Analysis of fracture initiation angle in some cracked ceramics using the generalized maximum tangential stress criterion
Brittle fracture in ceramics sometimes occurs under combined opening-sliding (or mixed mode I/II) crack deformation. In this paper, a generalized maximum tangential stress criterion is employed for predicting the fracture initiation angle under mixed mode I/II loading in some brittle ceramics includ...
Gespeichert in:
Veröffentlicht in: | International journal of solids and structures 2012-06, Vol.49 (13), p.1877-1883 |
---|---|
Hauptverfasser: | , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | 1883 |
---|---|
container_issue | 13 |
container_start_page | 1877 |
container_title | International journal of solids and structures |
container_volume | 49 |
creator | Aliha, M.R.M. Ayatollahi, M.R. |
description | Brittle fracture in ceramics sometimes occurs under combined opening-sliding (or mixed mode I/II) crack deformation. In this paper, a generalized maximum tangential stress criterion is employed for predicting the fracture initiation angle under mixed mode I/II loading in some brittle ceramics including alumina, zirconia, soda lime glass and three silicon based ceramics. The experimental results reported for the fracture angles in these ceramics have been obtained from fracture tests on the centrally cracked circular disc (often called the Brazilian disc). Very good agreement is shown to exist between the experimental results and the theoretical predictions. According to the fracture model, the mixed mode fracture angle is strongly dependent on the elastic T-stress in the tested ceramics. The negative T-stress that exists in the Brazilian disc specimen can be the main influencing parameter for decreasing the fracture initiation angle in the investigated ceramics. |
doi_str_mv | 10.1016/j.ijsolstr.2012.03.029 |
format | Article |
fullrecord | <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_1671292014</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S002076831200131X</els_id><sourcerecordid>1671292014</sourcerecordid><originalsourceid>FETCH-LOGICAL-c393t-5bc9876af5dc499ea5c635dbae5e9db5e32edf1be4e0a881ee3afcf9e9f97de83</originalsourceid><addsrcrecordid>eNqFkMtu2zAQRYkgAeKk-YWCy26kkKJe3MUI-ggQIJt0TdDU0BlHolwOVdj5-tJwu-6KwPDeg5nD2GcpSilke78rcUfzSCmWlZBVKVQpKn3BVrLvdFHJur1kKyEqUXRtr67ZDdFOCFErLVbssA52PBISnz330bq0ROAYMKFNOAduw3Y8DTjNE3CXE-8wcAfRTuiIL4Rhy9Mb8C2EPBzxI39P9oDTMvGU2xAyauR5PSDKAEwQM_gTu_J2JLj7-96yn9--vj7-KJ5fvj89rp8Lp7RKRbNxuu9a65vB1VqDbVyrmmFjoQE9bBpQFQxebqAGYfteAijrndegve4G6NUt-3Lm7uP8awFKZkJyMI42wLyQkW0nK53F1TnanqMuzkQRvNlHnGw8GinMSbXZmX-qzUm1Ecpk1bn4cC5CPuQ3QjTkEIKDASO4ZIYZ_4f4AyaPkI4</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1671292014</pqid></control><display><type>article</type><title>Analysis of fracture initiation angle in some cracked ceramics using the generalized maximum tangential stress criterion</title><source>Elsevier ScienceDirect Journals Complete</source><source>Elektronische Zeitschriftenbibliothek - Frei zugängliche E-Journals</source><creator>Aliha, M.R.M. ; Ayatollahi, M.R.</creator><creatorcontrib>Aliha, M.R.M. ; Ayatollahi, M.R.</creatorcontrib><description>Brittle fracture in ceramics sometimes occurs under combined opening-sliding (or mixed mode I/II) crack deformation. In this paper, a generalized maximum tangential stress criterion is employed for predicting the fracture initiation angle under mixed mode I/II loading in some brittle ceramics including alumina, zirconia, soda lime glass and three silicon based ceramics. The experimental results reported for the fracture angles in these ceramics have been obtained from fracture tests on the centrally cracked circular disc (often called the Brazilian disc). Very good agreement is shown to exist between the experimental results and the theoretical predictions. According to the fracture model, the mixed mode fracture angle is strongly dependent on the elastic T-stress in the tested ceramics. The negative T-stress that exists in the Brazilian disc specimen can be the main influencing parameter for decreasing the fracture initiation angle in the investigated ceramics.