Slow Relaxation Processes in CCTO Detected by Capacitance Versus Voltage Curves

The temperature and frequency dependence of capacitance versus voltage (C–V) curves was investigated for ceramic CaCu3Ti4O12 samples sintered in atmospheres of vacuum, air and oxygen, respectively. A drastic capacitance rise at higher dc voltages and low ac frequencies was observed for all these CaC...