Formation of TaB2 powders from high energy ball milling and borothermal reduction process

TaB2 powders were fabricated at reduced temperatures via borothermal reduction route by high energy ball milling of Ta2O5 and B powder blends. The effects of milling media (Steel, ZrO2 and WC), milling time (1,3,5 and 7 h) and heat treatment temperature (1650 °C and 1350 °C) on the formation and mic...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials chemistry and physics 2019-09, Vol.235, p.121732, Article 121732
Hauptverfasser: Gürcan, Kübra, Ayas, Erhan, Gaşan, Hakan
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!