Improving the mechanical and abrasion properties of silica-reinforced styrene-butadiene rubber composites by optimizing the concentrations of compatibilizers

Silica (chemical formula SiO 2 ) is a promising, more environmentally friendly alternative to carbon black (CB) used in the rubber industry as a filler. Although silica is already used in rubber products, it is not used as extensively as CB because the polar surface of silica cannot interact well wi...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Polymer bulletin (Berlin, Germany) Germany), 2024-09, Vol.81 (14), p.12715-12731
Hauptverfasser: Sayfo, Petra, Pölöskei, Kornél, Mészáros, László
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Silica (chemical formula SiO 2 ) is a promising, more environmentally friendly alternative to carbon black (CB) used in the rubber industry as a filler. Although silica is already used in rubber products, it is not used as extensively as CB because the polar surface of silica cannot interact well with the apolar polymer molecules of the most frequently used rubbers. To solve this problem, experts have tried different grafting methods and several coupling agents for a stronger silica-elastomer connection. In this article, we used bis[3-(triethoxysilyl)propyl] tetrasulfide (TESPT) and polyethylene glycol (PEG) combined to improve the connection between the surface of silica and the apolar styrene-butadiene rubber (SBR) matrix. We examined mechanical and structural properties and found that adding 3 phr PEG and 4.5 phr TESPT to SBR is optimal for 60 phr silica content. This ratio of additives resulted in a 48% improvement in tensile strength. The positive effect of the coupling agents shows up in abrasion mass loss and tear strength as well.
ISSN:0170-0839
1436-2449
DOI:10.1007/s00289-024-05314-w