Enhancement of hole mobility in high-rate reactively sputtered Cu2O thin films induced by laser thermal annealing

In presented work, a reactive high-power impulse magnetron sputtering (r-HiPIMS) was used for high-rate deposition ( 170 nm/min) of Cu2O films. Films were deposited on a standard soda-lime glass (SLG) substrate at a temperature of 190C. As-deposited films exhibit poor hole mobility in the orders of...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:arXiv.org 2024-04
Hauptverfasser: Rezek, Jiri, Kucera, Martin, Kozak, Tomas, Cerstvy, Radomir, Franc, Ales, Baroch, Pavel
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title arXiv.org
container_volume
creator Rezek, Jiri
Kucera, Martin
Kozak, Tomas
Cerstvy, Radomir
Franc, Ales
Baroch, Pavel
description In presented work, a reactive high-power impulse magnetron sputtering (r-HiPIMS) was used for high-rate deposition ( 170 nm/min) of Cu2O films. Films were deposited on a standard soda-lime glass (SLG) substrate at a temperature of 190C. As-deposited films exhibit poor hole mobility in the orders of 1 cm2/Vs. We have systematically studied the effect of laser thermal annealing (LTA) procedure performed using high-power infrared laser under different laser parameters (number of pulses, length of the pulse). We have found, LTA procedure could significantly enhance the hole mobility (up to 24 cm2/Vs in our case). We have also fitted the results of a temperature-dependent Hall measurement to clarify the mechanism of the reported increase in hole mobility. Moreover, we have discussed the effect of the LTA procedure on microstructure (crystallinity, surface morphology) and on the value of optical band gap.
format Article
fullrecord <record><control><sourceid>proquest</sourceid><recordid>TN_cdi_proquest_journals_3040962361</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>3040962361</sourcerecordid><originalsourceid>FETCH-proquest_journals_30409623613</originalsourceid><addsrcrecordid>eNqNi7EKwjAURYMgKNp_eOBciImtOovi5uIusX01KWlSkxehf28GP8DpwjnnzthSSLktDzshFqyIseeci3ovqkou2fvstHINDugIfAfaW4TBP401NIFxoM1Ll0ERQkDVkPmgnSCOiQgDtnBK4gakc9gZO8T8aFOT-XMCqyKG7DAMyoJyDpU17rVm807ZiMVvV2xzOd9P13IM_p0w0qP3KbisHpLv-LEWst7K_6ovN0NLPQ</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>3040962361</pqid></control><display><type>article</type><title>Enhancement of hole mobility in high-rate reactively sputtered Cu2O thin films induced by laser thermal annealing</title><source>Free E- Journals</source><creator>Rezek, Jiri ; Kucera, Martin ; Kozak, Tomas ; Cerstvy, Radomir ; Franc, Ales ; Baroch, Pavel</creator><creatorcontrib>Rezek, Jiri ; Kucera, Martin ; Kozak, Tomas ; Cerstvy, Radomir ; Franc, Ales ; Baroch, Pavel</creatorcontrib><description>In presented work, a reactive high-power impulse magnetron sputtering (r-HiPIMS) was used for high-rate deposition ( 170 nm/min) of Cu2O films. Films were deposited on a standard soda-lime glass (SLG) substrate at a temperature of 190C. As-deposited films exhibit poor hole mobility in the orders of 1 cm2/Vs. We have systematically studied the effect of laser thermal annealing (LTA) procedure performed using high-power infrared laser under different laser parameters (number of pulses, length of the pulse). We have found, LTA procedure could significantly enhance the hole mobility (up to 24 cm2/Vs in our case). We have also fitted the results of a temperature-dependent Hall measurement to clarify the mechanism of the reported increase in hole mobility. Moreover, we have discussed the effect of the LTA procedure on microstructure (crystallinity, surface morphology) and on the value of optical band gap.