Magnetic behavior in commercial iron-silicon alloys controlled by the dislocation dynamics at temperatures below 420 K

A decrease of the temperature dependent coercive forces up to around 370 K is discovered in iron silicon alloys, both in quenched samples and in samples which were previously thermally treated to achieve the highest magnetic quality. Alloys of composition Fe-6 wt.% Si and Fe-3 wt.% Si are studied. T...