Process control agent effect on the structural and magnetic properties of mechanically alloyed Fe(Al) disordered system

•The effects of ethanol during the mechanical alloying of Fe(Al) were investigated.•Fe(Al) disordered phase was reached after 6 hours of milling at 25 Hz without ethanol .•No presence of ethanol provokes high adherence of the powders to the milling tools..•Ethanol addition allowed a recovery rate of...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of magnetism and magnetic materials 2021-11, Vol.538, p.168246, Article 168246
Hauptverfasser: Montoya Rangel, Marvin, Marín Ramírez, Juan Marcos, Tirado Mejía, Liliana, Medina Barreto, Milton Humberto, Cruz Muñoz, Beatriz
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page 168246
container_title Journal of magnetism and magnetic materials
container_volume 538
creator Montoya Rangel, Marvin
Marín Ramírez, Juan Marcos
Tirado Mejía, Liliana
Medina Barreto, Milton Humberto
Cruz Muñoz, Beatriz
description •The effects of ethanol during the mechanical alloying of Fe(Al) were investigated.•Fe(Al) disordered phase was reached after 6 hours of milling at 25 Hz without ethanol .•No presence of ethanol provokes high adherence of the powders to the milling tools..•Ethanol addition allowed a recovery rate of the initial mixed powders up to 96%.•Ethanol inhibits the Fe(Al) phase formation even for prolonged milling times. The effect of ethanol as a process control agent (PCA) on the mechanical alloying (MA) of Fe-20 at. % Al powders is presented. MA was performed at room temperature in an oscillation ball mill and its dynamic was studied by changing the milling frequency and time. We characterized the milled powders using X-ray diffraction (XRD), Mössbauer spectroscopy, and vibrating sample magnetometry (VSM). X-ray patterns for the milled powders without PCA showed a rapid formation of the disordered Fe(Al) solid solution after 25 Hz for 6 h of milling. Mössbauer spectroscopy confirmed two ferromagnetic sites related to the α-Fe phase and Fe(Al) disordered solid solution. However, intense cold welding of the powders to the milling tools for all milling frequencies led to a powder recovery of only 40% on average. The addition of ethanol as a PCA at a 25 Hz increased the powder recovery up to 96% even for different milling times, whereas X-ray diffraction and Mössbauer spectra showed a single α-Fe phase. VSM results exhibit the presence of a soft ferromagnetic character, in which a correlation between the structural parameters with the coercive field and saturation magnetization was deduced. Thus, while ethanol increases the powder recovery rate it also modifies the milling kinetics affecting the domain walls’ movement and the corresponding magnetic interactions between iron atoms.
doi_str_mv 10.1016/j.jmmm.2021.168246
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_journals_2575097856</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0304885321005229</els_id><sourcerecordid>2575097856</sourcerecordid><originalsourceid>FETCH-LOGICAL-c328t-e0d9157266ab1b696941ae32a234ad3377d436f6ec19ddd83bb443e3d6dff29a3</originalsourceid><addsrcrecordid>eNp9kE9LAzEQxYMoWKtfwFPAix625t9md8FLEatCQQ96Dmky22bZ3dQkVfrtTalnLzMw897M44fQNSUzSqi872bdMAwzRhidUVkzIU_QhNYVL0Ql5SmaEE5EUdclP0cXMXaEECpqOUE_78EbiBEbP6bge6zXMCYMbQsmYT_itAEcU9iZtAs6r0eLB70eITmDt8FvISQHEfsWD2A2enRG9_0e5-L3YPECbuf9HbYu-mAh5EncxwTDJTprdR_h6q9P0efi6ePxpVi-Pb8-zpeF4axOBRDb0LJiUuoVXclGNoJq4EwzLrTlvKqs4LKVYGhjra35aiUEB26lbVvWaD5FN8e7OevXDmJSnd-FMb9UrKxK0lR1KbOKHVUm-BgDtGob3KDDXlGiDoBVpw6A1QGwOgLOpoejCXL-bwdBReNgNGBdyPCU9e4_-y-9UoYJ</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>2575097856</pqid></control><display><type>article</type><title>Process control agent effect on the structural and magnetic properties of mechanically alloyed Fe(Al) disordered system</title><source>Access via ScienceDirect (Elsevier)</source><creator>Montoya Rangel, Marvin ; Marín Ramírez, Juan Marcos ; Tirado Mejía, Liliana ; Medina Barreto, Milton Humberto ; Cruz Muñoz, Beatriz</creator><creatorcontrib>Montoya Rangel, Marvin ; Marín Ramírez, Juan Marcos ; Tirado Mejía, Liliana ; Medina Barreto, Milton Humberto ; Cruz Muñoz, Beatriz</creatorcontrib><description>•The effects of ethanol during the mechanical alloying of Fe(Al) were investigated.•Fe(Al) disordered phase was reached after 6 hours of milling at 25 Hz without ethanol .