Mechanical Properties and Damage Mechanism of Shale Ceramsite Concrete after High-Temperature Treatment
AbstractThe high-temperature resistance of lightweight shale ceramsite concrete (LWSCC) is seriously underestimated because the effect of moisture is not considered. To investigate the mechanical properties and damage of LWSCC after a high-temperature treatment, strength tests, X-ray diffraction (XR...
Gespeichert in:
Veröffentlicht in: | Journal of materials in civil engineering 2022-07, Vol.34 (7) |
---|---|
Hauptverfasser: | , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | 7 |
container_start_page | |
container_title | Journal of materials in civil engineering |
container_volume | 34 |
creator | Wu, Xiaogang Yang, Jianhui Lin, Haixiao Wang, Qinting Cao, Zhengzheng |
description | AbstractThe high-temperature resistance of lightweight shale ceramsite concrete (LWSCC) is seriously underestimated because the effect of moisture is not considered. To investigate the mechanical properties and damage of LWSCC after a high-temperature treatment, strength tests, X-ray diffraction (XRD), and scanning electron microscopy (SEM) were carried out, and a nondestructive ultrasonic testing device was used to quantify the damage. The results show that the spalling characteristics of LWSCC at high temperatures were closely related to its water content. The axial compressive strength of LWSCC linearly decreased with increasing target temperature. LWSCC showed a greater resistance to high-temperature deterioration than NWC with the same mass loss ratio. LWSCC with a moisture content of 4.1% had a high probability of spalling at temperatures above 500°C. However, dry LWSCC had a low probability of spalling even when heated to 800°C. Water in shale ceramsite with a porous structure was identified as a critical factor in the high-temperature deterioration. After the temperature exceeded 200°C, the high-pressure steam in the ceramsite expanded the cracks. These findings provide a basis for designing LWSCC with high-temperature resistance and evaluating the safety of LWSCC buildings after fires. |
doi_str_mv | 10.1061/(ASCE)MT.1943-5533.0004279 |
format | Article |
fullrecord | <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_journals_2652585426</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>2652585426</sourcerecordid><originalsourceid>FETCH-LOGICAL-a1826-335688adc3e07a8247fe8dcdf0c2aa489157c37bf518a3b616670e34541847343</originalsourceid><addsrcrecordid>eNp1kE1Lw0AQhhdRsFb_w6IXPaTuZj-y8Sa1WqFFofG8TDeTNqVJ6m568N-b0KonTzMMz_sOPIRcczbiTPP728fFeHI3z0Y8lSJSSogRY0zGSXpCBr-3UzJgJk0jrjQ_JxchbDpIMMkGZDVHt4a6dLCl777ZoW9LDBTqnD5BBSukRyBUtCnoYg1bpGP0UIWy7bamdh67BYoWPZ2Wq3WUYdXVQLv3SDOP0FZYt5fkrIBtwKvjHJKP50k2nkazt5fX8eMsAm5iHQmhtDGQO4EsARPLpECTu7xgLgaQJuUqcSJZFoobEEvNtU4YCqkkNzIRUgzJzaF355vPPYbWbpq9r7uXNtYqVkbJWHfUw4FyvgnBY2F3vqzAf1nObC_W2l6snWe2l2h7ifYotgvrQxiCw7_6n-T_wW_B3Xxa</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>2652585426</pqid></control><display><type>article</type><title>Mechanical Properties and Damage Mechanism of Shale Ceramsite Concrete after High-Temperature Treatment</title><source>American Society of Civil Engineers:NESLI2:Journals:2014</source><creator>Wu, Xiaogang ; Yang, Jianhui ; Lin, Haixiao ; Wang, Qinting ; Cao, Zhengzheng</creator><creatorcontrib>Wu, Xiaogang ; Yang, Jianhui ; Lin, Haixiao ; Wang, Qinting ; Cao, Zhengzheng</creatorcontrib><description>AbstractThe high-temperature resistance of lightweight shale ceramsite concrete (LWSCC) is seriously underestimated because the effect of moisture is not considered. To investigate the mechanical properties and damage of LWSCC after a high-temperature treatment, strength tests, X-ray diffraction (XRD), and scanning electron microscopy (SEM) were carried out, and a nondestructive ultrasonic testing device was used to quantify the damage. The results show that the spalling characteristics of LWSCC at high temperatures were closely related to its water content. The axial compressive strength of LWSCC linearly decreased with increasing target temperature. LWSCC showed a greater resistance to high-temperature deterioration than NWC with the same mass loss ratio. LWSCC with a moisture content of 4.1% had a high probability of spalling at temperatures above 500°C. However, dry LWSCC had a low probability of spalling even when heated to 800°C. Water in shale ceramsite with a porous structure was identified as a critical factor in the high-temperature deterioration. After the temperature exceeded 200°C, the high-pressure steam in the ceramsite expanded the cracks. These findings provide a basis for designing LWSCC with high-temperature resistance and evaluating the safety of LWSCC buildings after fires.