6EOhluVbXBT7zmMqfAwB03T5tBn7fS6wO8TUdxOdL8lZsNuMV797Tj6eHt8Xy3L1-vyyeFiVToAcSiECY0zzRqs1SO-bRgDlUqzRBiogWMsZrpUMnKlaS4eBW8dDowC9CjbwObk5-u5S_7XHPJg2Zofbre2mn8wYhnFNQdD_USlAcFBCj6g6oi71OScMZpdia9O3AWqmas3G_FVrpmoN1WasdhTeH4U4Zj5ETCa7iJ1DHxO6wfg-_mfxA0rdhMI</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1541431648</pqid></control><display><type>article</type><title>Heat treatment of 6H-SiC under different gaseous environments</title><source>ScienceDirect Journals (5 years ago - present)</source><creator>Lee, Woo Jin ; Li, Chaoen ; Burke, Nick ; Patel, Jim ; Wilson, Merrill ; Gerdes, Karl</creator><creatorcontrib>Lee, Woo Jin ; Li, Chaoen ; Burke, Nick ; Patel, Jim ; Wilson, Merrill ; Gerdes, Karl</creatorcontrib><description>Silicon carbide is a useful material for the reactors in chemical processes. In recent years, microreactors have gained significant attentions due to the high demand for process miniaturization. As heat and mass-transfer are highly improved inside the gas flow channels in microreactors, any change on the surface of inner channels under heating becomes critical to the performance of microreactors. To investigate the surface changes of silicon carbide during the heat treatment, 6H-SiC coupons were processed in five different gases—Ar, N2, air, 0.9% O2 in Ar and 50% H2O in air—that are commonly encountered in high temperature chemical processes. While the formation of oxide film was found to be dependent on the partial pressure of oxidizing gas, surface decomposition was found from the treatment in nitrogen environment. Characterization of the SiC surface by Raman spectroscopy and SEM–EDX revealed that a graphitic layer has formed at the oxide film/SiC interface. Crystallinity of graphitic layer at the interface seemed to be dependent on the partial pressure of oxidizing gas, which was revealed by the relationship between G peak position and R(ID/IG). The intensity ratio of FTO(0)/FTO(2/6) bands showed that stacking faults on the surface of SiC coupons were reduced after heat treatment.</description><identifier>ISSN: 0272-8842</identifier><identifier>EISSN: 1873-3956</identifier><identifier>DOI: 10.1016/j.ceramint.2013.08.071</identifier><language>eng</language><publisher>Elsevier Ltd</publisher><subject>B. Interfaces ; Bands ; Ceramics ; Crystallinity ; D. Silicon carbides ; Heat treatment ; Oxide coatings ; Partial pressure ; Raman spectroscopy ; Silicon carbide</subject><ispartof>Ceramics international, 2014-04, Vol.40 (3), p.4149-4154</ispartof><rights>2013</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c415t-44f22283986b15dd99410354beaf041faa32eb65f326785cef3ac3f961ed6faf3</citedby><cites>FETCH-LOGICAL-c415t-44f22283986b15dd99410354beaf041faa32eb65f326785cef3ac3f961ed6faf3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://dx.doi.org/10.1016/j.ceramint.2013.08.071$$EHTML$$P50$$Gelsevier$$H</linktohtml><link.rule.ids>314,780,784,3550,27924,27925,45995</link.rule.ids></links><search><creatorcontrib>Lee, Woo Jin</creatorcontrib><creatorcontrib>Li, Chaoen</creatorcontrib><creatorcontrib>Burke, Nick</creatorcontrib><creatorcontrib>Patel, Jim</creatorcontrib><creatorcontrib>Wilson, Merrill</creatorcontrib><creatorcontrib>Gerdes, Karl</creatorcontrib><title>Heat treatment of 6H-SiC under different gaseous environments</title><title>Ceramics international</title><description>Silicon carbide is a useful material for the reactors in chemical processes. In recent years, microreactors have gained significant attentions due to the high demand for process miniaturization. As heat and mass-transfer are highly improved inside the gas flow channels in microreactors, any change on the surface of inner channels under heating becomes critical to the performance of microreactors. To investigate the surface changes of silicon carbide during the heat treatment, 6H-SiC coupons were processed in five different gases—Ar, N2, air, 0.9% O2 in Ar and 50% H2O in air—that are commonly encountered in high temperature chemical processes. While the formation of oxide film was found to be dependent on the partial pressure of oxidizing gas, surface decomposition was found from the treatment in nitrogen environment. Characterization of the SiC surface by Raman spectroscopy and SEM–EDX revealed that a graphitic layer has formed at the oxide film/SiC interface. Crystallinity of graphitic layer at the interface seemed to be dependent on the partial pressure of oxidizing gas, which was revealed by the relationship between G peak position and R(ID/IG). The intensity ratio of FTO(0)/FTO(2/6) bands showed that stacking faults on the surface of SiC coupons were reduced after heat treatment.