Nanoindentation and wear properties of Ti and Ti-TiB composite materials produced by selective laser melting

Ti and Ti-TiB composite materials were produced by selective laser melting (SLM). Ti showed an α΄ microstructure, whereas the Ti-TiB composite revealed a distribution of needle-like TiB particles across an α-Ti matrix. Hardness (H) and reduced elastic modulus (Er) were investigated by nanoindentatio...