</description><identifier>ISSN: 0899-1561</identifier><identifier>EISSN: 1943-5533</identifier><identifier>DOI: 10.1061/(ASCE)MT.1943-5533.0004279</identifier><language>eng</language><publisher>New York: American Society of Civil Engineers</publisher><subject>Building materials ; Civil engineering ; Compressive strength ; Damage ; Deterioration ; High temperature ; Mechanical properties ; Moisture content ; Moisture effects ; Nondestructive testing ; Spalling ; Technical Papers ; Temperature ; Ultrasonic testing</subject><ispartof>Journal of materials in civil engineering, 2022-07, Vol.34 (7)</ispartof><rights>2022 American Society of Civil Engineers</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-a1826-335688adc3e07a8247fe8dcdf0c2aa489157c37bf518a3b616670e34541847343</citedby><cites>FETCH-LOGICAL-a1826-335688adc3e07a8247fe8dcdf0c2aa489157c37bf518a3b616670e34541847343</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktopdf>$$Uhttp://ascelibrary.org/doi/pdf/10.1061/(ASCE)MT.1943-5533.0004279$$EPDF$$P50$$Gasce$$H</linktopdf><linktohtml>$$Uhttp://ascelibrary.org/doi/abs/10.1061/(ASCE)MT.1943-5533.0004279$$EHTML$$P50$$Gasce$$H</linktohtml><link.rule.ids>315,782,786,27933,27934,76203,76211</link.rule.ids></links><search><creatorcontrib>Wu, Xiaogang</creatorcontrib><creatorcontrib>Yang, Jianhui</creatorcontrib><creatorcontrib>Lin, Haixiao</creatorcontrib><creatorcontrib>Wang, Qinting</creatorcontrib><creatorcontrib>Cao, Zhengzheng</creatorcontrib><title>Mechanical Properties and Damage Mechanism of Shale Ceramsite Concrete after High-Temperature Treatment</title><title>Journal of materials in civil engineering</title><description>AbstractThe high-temperature resistance of lightweight shale ceramsite concrete (LWSCC) is seriously underestimated because the effect of moisture is not considered. To investigate the mechanical properties and damage of LWSCC after a high-temperature treatment, strength tests, X-ray diffraction (XRD), and scanning electron microscopy (SEM) were carried out, and a nondestructive ultrasonic testing device was used to quantify the damage. The results show that the spalling characteristics of LWSCC at high temperatures were closely related to its water content. The axial compressive strength of LWSCC linearly decreased with increasing target temperature. LWSCC showed a greater resistance to high-temperature deterioration than NWC with the same mass loss ratio. LWSCC with a moisture content of 4.1% had a high probability of spalling at temperatures above 500°C. However, dry LWSCC had a low probability of spalling even when heated to 800°C. Water in shale ceramsite with a porous structure was identified as a critical factor in the high-temperature deterioration. After the temperature exceeded 200°C, the high-pressure steam in the ceramsite expanded the cracks. These findings provide a basis for designing LWSCC with high-temperature resistance and evaluating the safety of LWSCC buildings after fires.</description><subject>Building materials</subject><subject>Civil engineering</subject><subject>Compressive strength</subject><subject>Damage</subject><subject>Deterioration</subject><subject>High temperature</subject><subject>Mechanical properties</subject><subject>Moisture content</subject><subject>Moisture effects</subject><subject>Nondestructive testing</subject><subject>Spalling</subject><subject>Technical Papers</subject><subject>Temperature</subject><subject>Ultrasonic testing</subject><issn>0899-1561</issn><issn>1943-5533</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2022</creationdate><recordtype>article</recordtype><recordid>eNp1kE1Lw0AQhhdRsFb_w6IXPaTuZj-y8Sa1WqFFofG8TDeTNqVJ6m568N-b0KonTzMMz_sOPIRcczbiTPP728fFeHI3z0Y8lSJSSogRY0zGSXpCBr-3UzJgJk0jrjQ_JxchbDpIMMkGZDVHt4a6dLCl777ZoW9LDBTqnD5BBSukRyBUtCnoYg1bpGP0UIWy7bamdh67BYoWPZ2Wq3WUYdXVQLv3SDOP0FZYt5fkrIBtwKvjHJKP50k2nkazt5fX8eMsAm5iHQmhtDGQO4EsARPLpECTu7xgLgaQJuUqcSJZFoobEEvNtU4YCqkkNzIRUgzJzaF355vPPYbWbpq9r7uXNtYqVkbJWHfUw4FyvgnBY2F3vqzAf1nObC_W2l6snWe2l2h7ifYotgvrQxiCw7_6n-T_wW_B3Xxa</recordid><startdate>20220701</startdate><enddate>20220701</enddate><creator>Wu, Xiaogang</creator><creator>Yang, Jianhui</creator><creator>Lin, Haixiao</creator><creator>Wang, Qinting</creator><creator>Cao, Zhengzheng</creator><general>American Society of Civil Engineers</general><scope>AAYXX</scope><scope>CITATION</scope><scope>8FD</scope><scope>FR3</scope><scope>KR7</scope></search><sort><creationdate>20220701</creationdate><title>Mechanical