</description><subject>B. Interfaces</subject><subject>Bands</subject><subject>Ceramics</subject><subject>Crystallinity</subject><subject>D. Silicon carbides</subject><subject>Heat treatment</subject><subject>Oxide coatings</subject><subject>Partial pressure</subject><subject>Raman spectroscopy</subject><subject>Silicon carbide</subject><issn>0272-8842</issn><issn>1873-3956</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2014</creationdate><recordtype>article</recordtype><recordid>eNqFkE9LAzEQxYMoWKtfQfboZddM_m32IChFrVDwoJ5Dmkwkpbtbk23Bb-8u1bOXmcP83mPeI-QaaAUU1O2mcphsG7uhYhR4RXVFazghM9A1L3kj1SmZUVazUmvBzslFzhs6ChtBZ-RuiXYohjTOFruh6EOhluVbXBT7zmMqfAwB03T5tBn7fS6wO8TUdxOdL8lZsNuMV797Tj6eHt8Xy3L1-vyyeFiVToAcSiECY0zzRqs1SO-bRgDlUqzRBiogWMsZrpUMnKlaS4eBW8dDowC9CjbwObk5-u5S_7XHPJg2Zofbre2mn8wYhnFNQdD_USlAcFBCj6g6oi71OScMZpdia9O3AWqmas3G_FVrpmoN1WasdhTeH4U4Zj5ETCa7iJ1DHxO6wfg-_mfxA0rdhMI</recordid><startdate>20140401</startdate><enddate>20140401</enddate><creator>Lee, Woo Jin</creator><creator>Li, Chaoen</creator><creator>Burke, Nick</creator><creator>Patel, Jim</creator><creator>Wilson, Merrill</creator><creator>Gerdes, Karl</creator><general>Elsevier Ltd</general><scope>AAYXX</scope><scope>CITATION</scope><scope>7QQ</scope><scope>7SR</scope><scope>7U5</scope><scope>8FD</scope><scope>JG9</scope><scope>L7M</scope></search><sort><creationdate>20140401</creationdate><title>Heat treatment of 6H-SiC under different gaseous environments</title><author>Lee, Woo Jin ; Li, Chaoen ; Burke, Nick ; Patel, Jim ; Wilson, Merrill ; Gerdes, Karl</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c415t-44f22283986b15dd99410354beaf041faa32eb65f326785cef3ac3f961ed6faf3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2014</creationdate><topic>B. Interfaces</topic><topic>Bands</topic><topic>Ceramics</topic><topic>Crystallinity</topic><topic>D. Silicon carbides</topic><topic>Heat treatment</topic><topic>Oxide coatings</topic><topic>Partial pressure</topic><topic>Raman spectroscopy</topic><topic>Silicon carbide</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Lee, Woo Jin</creatorcontrib><creatorcontrib>Li, Chaoen</creatorcontrib><creatorcontrib>Burke, Nick</creatorcontrib><creatorcontrib>Patel, Jim</creatorcontrib><creatorcontrib>Wilson, Merrill</creatorcontrib><creatorcontrib>Gerdes, Karl</creatorcontrib><collection>CrossRef</collection><collection>Ceramic Abstracts</collection><collection>Engineered Materials Abstracts</collection><collection>Solid State and Superconductivity Abstracts</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><collection>Advanced Technologies Database with Aerospace</collection><jtitle>Ceramics international</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Lee, Woo Jin</au><au>Li, Chaoen</au><au>Burke, Nick</au><au>Patel, Jim</au><au>Wilson, Merrill</au><au>Gerdes, Karl</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Heat treatment of 6H-SiC under different gaseous environments</atitle><jtitle>Ceramics international</jtitle><date>2014-04-01</date><risdate>2014</risdate><volume>40</volume><issue>3</issue><spage>4149</spage><epage>4154</epage><pages>4149-4154</pages><issn>0272-8842</issn><eissn>1873-3956</eissn><abstract>Silicon carbide is a useful material for the reactors in chemical processes. In recent years, microreactors have gained significant attentions due to the high demand for process miniaturization. As heat and mass-transfer are highly improved inside the gas flow channels in microreactors, any change on the surface of inner channels under heating becomes critical to the performance of microreactors. To investigate the surface changes of silicon carbide during the heat treatment, 6H-SiC coupons were processed in five different gases—Ar, N2, air, 0.9% O2 in Ar and 50% H2O in air—that are commonly encountered in high temperature chemical processes. While the formation of oxide film was found to be dependent on the partial pressure of oxidizing gas, surface decomposition was found from the treatment in nitrogen environment. Characterization of the SiC surface by Raman spectroscopy and SEM–EDX revealed that a graphitic layer has formed at the oxide film/SiC interface. Crystallinity of graphitic layer at the interface seemed to be dependent on the partial pressure of oxidizing gas, which was revealed by the relationship between G peak position and R(ID/IG). The intensity ratio of FTO(0)/FTO(2/6) bands showed that stacking faults on the surface of SiC coupons were reduced after heat treatment.</abstract><pub>Elsevier Ltd</pub><doi>10.1016/j.ceramint.2013.08.071</doi><tpages>6</tpages></addata></record> |
fulltext | fulltext |
identifier | ISSN: 0272-8842 |
ispartof | Ceramics international, 2014-04, Vol.40 (3), p.4149-4154 |
issn | 0272-8842 1873-3956 |
language | eng |
recordid | cdi_proquest_miscellaneous_1692380140 |
source | ScienceDirect Journals (5 years ago - present) |
subjects | B. Interfaces Bands Ceramics Crystallinity D. Silicon carbides Heat treatment Oxide coatings Partial pressure Raman spectroscopy Silicon carbide |
title | Heat treatment of 6H-SiC under different gaseous environments |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-07T01%3A18%3A45IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Heat%20treatment%20of%206H-SiC%20under%20different%20gaseous%20environments&rft.jtitle=Ceramics%20international&rft.au=Lee,%20Woo%20Jin&rft.date=2014-04-01&rft.volume=40&rft.issue=3&rft.spage=4149&rft.epage=4154&rft.pages=4149-4154&rft.issn=0272-8842&rft.eissn=1873-3956&rft_id=info:doi/10.1016/j.ceramint.2013.08.071&rft_dat=%3Cproquest_cross%3E1541431648%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=1541431648&rft_id=info:pmid/&rft_els_id=S0272884213010298&rfr_iscdi=true |