Production and Properties of Ceramic Made From Nickel Oxide Nanopowder

A fine-grained (of the order of 250 – 500 nm), dense (5.93 g/cm 3 ), strong ceramic with microhardness Hv = 8.2 GPa, compressive strength σ r = 0.4 GPa, and Young’s modulus E = 140 GPa was produced, by means of spark plasma sintering (SPS), using nickel oxide nanopowder. The resulting ceramic sample...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Glass and ceramics 2022-05, Vol.79 (1-2), p.9-10
1. Verfasser: Lysenko, V. I.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A fine-grained (of the order of 250 – 500 nm), dense (5.93 g/cm 3 ), strong ceramic with microhardness Hv = 8.2 GPa, compressive strength σ r = 0.4 GPa, and Young’s modulus E = 140 GPa was produced, by means of spark plasma sintering (SPS), using nickel oxide nanopowder. The resulting ceramic sample was nickel oxide NiO (73-1519) with a cubic structure, space group Fm3m (No. 225), and lattice size a = 4.168 Å.
ISSN:0361-7610
1573-8515
DOI:10.1007/s10717-022-00444-x