•No presence of ethanol provokes high adherence of the powders to the milling tools..•Ethanol addition allowed a recovery rate of the initial mixed powders up to 96%.•Ethanol inhibits the Fe(Al) phase formation even for prolonged milling times. The effect of ethanol as a process control agent (PCA) on the mechanical alloying (MA) of Fe-20 at. % Al powders is presented. MA was performed at room temperature in an oscillation ball mill and its dynamic was studied by changing the milling frequency and time. We characterized the milled powders using X-ray diffraction (XRD), Mössbauer spectroscopy, and vibrating sample magnetometry (VSM). X-ray patterns for the milled powders without PCA showed a rapid formation of the disordered Fe(Al) solid solution after 25 Hz for 6 h of milling. Mössbauer spectroscopy confirmed two ferromagnetic sites related to the α-Fe phase and Fe(Al) disordered solid solution. However, intense cold welding of the powders to the milling tools for all milling frequencies led to a powder recovery of only 40% on average. The addition of ethanol as a PCA at a 25 Hz increased the powder recovery up to 96% even for different milling times, whereas X-ray diffraction and Mössbauer spectra showed a single α-Fe phase. VSM results exhibit the presence of a soft ferromagnetic character, in which a correlation between the structural parameters with the coercive field and saturation magnetization was deduced. Thus, while ethanol increases the powder recovery rate it also modifies the milling kinetics affecting the domain walls’ movement and the corresponding magnetic interactions between iron atoms.</description><identifier>ISSN: 0304-8853</identifier><identifier>EISSN: 1873-4766</identifier><identifier>DOI: 10.1016/j.jmmm.2021.168246</identifier><language>eng</language><publisher>Amsterdam: Elsevier B.V</publisher><subject>Ball milling ; Ball mills ; Coercivity ; Cold welding ; Diffraction patterns ; Domain walls ; Ethanol ; Fe(Al) disordered alloy ; Ferromagnetism ; Iron ; Magnetic measurement ; Magnetic properties ; Magnetic saturation ; Mechanical alloying ; Mossbauer spectroscopy ; Mössbauer spectroscopy ; Powder metallurgy ; Process control agent ; Process controls ; Recovery ; Room temperature ; Solid solutions ; Spectrum analysis ; X-ray diffraction</subject><ispartof>Journal of magnetism and magnetic materials, 2021-11, Vol.538, p.168246, Article 168246</ispartof><rights>2021 Elsevier B.V.</rights><rights>Copyright Elsevier BV Nov 15, 2021</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c328t-e0d9157266ab1b696941ae32a234ad3377d436f6ec19ddd83bb443e3d6dff29a3</citedby><cites>FETCH-LOGICAL-c328t-e0d9157266ab1b696941ae32a234ad3377d436f6ec19ddd83bb443e3d6dff29a3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://dx.doi.org/10.1016/j.jmmm.2021.168246$$EHTML$$P50$$Gelsevier$$H</linktohtml><link.rule.ids>314,780,784,3550,27924,27925,45995</link.rule.ids></links><search><creatorcontrib>Montoya Rangel, Marvin</creatorcontrib><creatorcontrib>Marín Ramírez, Juan Marcos</creatorcontrib><creatorcontrib>Tirado Mejía, Liliana</creatorcontrib><creatorcontrib>Medina Barreto, Milton Humberto</creatorcontrib><creatorcontrib>Cruz Muñoz, Beatriz</creatorcontrib><title>Process control agent effect on the structural and magnetic properties of mechanically alloyed Fe(Al) disordered system</title><title>Journal of magnetism and magnetic materials</title><description>•The effects of ethanol during the mechanical alloying of Fe(Al) were investigated.•Fe(Al) disordered phase was reached after 6 hours of milling at 25 Hz without ethanol .•No presence of ethanol provokes high adherence of the powders to the milling tools..•Ethanol addition allowed a recovery rate of the initial mixed powders up to 96%.