Tribological investigation of MoS2 coatings deposited on the laser textured surface

► MoS2 solid lubricant coating was fabricated by a combination technology of laser texturing and hot-pressing. ► We examine influences of preparation methods and texture density on the wear life and wears mechanism of coatings. ► The coating by hot pressing on textured surface shows excellent tribol...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Wear 2012-03, Vol.278-279, p.77-82
Hauptverfasser: Hu, Tianchang, Zhang, Yongsheng, Hu, Litian
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 82
container_issue
container_start_page 77
container_title Wear
container_volume 278-279
creator Hu, Tianchang
Zhang, Yongsheng
Hu, Litian
description ► MoS2 solid lubricant coating was fabricated by a combination technology of laser texturing and hot-pressing. ► We examine influences of preparation methods and texture density on the wear life and wears mechanism of coatings. ► The coating by hot pressing on textured surface shows excellent tribological behavior. ► Increasing texture density will increase wear life of coating. Deposition of solid lubricant on the textured surface is an effective way to improve tribological properties of counterparts. In this paper, MoS2 solid lubricant coating was fabricated by a combination technology of laser texturing and hot-pressing. The influences of preparation methods and texture density on the tribological properties of coatings were also investigated. Research results show that a thicker and denser coating having better adhesion with the textured steel substrate was fabricated by this combination technology, which results in excellent tribological properties. The friction coefficients of hot pressed coatings are less than 0.1. The wear life of hot pressed coating can be reached 90min with a texture density of 8.5%, which is 15 times higher than that of coating fabricated by burnishing. In addition, the wear life of hot pressed coating significantly increases with the increase of texture density. The possible friction reduction and wear resistant mechanisms are discussed.
doi_str_mv 10.1016/j.wear.2012.01.001
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_1019652557</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0043164812000026</els_id><sourcerecordid>1019652557</sourcerecordid><originalsourceid>FETCH-LOGICAL-c359t-fbd176944d28665f67021643ce52b33c9e9f606b1e2a8ff1604653b08d7c97253</originalsourceid><addsrcrecordid>eNp9kMtOwzAQRS0EEqXwA6yyQWKT4EfsJBIbVPGSili0rC3HGRdXaVxsh8ff46oVS1aWPWdmrg9ClwQXBBNxsy6-QPmCYkILTAqMyRGakLpiOeVVdYwmGJcsJ6KsT9FZCGuciIaLCVosvW1d71ZWqz6zwyeEaFcqWjdkzmQvbkEz7dJ9WIWsg60LNkKXpWp8h6xXAXwW4TuOPr2G0Rul4RydGNUHuDicU_T2cL-cPeXz18fn2d0814w3MTdtRyrRlGVHayG4ERWmKSHTwGnLmG6gMQKLlgBVtTFE4FJw1uK6q3RTUc6m6Ho_d-vdx5iCy40NGvpeDeDGIJOZRnDKeZVQuke1dyF4MHLr7Ub5nwTtOCHXcmdQ7gxKTGTyk5quDvNVSHaMV4O24a8zmaWYMZG42z0H6bOfFrwM2sKgobMedJSds_-t-QW8xIZZ</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1019652557</pqid></control><display><type>article</type><title>Tribological investigation of MoS2 coatings deposited on the laser textured surface</title><source>Elsevier ScienceDirect Journals Complete</source><creator>Hu, Tianchang ; Zhang, Yongsheng ; Hu, Litian</creator><creatorcontrib>Hu, Tianchang ; Zhang, Yongsheng ; Hu, Litian</creatorcontrib><description>► MoS2 solid lubricant coating was fabricated by a combination technology of laser texturing and hot-pressing. ► We examine influences of preparation methods and texture density on the wear life and wears mechanism of coatings. ► The coating by hot pressing on textured surface shows excellent tribological behavior. ► Increasing texture density will increase wear life of coating. Deposition of solid lubricant on the textured surface is an effective way to improve tribological properties of counterparts. In this paper, MoS2 solid lubricant coating was fabricated by a combination technology of laser texturing and hot-pressing. The influences of preparation methods and texture density on the tribological properties of coatings were also investigated. Research results show that a thicker and denser coating having better adhesion with the textured steel substrate was fabricated by this combination technology, which results in excellent tribological properties. The friction coefficients of hot pressed coatings are less than 0.1. The wear life of hot pressed coating can be reached 90min with a texture density of 8.5%, which is 15 times higher than that of coating fabricated by burnishing. In addition, the wear life of hot pressed coating significantly increases with the increase of texture density. The possible friction reduction and wear resistant mechanisms are discussed.