</description><identifier>EISSN: 2331-8422</identifier><language>eng</language><publisher>Ithaca: Cornell University Library, arXiv.org</publisher><subject>Annealing ; Copper oxides ; Glass substrates ; Hall effect ; Hole mobility ; Infrared lasers ; Magnetron sputtering ; Soda-lime glass ; Temperature dependence ; Thin films</subject><ispartof>arXiv.org, 2024-04</ispartof><rights>2024. This work is published under http://arxiv.org/licenses/nonexclusive-distrib/1.0/ (the “License”). Notwithstanding the ProQuest Terms and Conditions, you may use this content in accordance with the terms of the License.</rights><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>776,780</link.rule.ids></links><search><creatorcontrib>Rezek, Jiri</creatorcontrib><creatorcontrib>Kucera, Martin</creatorcontrib><creatorcontrib>Kozak, Tomas</creatorcontrib><creatorcontrib>Cerstvy, Radomir</creatorcontrib><creatorcontrib>Franc, Ales</creatorcontrib><creatorcontrib>Baroch, Pavel</creatorcontrib><title>Enhancement of hole mobility in high-rate reactively sputtered Cu2O thin films induced by laser thermal annealing</title><title>arXiv.org</title><description>In presented work, a reactive high-power impulse magnetron sputtering (r-HiPIMS) was used for high-rate deposition ( 170 nm/min) of Cu2O films. Films were deposited on a standard soda-lime glass (SLG) substrate at a temperature of 190C. As-deposited films exhibit poor hole mobility in the orders of 1 cm2/Vs. We have systematically studied the effect of laser thermal annealing (LTA) procedure performed using high-power infrared laser under different laser parameters (number of pulses, length of the pulse). We have found, LTA procedure could significantly enhance the hole mobility (up to 24 cm2/Vs in our case). We have also fitted the results of a temperature-dependent Hall measurement to clarify the mechanism of the reported increase in hole mobility. Moreover, we have discussed the effect of the LTA procedure on microstructure (crystallinity, surface morphology) and on the value of optical band gap.</description><subject>Annealing</subject><subject>Copper oxides</subject><subject>Glass substrates</subject><subject>Hall effect</subject><subject>Hole mobility</subject><subject>Infrared lasers</subject><subject>Magnetron sputtering</subject><subject>Soda-lime glass</subject><subject>Temperature dependence</subject><subject>Thin films</subject><issn>2331-8422</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2024</creationdate><recordtype>article</recordtype><sourceid>BENPR</sourceid><recordid>eNqNi7EKwjAURYMgKNp_eOBciImtOovi5uIusX01KWlSkxehf28GP8DpwjnnzthSSLktDzshFqyIseeci3ovqkou2fvstHINDugIfAfaW4TBP401NIFxoM1Ll0ERQkDVkPmgnSCOiQgDtnBK4gakc9gZO8T8aFOT-XMCqyKG7DAMyoJyDpU17rVm807ZiMVvV2xzOd9P13IM_p0w0qP3KbisHpLv-LEWst7K_6ovN0NLPQ</recordid><startdate>20240417</startdate><enddate>20240417</enddate><creator>Rezek, Jiri</creator><creator>Kucera, Martin</creator><creator>Kozak, Tomas</creator><creator>Cerstvy, Radomir</creator><creator>Franc, Ales</creator><creator>Baroch, Pavel</creator><general>Cornell University Library, arXiv.org</general><scope>8FE</scope><scope>8FG</scope><scope>ABJCF</scope><scope>ABUWG</scope><scope>AFKRA</scope><scope>AZQEC</scope><scope>BENPR</scope><scope>BGLVJ</scope><scope>CCPQU</scope><scope>DWQXO</scope><scope>HCIFZ</scope><scope>L6V</scope><scope>M7S</scope><scope>PIMPY</scope><scope>PQEST</scope><scope>PQQKQ</scope><scope>PQUKI</scope><scope>PRINS</scope><scope>PTHSS</scope></search><sort><creationdate>20240417</creationdate><title>Enhancement of hole mobility in high-rate reactively sputtered Cu2O thin films induced by laser thermal annealing</title><author>Rezek, Jiri ; Kucera, Martin ; Kozak, Tomas ; Cerstvy, Radomir ; Franc, Ales ; Baroch, Pavel</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-proquest_journals_30409623613</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2024</creationdate><topic>Annealing</topic><topic>Copper oxides</topic><topic>Glass substrates</topic><topic>Hall effect</topic><topic>Hole mobility</topic><topic>Infrared lasers</topic><topic>Magnetron sputtering</topic><topic>Soda-lime glass</topic><topic>Temperature