•Ethanol inhibits the Fe(Al) phase formation even for prolonged milling times. The effect of ethanol as a process control agent (PCA) on the mechanical alloying (MA) of Fe-20 at. % Al powders is presented. MA was performed at room temperature in an oscillation ball mill and its dynamic was studied by changing the milling frequency and time. We characterized the milled powders using X-ray diffraction (XRD), Mössbauer spectroscopy, and vibrating sample magnetometry (VSM). X-ray patterns for the milled powders without PCA showed a rapid formation of the disordered Fe(Al) solid solution after 25 Hz for 6 h of milling. Mössbauer spectroscopy confirmed two ferromagnetic sites related to the α-Fe phase and Fe(Al) disordered solid solution. However, intense cold welding of the powders to the milling tools for all milling frequencies led to a powder recovery of only 40% on average. The addition of ethanol as a PCA at a 25 Hz increased the powder recovery up to 96% even for different milling times, whereas X-ray diffraction and Mössbauer spectra showed a single α-Fe phase. VSM results exhibit the presence of a soft ferromagnetic character, in which a correlation between the structural parameters with the coercive field and saturation magnetization was deduced. Thus, while ethanol increases the powder recovery rate it also modifies the milling kinetics affecting the domain walls’ movement and the corresponding magnetic interactions between iron atoms.</description><subject>Ball milling</subject><subject>Ball mills</subject><subject>Coercivity</subject><subject>Cold welding</subject><subject>Diffraction patterns</subject><subject>Domain walls</subject><subject>Ethanol</subject><subject>Fe(Al) disordered alloy</subject><subject>Ferromagnetism</subject><subject>Iron</subject><subject>Magnetic measurement</subject><subject>Magnetic properties</subject><subject>Magnetic saturation</subject><subject>Mechanical alloying</subject><subject>Mossbauer spectroscopy</subject><subject>Mössbauer spectroscopy</subject><subject>Powder metallurgy</subject><subject>Process control agent</subject><subject>Process controls</subject><subject>Recovery</subject><subject>Room temperature</subject><subject>Solid solutions</subject><subject>Spectrum analysis</subject><subject>X-ray diffraction</subject><issn>0304-8853</issn><issn>1873-4766</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2021</creationdate><recordtype>article</recordtype><recordid>eNp9kE9LAzEQxYMoWKtfwFPAix625t9md8FLEatCQQ96Dmky22bZ3dQkVfrtTalnLzMw897M44fQNSUzSqi872bdMAwzRhidUVkzIU_QhNYVL0Ql5SmaEE5EUdclP0cXMXaEECpqOUE_78EbiBEbP6bge6zXMCYMbQsmYT_itAEcU9iZtAs6r0eLB70eITmDt8FvISQHEfsWD2A2enRG9_0e5-L3YPECbuf9HbYu-mAh5EncxwTDJTprdR_h6q9P0efi6ePxpVi-Pb8-zpeF4axOBRDb0LJiUuoVXclGNoJq4EwzLrTlvKqs4LKVYGhjra35aiUEB26lbVvWaD5FN8e7OevXDmJSnd-FMb9UrKxK0lR1KbOKHVUm-BgDtGob3KDDXlGiDoBVpw6A1QGwOgLOpoejCXL-bwdBReNgNGBdyPCU9e4_-y-9UoYJ</recordid><startdate>20211115</startdate><enddate>20211115</enddate><creator>Montoya Rangel, Marvin</creator><creator>Marín Ramírez, Juan Marcos</creator><creator>Tirado Mejía, Liliana</creator><creator>Medina Barreto, Milton Humberto</creator><creator>Cruz Muñoz, Beatriz</creator><general>Elsevier B.V</general><general>Elsevier BV</general><scope>AAYXX</scope><scope>CITATION</scope><scope>7SR</scope><scope>7U5</scope><scope>8BQ</scope><scope>8FD</scope><scope>JG9</scope><scope>L7M</scope></search><sort><creationdate>20211115</creationdate><title>Process control agent effect on the structural and magnetic properties of mechanically alloyed Fe(Al) disordered system</title><author>Montoya Rangel, Marvin ; Marín Ramírez, Juan Marcos ; Tirado Mejía, Liliana ; Medina Barreto, Milton Humberto ; Cruz Muñoz, Beatriz</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c328t-e0d9157266ab1b696941ae32a234ad3377d436f6ec19ddd83bb443e3d6dff29a3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2021</creationdate><topic>Ball milling</topic><topic>Ball mills</topic><topic>Coercivity</topic><topic>Cold welding</topic><topic>Diffraction patterns</topic><topic>Domain walls</topic><topic>Ethanol</topic><topic>Fe(Al) disordered alloy</topic><topic>Ferromagnetism</topic><topic>Iron</topic><topic>Magnetic measurement</topic><topic>Magnetic properties</topic><topic>Magnetic saturation</topic><topic>Mechanical alloying</topic><topic>Mossbauer spectroscopy</topic><topic>Mössbauer spectroscopy</topic><topic>Powder metallurgy</topic><topic>Process control agent</topic><topic>Process controls</topic><topic>Recovery</topic><topic>Room temperature</topic><topic>Solid solutions</topic><topic>Spectrum analysis</topic><topic>X-ray diffraction</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Montoya Rangel, Marvin</creatorcontrib><creatorcontrib>Marín Ramírez, Juan Marcos</creatorcontrib><creatorcontrib>Tirado Mejía, Liliana</creatorcontrib><creatorcontrib>Medina Barreto, Milton Humberto</creatorcontrib><creatorcontrib>Cruz