</description><identifier>ISSN: 0043-1648</identifier><identifier>EISSN: 1873-2577</identifier><identifier>DOI: 10.1016/j.wear.2012.01.001</identifier><identifier>CODEN: WEARAH</identifier><language>eng</language><publisher>Amsterdam: Elsevier B.V</publisher><subject>Applied sciences ; Coatings ; Density ; Exact sciences and technology ; Friction, wear, lubrication ; Hot-pressing ; Laser surface texturing ; Lasers ; Machine components ; Mechanical engineering. Machine design ; Molybdenum disulfide ; MoS2 coatings ; Solid lubrication ; Surface layer ; Texture ; Tribology ; Wear ; Wear life</subject><ispartof>Wear, 2012-03, Vol.278-279, p.77-82</ispartof><rights>2012 Elsevier B.V.</rights><rights>2015 INIST-CNRS</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c359t-fbd176944d28665f67021643ce52b33c9e9f606b1e2a8ff1604653b08d7c97253</citedby><cites>FETCH-LOGICAL-c359t-fbd176944d28665f67021643ce52b33c9e9f606b1e2a8ff1604653b08d7c97253</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://dx.doi.org/10.1016/j.wear.2012.01.001$$EHTML$$P50$$Gelsevier$$H</linktohtml><link.rule.ids>314,780,784,3550,27924,27925,45995</link.rule.ids><backlink>$$Uhttp://pascal-francis.inist.fr/vibad/index.php?action=getRecordDetail&amp;idt=25720336$$DView record in Pascal Francis$$Hfree_for_read</backlink></links><search><creatorcontrib>Hu, Tianchang</creatorcontrib><creatorcontrib>Zhang, Yongsheng</creatorcontrib><creatorcontrib>Hu, Litian</creatorcontrib><title>Tribological investigation of MoS2 coatings deposited on the laser textured surface</title><title>Wear</title><description>► MoS2 solid lubricant coating was fabricated by a combination technology of laser texturing and hot-pressing. ► We examine influences of preparation methods and texture density on the wear life and wears mechanism of coatings. ► The coating by hot pressing on textured surface shows excellent tribological behavior. ► Increasing texture density will increase wear life of coating. Deposition of solid lubricant on the textured surface is an effective way to improve tribological properties of counterparts. In this paper, MoS2 solid lubricant coating was fabricated by a combination technology of laser texturing and hot-pressing. The influences of preparation methods and texture density on the tribological properties of coatings were also investigated. Research results show that a thicker and denser coating having better adhesion with the textured steel substrate was fabricated by this combination technology, which results in excellent tribological properties. The friction coefficients of hot pressed coatings are less than 0.1. The wear life of hot pressed coating can be reached 90min with a texture density of 8.5%, which is 15 times higher than that of coating fabricated by burnishing. In addition, the wear life of hot pressed coating significantly increases with the increase of texture density. The possible friction reduction and wear resistant mechanisms are discussed.</description><subject>Applied sciences</subject><subject>Coatings</subject><subject>Density</subject><subject>Exact sciences and technology</subject><subject>Friction, wear, lubrication</subject><subject>Hot-pressing</subject><subject>Laser surface texturing</subject><subject>Lasers</subject><subject>Machine components</subject><subject>Mechanical engineering. Machine design</subject><subject>Molybdenum disulfide</subject><subject>MoS2 coatings</subject><subject>Solid lubrication</subject><subject>Surface layer</subject><subject>Texture</subject><subject>Tribology</subject><subject>Wear</subject><subject>Wear life</subject><issn>0043-1648</issn><issn>1873-2577</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2012</creationdate><recordtype>article</recordtype><recordid>eNp9kMtOwzAQRS0EEqXwA6yyQWKT4EfsJBIbVPGSili0rC3HGRdXaVxsh8ff46oVS1aWPWdmrg9ClwQXBBNxsy6-QPmCYkILTAqMyRGakLpiOeVVdYwmGJcsJ6KsT9FZCGuciIaLCVosvW1d71ZWqz6zwyeEaFcqWjdkzmQvbkEz7dJ9WIWsg60LNkKXpWp8h6xXAXwW4TuOPr2G0Rul4RydGNUHuDicU_T2cL-cPeXz18fn2d0814w3MTdtRyrRlGVHayG4ERWmKSHTwGnLmG6gMQKLlgBVtTFE4FJw1uK6q3RTUc6m6Ho_d-vdx5iCy40NGvpeDeDGIJOZRnDKeZVQuke1dyF4MHLr7Ub5nwTtOCHXcmdQ7gxKTGTyk5quDvNVSHaMV4O24a8zmaWYMZG42z0H6bOfFrwM2sKgobMedJSds_-t-QW8xIZZ</recordid><startdate>20120308</startdate><enddate>20120308</enddate><creator>Hu, Tianchang</creator><creator>Zhang, Yongsheng</creator><creator>Hu, Litian</creator><general>Elsevier B.V</general><general>Elsevier</general><scope>IQODW</scope><scope>AAYXX</scope><scope>CITATION</scope><scope>7SR</scope><scope>7TB</scope><scope>7U5</scope><scope>8BQ</scope><scope>8FD</scope><scope>FR3</scope><scope>JG9</scope><scope>L7M</scope></search><sort><creationdate>20120308</creationdate><title>Tribological investigation