</description><identifier>ISSN: 0020-7683</identifier><identifier>EISSN: 1879-2146</identifier><identifier>DOI: 10.1016/j.ijsolstr.2012.03.029</identifier><language>eng</language><publisher>Elsevier Ltd</publisher><subject>Brazil ; Brazilian disc specimen ; Ceramics ; Crack initiation ; Criteria ; Discs ; Disks ; Fracture initiation angle ; Fracture mechanics ; Mathematical models ; Mixed mode fracture</subject><ispartof>International journal of solids and structures, 2012-06, Vol.49 (13), p.1877-1883</ispartof><rights>2012 Elsevier Ltd</rights><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c393t-5bc9876af5dc499ea5c635dbae5e9db5e32edf1be4e0a881ee3afcf9e9f97de83</citedby><cites>FETCH-LOGICAL-c393t-5bc9876af5dc499ea5c635dbae5e9db5e32edf1be4e0a881ee3afcf9e9f97de83</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://dx.doi.org/10.1016/j.ijsolstr.2012.03.029$$EHTML$$P50$$Gelsevier$$Hfree_for_read</linktohtml><link.rule.ids>314,780,784,3550,27924,27925,45995</link.rule.ids></links><search><creatorcontrib>Aliha, M.R.M.</creatorcontrib><creatorcontrib>Ayatollahi, M.R.</creatorcontrib><title>Analysis of fracture initiation angle in some cracked ceramics using the generalized maximum tangential stress criterion</title><title>International journal of solids and structures</title><description>Brittle fracture in ceramics sometimes occurs under combined opening-sliding (or mixed mode I/II) crack deformation. In this paper, a generalized maximum tangential stress criterion is employed for predicting the fracture initiation angle under mixed mode I/II loading in some brittle ceramics including alumina, zirconia, soda lime glass and three silicon based ceramics. The experimental results reported for the fracture angles in these ceramics have been obtained from fracture tests on the centrally cracked circular disc (often called the Brazilian disc). Very good agreement is shown to exist between the experimental results and the theoretical predictions. According to the fracture model, the mixed mode fracture angle is strongly dependent on the elastic T-stress in the tested ceramics. The negative T-stress that exists in the Brazilian disc specimen can be the main influencing parameter for decreasing the fracture initiation angle in the investigated ceramics.</description><subject>Brazil</subject><subject>Brazilian disc specimen</subject><subject>Ceramics</subject><subject>Crack initiation</subject><subject>Criteria</subject><subject>Discs</subject><subject>Disks</subject><subject>Fracture initiation angle</subject><subject>Fracture mechanics</subject><subject>Mathematical models</subject><subject>Mixed mode fracture</subject><issn>0020-7683</issn><issn>1879-2146</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2012</creationdate><recordtype>article</recordtype><recordid>eNqFkMtu2zAQRYkgAeKk-YWCy26kkKJe3MUI-ggQIJt0TdDU0BlHolwOVdj5-tJwu-6KwPDeg5nD2GcpSilke78rcUfzSCmWlZBVKVQpKn3BVrLvdFHJur1kKyEqUXRtr67ZDdFOCFErLVbssA52PBISnz330bq0ROAYMKFNOAduw3Y8DTjNE3CXE-8wcAfRTuiIL4Rhy9Mb8C2EPBzxI39P9oDTMvGU2xAyauR5PSDKAEwQM_gTu_J2JLj7-96yn9--vj7-KJ5fvj89rp8Lp7RKRbNxuu9a65vB1VqDbVyrmmFjoQE9bBpQFQxebqAGYfteAijrndegve4G6NUt-3Lm7uP8awFKZkJyMI42wLyQkW0nK53F1TnanqMuzkQRvNlHnGw8GinMSbXZmX-qzUm1Ecpk1bn4cC5CPuQ3QjTkEIKDASO4ZIYZ_4f4AyaPkI4</recordid><startdate>20120615</startdate><enddate>20120615</enddate><creator>Aliha, M.R.M.</creator><creator>Ayatollahi, M.R.</creator><general>Elsevier Ltd</general><scope>6I.</scope><scope>AAFTH</scope><scope>AAYXX</scope><scope>CITATION</scope><scope>7QF</scope><scope>7QQ</scope><scope>7SR</scope><scope>7TB</scope><scope>8BQ</scope><scope>8FD</scope><scope>FR3</scope><scope>JG9</scope><scope>KR7</scope></search><sort><creationdate>20120615</creationdate><title>Analysis of fracture initiation angle in some cracked ceramics using the generalized maximum tangential stress criterion</title><author>Aliha, M.R.M. ; Ayatollahi, M.R.