Influence of joining time and temperature on the flexural strength of joined boron carbide ceramics
The influence of the joining time and temperature on the flexural strength of B4C ceramics joined using an Al sheet was investigated. The B4C ceramics were joined over a temperature range 600–1400°C for 2–72 h in vacuum (10−2–10−4 Pa) and in an Ar atmosphere. A joining interlayer with a dense struct...