High-K Dielectric Ceramics from Donor/Acceptor-Codoped (Ba1−xCax)(Ti1-yZry)O3 (BCTZ)
(Ba1−xCax)(Ti1−yZry)O3 ceramics doped with various donors and acceptors were sintered in a reducing atmosphere and then annealed at different oxygen partial pressures. The dielectric maxima at the Curie point increased up to ∼30000 after reoxidation, depending on the grain size, the type of acceptor...
Gespeichert in:
Veröffentlicht in: | Journal of the American Ceramic Society 1998-05, Vol.81 (5), p.1369-1373 |
---|---|
Hauptverfasser: | , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | 1373 |
---|---|
container_issue | 5 |
container_start_page | 1369 |
container_title | Journal of the American Ceramic Society |
container_volume | 81 |
creator | Hansen, Peter Hennings, Detlev Schreinemacher, Herbert |
description | (Ba1−xCax)(Ti1−yZry)O3 ceramics doped with various donors and acceptors were sintered in a reducing atmosphere and then annealed at different oxygen partial pressures. The dielectric maxima at the Curie point increased up to ∼30000 after reoxidation, depending on the grain size, the type of acceptor, and the annealing conditions. The increase of the dielectric maxima seems to be correlated with oxidation of the grain boundaries. The dielectric properties show relaxation effects with increased frequency. |
doi_str_mv | 10.1111/j.1151-2916.1998.tb02494.x |
format | Article |
fullrecord | <record><control><sourceid>proquest_pasca</sourceid><recordid>TN_cdi_proquest_journals_217894963</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>41254786</sourcerecordid><originalsourceid>FETCH-LOGICAL-i2859-c024a2c32e09b55a9403d0ee073a10bc5fb1ada26f998556964bbbe7f0faca0a3</originalsourceid><addsrcrecordid>eNo9kE1OwzAQhS0EEuXnDhFi0S5cbCd24h0lhfJTQEIFpG6sieuAS9sEJ4j0Bqw5IifBVavOZjR6T29mPoROKOlSX2dT3zjFTFLRpVIm3TojLJJRt9lBLco30i5qEUIYjhNG9tFBVU39SGUStdDLtX17x3dB35qZ0bWzOkiNg7nVVZC7Yh70i0Xhznpam7IuHE6LSVGaSdC-APr389uk0HTaI0vxcuyWncfQC-lo3DlCeznMKnO86Yfo-epylF7j4ePgJu0NsWUJl1j7Y4HpkBkiM85BRiScEGNIHAIlmeZ5RmECTOT-N86FFFGWZSbOSQ4aCISH6GSdW7ri88tUtZoWX27hVypG40RGUoTedLoxQaVhljtYaFup0tk5uKViTBAuYm87X9u-7cwstzIlaoVaTdUKtVrxVCvUaoNaNeq2l17SUEgfgdcRtqpNs40A96H8gpir14eBehqOh_eDW6Hi8B_ZpILJ</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>217894963</pqid></control><display><type>article</type><title>High-K Dielectric Ceramics from Donor/Acceptor-Codoped (Ba1−xCax)(Ti1-yZry)O3 (BCTZ)</title><source>Access via Wiley Online Library</source><creator>Hansen, Peter ; Hennings, Detlev ; Schreinemacher, Herbert</creator><creatorcontrib>Hansen, Peter ; Hennings, Detlev ; Schreinemacher, Herbert</creatorcontrib><description>(Ba1−xCax)(Ti1−yZry)O3 ceramics doped with various donors and acceptors were sintered in a reducing atmosphere and then annealed at different oxygen partial pressures. The dielectric maxima at the Curie point increased up to ∼30000 after reoxidation, depending on the grain size, the type of acceptor, and the annealing conditions. The increase of the dielectric maxima seems to be correlated with oxidation of the grain boundaries. The dielectric properties show relaxation effects with increased frequency.