Properties and Damage Mechanism of Shale Ceramsite Concrete after High-Temperature Treatment</title><author>Wu, Xiaogang ; Yang, Jianhui ; Lin, Haixiao ; Wang, Qinting ; Cao, Zhengzheng</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-a1826-335688adc3e07a8247fe8dcdf0c2aa489157c37bf518a3b616670e34541847343</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2022</creationdate><topic>Building materials</topic><topic>Civil engineering</topic><topic>Compressive strength</topic><topic>Damage</topic><topic>Deterioration</topic><topic>High temperature</topic><topic>Mechanical properties</topic><topic>Moisture content</topic><topic>Moisture effects</topic><topic>Nondestructive testing</topic><topic>Spalling</topic><topic>Technical Papers</topic><topic>Temperature</topic><topic>Ultrasonic testing</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Wu, Xiaogang</creatorcontrib><creatorcontrib>Yang, Jianhui</creatorcontrib><creatorcontrib>Lin, Haixiao</creatorcontrib><creatorcontrib>Wang, Qinting</creatorcontrib><creatorcontrib>Cao, Zhengzheng</creatorcontrib><collection>CrossRef</collection><collection>Technology Research Database</collection><collection>Engineering Research Database</collection><collection>Civil Engineering Abstracts</collection><jtitle>Journal of materials in civil engineering</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Wu, Xiaogang</au><au>Yang, Jianhui</au><au>Lin, Haixiao</au><au>Wang, Qinting</au><au>Cao, Zhengzheng</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Mechanical Properties and Damage Mechanism of Shale Ceramsite Concrete after High-Temperature Treatment</atitle><jtitle>Journal of materials in civil engineering</jtitle><date>2022-07-01</date><risdate>2022</risdate><volume>34</volume><issue>7</issue><issn>0899-1561</issn><eissn>1943-5533</eissn><abstract>AbstractThe high-temperature resistance of lightweight shale ceramsite concrete (LWSCC) is seriously underestimated because the effect of moisture is not considered. To investigate the mechanical properties and damage of LWSCC after a high-temperature treatment, strength tests, X-ray diffraction (XRD), and scanning electron microscopy (SEM) were carried out, and a nondestructive ultrasonic testing device was used to quantify the damage. The results show that the spalling characteristics of LWSCC at high temperatures were closely related to its water content. The axial compressive strength of LWSCC linearly decreased with increasing target temperature. LWSCC showed a greater resistance to high-temperature deterioration than NWC with the same mass loss ratio. LWSCC with a moisture content of 4.1% had a high probability of spalling at temperatures above 500°C. However, dry LWSCC had a low probability of spalling even when heated to 800°C. Water in shale ceramsite with a porous structure was identified as a critical factor in the high-temperature deterioration. After the temperature exceeded 200°C, the high-pressure steam in the ceramsite expanded the cracks. These findings provide a basis for designing LWSCC with high-temperature resistance and evaluating the safety of LWSCC buildings after fires.</abstract><cop>New York</cop><pub>American Society of Civil Engineers</pub><doi>10.1061/(ASCE)MT.1943-5533.0004279</doi></addata></record> |
fulltext | fulltext |
identifier | ISSN: 0899-1561 |
ispartof | Journal of materials in civil engineering, 2022-07, Vol.34 (7) |
issn | 0899-1561 1943-5533 |
language | eng |
recordid | cdi_proquest_journals_2652585426 |
source | American Society of Civil Engineers:NESLI2:Journals:2014 |
subjects | Building materials Civil engineering Compressive strength Damage Deterioration High temperature Mechanical properties Moisture content Moisture effects Nondestructive testing Spalling Technical Papers Temperature Ultrasonic testing |
title | Mechanical Properties and Damage Mechanism of Shale Ceramsite Concrete after High-Temperature Treatment |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-02T16%3A34%3A59IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Mechanical%20Properties%20and%20Damage%20Mechanism%20of%20Shale%20Ceramsite%20Concrete%20after%20High-Temperature%20Treatment&rft.jtitle=Journal%20of%20materials%20in%20civil%20engineering&rft.au=Wu,%20Xiaogang&rft.date=2022-07-01&rft.volume=34&rft.issue=7&rft.issn=0899-1561&rft.eissn=1943-5533&rft_id=info:doi/10.1061/(ASCE)MT.1943-5533.0004279&rft_dat=%3Cproquest_cross%3E2652585426%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=2652585426&rft_id=info:pmid/&rfr_iscdi=true |