Muñoz, Beatriz</creatorcontrib><collection>CrossRef</collection><collection>Engineered Materials Abstracts</collection><collection>Solid State and Superconductivity Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><collection>Advanced Technologies Database with Aerospace</collection><jtitle>Journal of magnetism and magnetic materials</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Montoya Rangel, Marvin</au><au>Marín Ramírez, Juan Marcos</au><au>Tirado Mejía, Liliana</au><au>Medina Barreto, Milton Humberto</au><au>Cruz Muñoz, Beatriz</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Process control agent effect on the structural and magnetic properties of mechanically alloyed Fe(Al) disordered system</atitle><jtitle>Journal of magnetism and magnetic materials</jtitle><date>2021-11-15</date><risdate>2021</risdate><volume>538</volume><spage>168246</spage><pages>168246-</pages><artnum>168246</artnum><issn>0304-8853</issn><eissn>1873-4766</eissn><abstract>•The effects of ethanol during the mechanical alloying of Fe(Al) were investigated.•Fe(Al) disordered phase was reached after 6 hours of milling at 25 Hz without ethanol .•No presence of ethanol provokes high adherence of the powders to the milling tools..•Ethanol addition allowed a recovery rate of the initial mixed powders up to 96%.•Ethanol inhibits the Fe(Al) phase formation even for prolonged milling times. The effect of ethanol as a process control agent (PCA) on the mechanical alloying (MA) of Fe-20 at. % Al powders is presented. MA was performed at room temperature in an oscillation ball mill and its dynamic was studied by changing the milling frequency and time. We characterized the milled powders using X-ray diffraction (XRD), Mössbauer spectroscopy, and vibrating sample magnetometry (VSM). X-ray patterns for the milled powders without PCA showed a rapid formation of the disordered Fe(Al) solid solution after 25 Hz for 6 h of milling. Mössbauer spectroscopy confirmed two ferromagnetic sites related to the α-Fe phase and Fe(Al) disordered solid solution. However, intense cold welding of the powders to the milling tools for all milling frequencies led to a powder recovery of only 40% on average. The addition of ethanol as a PCA at a 25 Hz increased the powder recovery up to 96% even for different milling times, whereas X-ray diffraction and Mössbauer spectra showed a single α-Fe phase. VSM results exhibit the presence of a soft ferromagnetic character, in which a correlation between the structural parameters with the coercive field and saturation magnetization was deduced. Thus, while ethanol increases the powder recovery rate it also modifies the milling kinetics affecting the domain walls’ movement and the corresponding magnetic interactions between iron atoms.</abstract><cop>Amsterdam</cop><pub>Elsevier B.V</pub><doi>10.1016/j.jmmm.2021.168246</doi></addata></record>
fulltext fulltext
identifier ISSN: 0304-8853
ispartof Journal of magnetism and magnetic materials, 2021-11, Vol.538, p.168246, Article 168246
issn 0304-8853
1873-4766
language eng
recordid cdi_proquest_journals_2575097856
source Access via ScienceDirect (Elsevier)
subjects Ball milling
Ball mills
Coercivity
Cold welding
Diffraction patterns
Domain walls
Ethanol
Fe(Al) disordered alloy
Ferromagnetism
Iron
Magnetic measurement
Magnetic properties
Magnetic saturation
Mechanical alloying
Mossbauer spectroscopy
Mössbauer spectroscopy
Powder metallurgy
Process control agent
Process controls
Recovery
Room temperature
Solid solutions
Spectrum analysis
X-ray diffraction
title Process control agent effect on the structural and magnetic properties of mechanically alloyed Fe(Al) disordered system
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-01T21%3A25%3A13IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Process%20control%20agent%20effect%20on%20the%20structural%20and%20magnetic%20properties%20of%20mechanically%20alloyed%20Fe(Al)%20disordered%20system&rft.jtitle=Journal%20of%20magnetism%20and%20magnetic%20materials&rft.au=Montoya%20Rangel,%20Marvin&rft.date=2021-11-15&rft.volume=538&rft.spage=168246&rft.pages=168246-&rft.artnum=168246&rft.issn=0304-8853&rft.eissn=1873-4766&rft_id=info:doi/10.1016/j.jmmm.2021.168246&rft_dat=%3Cproquest_cross%3E2575097856%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=2575097856&rft_id=info:pmid/&rft_els_id=S0304885321005229&rfr_iscdi=true