</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c393t-5bc9876af5dc499ea5c635dbae5e9db5e32edf1be4e0a881ee3afcf9e9f97de83</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2012</creationdate><topic>Brazil</topic><topic>Brazilian disc specimen</topic><topic>Ceramics</topic><topic>Crack initiation</topic><topic>Criteria</topic><topic>Discs</topic><topic>Disks</topic><topic>Fracture initiation angle</topic><topic>Fracture mechanics</topic><topic>Mathematical models</topic><topic>Mixed mode fracture</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Aliha, M.R.M.</creatorcontrib><creatorcontrib>Ayatollahi, M.R.</creatorcontrib><collection>ScienceDirect Open Access Titles</collection><collection>Elsevier:ScienceDirect:Open Access</collection><collection>CrossRef</collection><collection>Aluminium Industry Abstracts</collection><collection>Ceramic Abstracts</collection><collection>Engineered Materials Abstracts</collection><collection>Mechanical & Transportation Engineering Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Engineering Research Database</collection><collection>Materials Research Database</collection><collection>Civil Engineering Abstracts</collection><jtitle>International journal of solids and structures</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Aliha, M.R.M.</au><au>Ayatollahi, M.R.</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Analysis of fracture initiation angle in some cracked ceramics using the generalized maximum tangential stress criterion</atitle><jtitle>International journal of solids and structures</jtitle><date>2012-06-15</date><risdate>2012</risdate><volume>49</volume><issue>13</issue><spage>1877</spage><epage>1883</epage><pages>1877-1883</pages><issn>0020-7683</issn><eissn>1879-2146</eissn><abstract>Brittle fracture in ceramics sometimes occurs under combined opening-sliding (or mixed mode I/II) crack deformation. In this paper, a generalized maximum tangential stress criterion is employed for predicting the fracture initiation angle under mixed mode I/II loading in some brittle ceramics including alumina, zirconia, soda lime glass and three silicon based ceramics. The experimental results reported for the fracture angles in these ceramics have been obtained from fracture tests on the centrally cracked circular disc (often called the Brazilian disc). Very good agreement is shown to exist between the experimental results and the theoretical predictions. According to the fracture model, the mixed mode fracture angle is strongly dependent on the elastic T-stress in the tested ceramics. The negative T-stress that exists in the Brazilian disc specimen can be the main influencing parameter for decreasing the fracture initiation angle in the investigated ceramics.</abstract><pub>Elsevier Ltd</pub><doi>10.1016/j.ijsolstr.2012.03.029</doi><tpages>7</tpages><oa>free_for_read</oa></addata></record> |
fulltext | fulltext |
identifier | ISSN: 0020-7683 |
ispartof | International journal of solids and structures, 2012-06, Vol.49 (13), p.1877-1883 |
issn | 0020-7683 1879-2146 |
language | eng |
recordid | cdi_proquest_miscellaneous_1671292014 |
source | Elsevier ScienceDirect Journals Complete; Elektronische Zeitschriftenbibliothek - Frei zugängliche E-Journals |
subjects | Brazil Brazilian disc specimen Ceramics Crack initiation Criteria Discs Disks Fracture initiation angle Fracture mechanics Mathematical models Mixed mode fracture |
title | Analysis of fracture initiation angle in some cracked ceramics using the generalized maximum tangential stress criterion |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-04T09%3A29%3A28IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Analysis%20of%20fracture%20initiation%20angle%20in%20some%20cracked%20ceramics%20using%20the%20generalized%20maximum%20tangential%20stress%20criterion&rft.jtitle=International%20journal%20of%20solids%20and%20structures&rft.au=Aliha,%20M.R.M.&rft.date=2012-06-15&rft.volume=49&rft.issue=13&rft.spage=1877&rft.epage=1883&rft.pages=1877-1883&rft.issn=0020-7683&rft.eissn=1879-2146&rft_id=info:doi/10.1016/j.ijsolstr.2012.03.029&rft_dat=%3Cproquest_cross%3E1671292014%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=1671292014&rft_id=info:pmid/&rft_els_id=S002076831200131X&rfr_iscdi=true |