of MoS2 coatings deposited on the laser textured surface</title><author>Hu, Tianchang ; Zhang, Yongsheng ; Hu, Litian</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c359t-fbd176944d28665f67021643ce52b33c9e9f606b1e2a8ff1604653b08d7c97253</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2012</creationdate><topic>Applied sciences</topic><topic>Coatings</topic><topic>Density</topic><topic>Exact sciences and technology</topic><topic>Friction, wear, lubrication</topic><topic>Hot-pressing</topic><topic>Laser surface texturing</topic><topic>Lasers</topic><topic>Machine components</topic><topic>Mechanical engineering. Machine design</topic><topic>Molybdenum disulfide</topic><topic>MoS2 coatings</topic><topic>Solid lubrication</topic><topic>Surface layer</topic><topic>Texture</topic><topic>Tribology</topic><topic>Wear</topic><topic>Wear life</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Hu, Tianchang</creatorcontrib><creatorcontrib>Zhang, Yongsheng</creatorcontrib><creatorcontrib>Hu, Litian</creatorcontrib><collection>Pascal-Francis</collection><collection>CrossRef</collection><collection>Engineered Materials Abstracts</collection><collection>Mechanical &amp; Transportation Engineering Abstracts</collection><collection>Solid State and Superconductivity Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Engineering Research Database</collection><collection>Materials Research Database</collection><collection>Advanced Technologies Database with Aerospace</collection><jtitle>Wear</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Hu, Tianchang</au><au>Zhang, Yongsheng</au><au>Hu, Litian</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Tribological investigation of MoS2 coatings deposited on the laser textured surface</atitle><jtitle>Wear</jtitle><date>2012-03-08</date><risdate>2012</risdate><volume>278-279</volume><spage>77</spage><epage>82</epage><pages>77-82</pages><issn>0043-1648</issn><eissn>1873-2577</eissn><coden>WEARAH</coden><abstract>► MoS2 solid lubricant coating was fabricated by a combination technology of laser texturing and hot-pressing. ► We examine influences of preparation methods and texture density on the wear life and wears mechanism of coatings. ► The coating by hot pressing on textured surface shows excellent tribological behavior. ► Increasing texture density will increase wear life of coating. Deposition of solid lubricant on the textured surface is an effective way to improve tribological properties of counterparts. In this paper, MoS2 solid lubricant coating was fabricated by a combination technology of laser texturing and hot-pressing. The influences of preparation methods and texture density on the tribological properties of coatings were also investigated. Research results show that a thicker and denser coating having better adhesion with the textured steel substrate was fabricated by this combination technology, which results in excellent tribological properties. The friction coefficients of hot pressed coatings are less than 0.1. The wear life of hot pressed coating can be reached 90min with a texture density of 8.5%, which is 15 times higher than that of coating fabricated by burnishing. In addition, the wear life of hot pressed coating significantly increases with the increase of texture density. The possible friction reduction and wear resistant mechanisms are discussed.</abstract><cop>Amsterdam</cop><pub>Elsevier B.V</pub><doi>10.1016/j.wear.2012.01.001</doi><tpages>6</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0043-1648
ispartof Wear, 2012-03, Vol.278-279, p.77-82
issn 0043-1648
1873-2577
language eng
recordid cdi_proquest_miscellaneous_1019652557
source Elsevier ScienceDirect Journals Complete
subjects Applied sciences
Coatings
Density
Exact sciences and technology
Friction, wear, lubrication
Hot-pressing
Laser surface texturing
Lasers
Machine components
Mechanical engineering. Machine design
Molybdenum disulfide
MoS2 coatings
Solid lubrication
Surface layer
Texture
Tribology
Wear
Wear life
title Tribological investigation of MoS2 coatings deposited on the laser textured surface
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-04T07%3A12%3A49IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Tribological%20investigation%20of%20MoS2%20coatings%20deposited%20on%20the%20laser%20textured%20surface&rft.jtitle=Wear&rft.au=Hu,%20Tianchang&rft.date=2012-03-08&rft.volume=278-279&rft.spage=77&rft.epage=82&rft.pages=77-82&rft.issn=0043-1648&rft.eissn=1873-2577&rft.coden=WEARAH&rft_id=info:doi/10.1016/j.wear.2012.01.001&rft_dat=%3Cproquest_cross%3E1019652557%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=1019652557&rft_id=info:pmid/&rft_els_id=S0043164812000026&rfr_iscdi=true