dependence</topic><topic>Thin films</topic><toplevel>online_resources</toplevel><creatorcontrib>Rezek, Jiri</creatorcontrib><creatorcontrib>Kucera, Martin</creatorcontrib><creatorcontrib>Kozak, Tomas</creatorcontrib><creatorcontrib>Cerstvy, Radomir</creatorcontrib><creatorcontrib>Franc, Ales</creatorcontrib><creatorcontrib>Baroch, Pavel</creatorcontrib><collection>ProQuest SciTech Collection</collection><collection>ProQuest Technology Collection</collection><collection>Materials Science &amp; Engineering Collection</collection><collection>ProQuest Central (Alumni Edition)</collection><collection>ProQuest Central UK/Ireland</collection><collection>ProQuest Central Essentials</collection><collection>ProQuest Central</collection><collection>Technology Collection (ProQuest)</collection><collection>ProQuest One Community College</collection><collection>ProQuest Central Korea</collection><collection>SciTech Premium Collection</collection><collection>ProQuest Engineering Collection</collection><collection>Engineering Database</collection><collection>Publicly Available Content Database</collection><collection>ProQuest One Academic Eastern Edition (DO NOT USE)</collection><collection>ProQuest One Academic</collection><collection>ProQuest One Academic UKI Edition</collection><collection>ProQuest Central China</collection><collection>Engineering Collection</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Rezek, Jiri</au><au>Kucera, Martin</au><au>Kozak, Tomas</au><au>Cerstvy, Radomir</au><au>Franc, Ales</au><au>Baroch, Pavel</au><format>book</format><genre>document</genre><ristype>GEN</ristype><atitle>Enhancement of hole mobility in high-rate reactively sputtered Cu2O thin films induced by laser thermal annealing</atitle><jtitle>arXiv.org</jtitle><date>2024-04-17</date><risdate>2024</risdate><eissn>2331-8422</eissn><abstract>In presented work, a reactive high-power impulse magnetron sputtering (r-HiPIMS) was used for high-rate deposition ( 170 nm/min) of Cu2O films. Films were deposited on a standard soda-lime glass (SLG) substrate at a temperature of 190C. As-deposited films exhibit poor hole mobility in the orders of 1 cm2/Vs. We have systematically studied the effect of laser thermal annealing (LTA) procedure performed using high-power infrared laser under different laser parameters (number of pulses, length of the pulse). We have found, LTA procedure could significantly enhance the hole mobility (up to 24 cm2/Vs in our case). We have also fitted the results of a temperature-dependent Hall measurement to clarify the mechanism of the reported increase in hole mobility. Moreover, we have discussed the effect of the LTA procedure on microstructure (crystallinity, surface morphology) and on the value of optical band gap.</abstract><cop>Ithaca</cop><pub>Cornell University Library, arXiv.org</pub><oa>free_for_read</oa></addata></record>
fulltext fulltext
identifier EISSN: 2331-8422
ispartof arXiv.org, 2024-04
issn 2331-8422
language eng
recordid cdi_proquest_journals_3040962361
source Free E- Journals
subjects Annealing
Copper oxides
Glass substrates
Hall effect
Hole mobility
Infrared lasers
Magnetron sputtering
Soda-lime glass
Temperature dependence
Thin films
title Enhancement of hole mobility in high-rate reactively sputtered Cu2O thin films induced by laser thermal annealing
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-06T08%3A09%3A40IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest&rft_val_fmt=info:ofi/fmt:kev:mtx:book&rft.genre=document&rft.atitle=Enhancement%20of%20hole%20mobility%20in%20high-rate%20reactively%20sputtered%20Cu2O%20thin%20films%20induced%20by%20laser%20thermal%20annealing&rft.jtitle=arXiv.org&rft.au=Rezek,%20Jiri&rft.date=2024-04-17&rft.eissn=2331-8422&rft_id=info:doi/&rft_dat=%3Cproquest%3E3040962361%3C/proquest%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=3040962361&rft_id=info:pmid/&rfr_iscdi=true