Microstructure, Residual Strain and Stress Corrosion Cracking Behavior in 316L Heat-Affected Zone
Austenitic stainless steels are usually chosen to make many components of nuclear power plants (NPPs). However, their microstructure in the heat-affected zone (HAZ) will change during the welding process. Some failures of the weld joints, mainly stress corrosion cracking (SCC), have been found to be...