Melt-derived bioactive glass based on SiO^sub 2^-CaO-Na^sub 2^O-P^sub 2^O^sub 5^ system fabricated at lower melting temperature
This work addresses the development and fabrication of new bioactive glass composition based on SiO2-CaO-Na2O-P2O5 system that can be melted at lower melting temperature (1377 °C and 1348 °C) than 1400 °C through melt-derived route. All BG compositions did not show significant differences on their p...