</description><identifier>ISSN: 0002-7820</identifier><identifier>EISSN: 1551-2916</identifier><identifier>DOI: 10.1111/j.1151-2916.1998.tb02494.x</identifier><identifier>CODEN: JACTAW</identifier><language>eng</language><publisher>Westerville, Ohio: American Ceramics Society</publisher><subject>Applied sciences ; Building materials. Ceramics. Glasses ; Ceramic industries ; Chemical industry and chemicals ; Electrotechnical and electronic ceramics ; Exact sciences and technology ; Technical ceramics</subject><ispartof>Journal of the American Ceramic Society, 1998-05, Vol.81 (5), p.1369-1373</ispartof><rights>1998 INIST-CNRS</rights><rights>Copyright American Ceramic Society May 1998</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktopdf>$$Uhttps://onlinelibrary.wiley.com/doi/pdf/10.1111%2Fj.1151-2916.1998.tb02494.x$$EPDF$$P50$$Gwiley$$H</linktopdf><linktohtml>$$Uhttps://onlinelibrary.wiley.com/doi/full/10.1111%2Fj.1151-2916.1998.tb02494.x$$EHTML$$P50$$Gwiley$$H</linktohtml><link.rule.ids>314,780,784,1417,27924,27925,45574,45575</link.rule.ids><backlink>$$Uhttp://pascal-francis.inist.fr/vibad/index.php?action=getRecordDetail&idt=2260567$$DView record in Pascal Francis$$Hfree_for_read</backlink></links><search><creatorcontrib>Hansen, Peter</creatorcontrib><creatorcontrib>Hennings, Detlev</creatorcontrib><creatorcontrib>Schreinemacher, Herbert</creatorcontrib><title>High-K Dielectric Ceramics from Donor/Acceptor-Codoped (Ba1−xCax)(Ti1-yZry)O3 (BCTZ)</title><title>Journal of the American Ceramic Society</title><description>(Ba1−xCax)(Ti1−yZry)O3 ceramics doped with various donors and acceptors were sintered in a reducing atmosphere and then annealed at different oxygen partial pressures. The dielectric maxima at the Curie point increased up to ∼30000 after reoxidation, depending on the grain size, the type of acceptor, and the annealing conditions. The increase of the dielectric maxima seems to be correlated with oxidation of the grain boundaries. The dielectric properties show relaxation effects with increased frequency.</description><subject>Applied sciences</subject><subject>Building materials. Ceramics. Glasses</subject><subject>Ceramic industries</subject><subject>Chemical industry and chemicals</subject><subject>Electrotechnical and electronic ceramics</subject><subject>Exact sciences and technology</subject><subject>Technical ceramics</subject><issn>0002-7820</issn><issn>1551-2916</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>1998</creationdate><recordtype>article</recordtype><recordid>eNo9kE1OwzAQhS0EEuXnDhFi0S5cbCd24h0lhfJTQEIFpG6sieuAS9sEJ4j0Bqw5IifBVavOZjR6T29mPoROKOlSX2dT3zjFTFLRpVIm3TojLJJRt9lBLco30i5qEUIYjhNG9tFBVU39SGUStdDLtX17x3dB35qZ0bWzOkiNg7nVVZC7Yh70i0Xhznpam7IuHE6LSVGaSdC-APr389uk0HTaI0vxcuyWncfQC-lo3DlCeznMKnO86Yfo-epylF7j4ePgJu0NsWUJl1j7Y4HpkBkiM85BRiScEGNIHAIlmeZ5RmECTOT-N86FFFGWZSbOSQ4aCISH6GSdW7ri88tUtZoWX27hVypG40RGUoTedLoxQaVhljtYaFup0tk5uKViTBAuYm87X9u-7cwstzIlaoVaTdUKtVrxVCvUaoNaNeq2l17SUEgfgdcRtqpNs40A96H8gpir14eBehqOh_eDW6Hi8B_ZpILJ</recordid><startdate>199805</startdate><enddate>199805</enddate><creator>Hansen, Peter</creator><creator>Hennings, Detlev</creator><creator>Schreinemacher, Herbert</creator><general>American Ceramics Society</general><general>Blackwell</general><general>Wiley Subscription Services, Inc</general><scope>BSCLL</scope><scope>IQODW</scope><scope>7QQ</scope><scope>7SR</scope><scope>8FD</scope><scope>JG9</scope></search><sort><creationdate>199805</creationdate><title>High-K Dielectric Ceramics from Donor/Acceptor-Codoped (Ba1−xCax)(Ti1-yZry)O3 (BCTZ)</title><author>Hansen, Peter ; Hennings, Detlev ; Schreinemacher, Herbert</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-i2859-c024a2c32e09b55a9403d0ee073a10bc5fb1ada26f998556964bbbe7f0faca0a3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>1998</creationdate><topic>Applied sciences</topic><topic>Building materials. Ceramics. Glasses</topic><topic>Ceramic industries</topic><topic>Chemical industry and chemicals</topic><topic>Electrotechnical and electronic ceramics</topic><topic>Exact sciences and technology</topic><topic>Technical ceramics</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Hansen, Peter</creatorcontrib><creatorcontrib>Hennings, Detlev</creatorcontrib><creatorcontrib>Schreinemacher, Herbert</creatorcontrib><collection>Istex</collection><collection>Pascal-Francis</collection><collection>Ceramic Abstracts</collection><collection>Engineered Materials Abstracts</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><jtitle>Journal of the American Ceramic Society</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Hansen, Peter</au><au>Hennings, Detlev</au><au>Schreinemacher, Herbert</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>High-K Dielectric Ceramics from Donor/Acceptor-Codoped (Ba1−xCax)(Ti1-yZry)O3 (BCTZ)</atitle><jtitle>Journal of the American Ceramic Society</jtitle><date>1998-05</date><risdate>1998</risdate><volume>81</volume><issue>5</issue><spage>1369</spage><epage>1373</epage><pages>1369-1373</pages><issn>0002-7820</issn><eissn>1551-2916</eissn><coden>JACTAW</coden><abstract>(Ba1−xCax)(Ti1−yZry)O3 ceramics doped with various donors and acceptors were sintered in a reducing atmosphere and then annealed at different oxygen partial pressures. The dielectric maxima at the Curie point increased up to ∼30000 after reoxidation, depending on the grain size, the type of acceptor, and the annealing conditions. The increase of the dielectric maxima seems to be correlated with oxidation of the grain boundaries. The dielectric properties show relaxation effects with increased frequency.</abstract><cop>Westerville, Ohio</cop><pub>American Ceramics Society</pub><doi>10.1111/j.1151-2916.1998.tb02494.x</doi><tpages>5</tpages></addata></record> |
fulltext | fulltext |
identifier | ISSN: 0002-7820 |
ispartof | Journal of the American Ceramic Society, 1998-05, Vol.81 (5), p.1369-1373 |
issn | 0002-7820 1551-2916 |
language | eng |
recordid | cdi_proquest_journals_217894963 |
source | Access via Wiley Online Library |
subjects | Applied sciences Building materials. Ceramics. Glasses Ceramic industries Chemical industry and chemicals Electrotechnical and electronic ceramics Exact sciences and technology Technical ceramics |
title | High-K Dielectric Ceramics from Donor/Acceptor-Codoped (Ba1−xCax)(Ti1-yZry)O3 (BCTZ) |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-27T21%3A18%3A03IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_pasca&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=High-K%20Dielectric%20Ceramics%20from%20Donor/Acceptor-Codoped%20(Ba1%E2%88%92xCax)(Ti1-yZry)O3%20(BCTZ)&rft.jtitle=Journal%20of%20the%20American%20Ceramic%20Society&rft.au=Hansen,%20Peter&rft.date=1998-05&rft.volume=81&rft.issue=5&rft.spage=1369&rft.epage=1373&rft.pages=1369-1373&rft.issn=0002-7820&rft.eissn=1551-2916&rft.coden=JACTAW&rft_id=info:doi/10.1111/j.1151-2916.1998.tb02494.x&rft_dat=%3Cproquest_pasca%3E41254786%3C/proquest_pasca%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=217894963&rft_id=info:pmid/&rfr_iscdi=true |