Distribution and Behavior of Arsenic During the Reducing-Matting Smelting Process
The distribution and behavior of arsenic during the reducing-matting smelting process were investigated with various values of the carbon addition ratio, arsenic content, CaO/SiO 2 ratio, and Fe/SiO 2 ratio. The carbon addition ratio significantly affected the arsenic distribution among the phases,...