Effect of compaction pressure and heating rate on microstructure and mechanical properties of spark plasma sintered Ti6Al4V alloy

In the present paper, the use of spark plasma sintering on Ti6Al4V powder was investigated. Sintering experiments were conducted at the temperature of 10008C for 5 min. The simultaneous effect of compaction pressures of 5, 25 and 50 MPa and heating rates of 200, 300 and 4008C/min on the structure, d...