Effect of aging treatment on the microstructure, fracture toughness and fracture behavior of the extruded Mg-7Gd-2Y–1Zn-0.5Zr alloy
A commercial scale Mg-7Gd-2Y–1Zn-0.5Zr alloy extrusion rod with synergetic high yield strength of 350 MPa and fracture toughness KIC of 22.4 MPa m1/2 was fabricated by direct-chill casting, hot extrusion and subsequent aging treatment at 200 °C for 108 h. The microstructures and mechanical propertie...