Desempeño de insertos de WC recubiertos con nanomulticapas de [TiN/TiAlN]^sub n^ en el mecanizado del acero endurecido AISI 4340/Performance of WC- inserts coated with nanometric [TiN/TiAlN]^sub n^- multilayer for the cutting processing of hardened AISI 4340 steel
In this paper, wear resistance of 4 μm uncoated tungsten carbide inserts (WC) and coated with (TiN/TiAlN)n multinanolayered or with commercial TiCN-Al2O3-TiN monolayers (TINAL) are examined. Life tests, cutting area temperature analysis, surface roughness measurements on work pieces, roughness measu...
Gespeichert in:
Veröffentlicht in: | Revista Facultad de Ingeniería 2011-03 (58), p.85 |
---|---|
Hauptverfasser: | , , , , |
Format: | Artikel |
Sprache: | spa |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | 58 |
container_start_page | 85 |
container_title | Revista Facultad de Ingeniería |
container_volume | |
creator | Moreno, Luis Henry Caicedo, Julio Cesar Gaitan, Gilberto Bejarano Martínez, Federico Pulido, Pedro Prieto |
description | In this paper, wear resistance of 4 μm uncoated tungsten carbide inserts (WC) and coated with (TiN/TiAlN)n multinanolayered or with commercial TiCN-Al2O3-TiN monolayers (TINAL) are examined. Life tests, cutting area temperature analysis, surface roughness measurements on work pieces, roughness measurements on the attacked surface, contact track analysis between chip-insert and chemical composition analysis were carried out. Mechanical tests were conducted on AISI 4340 steel parts using cutting regime and applying high speed cutting. The machining results showed that for a distance of 8,000 m the inserts coated with 300 bilayers exhibited wear values of 0.117 mm, inserts coated with 200 bilayers showed values of 0.138 mm and those coated with TINAL presented wear values of 0.174 mm. Moreover, the temperature values for cutting speed at 176.6 m/mim for 300 bilayers was 522.6°C, for 200 bilayers was 721.4 °C and 1,327.6°C for inserts coated with TINAL. Lower temperatures, caused by a lower friction coefficient and cutting force, contribute to life-time increasing at WC inserts. |
format | Article |
fullrecord | <record><control><sourceid>proquest</sourceid><recordid>TN_cdi_proquest_journals_1612427122</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>3462537421</sourcerecordid><originalsourceid>FETCH-proquest_journals_16124271223</originalsourceid><addsrcrecordid>eNqNkE1OwzAQhQMCifBzh5FYR3UcE7KtCohuKiQisUC0cp0JceXYwT9CcCvOwMVw2ooVC1Yzmjfzvac5TFLKKM1oxdhRkpKckqykBTlJTp3bEHJVlaRKD9IbdNgP-P1loEGQ2qH1xo390wwsirCWu4kwGjTXpg_KS8EHvl16ruViUsupWrwsXViDXgJqQAU9Cq7lJ29GrgIu0JooNSEyZRxO549zYAUjkwe0rbE91wLBtNE228cYPbnHBt6l73be6K0Uf5hmsI2l-AdaiDTwHYII3kv9CoM1Ap0b28jvuG1QR-pvAnAeUZ0nxy1XDi_29Sy5vLutZ_dZPH8L6PxqY4LVUVrlZR5_e51TWvxv6wdiboCY</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1612427122</pqid></control><display><type>article</type><title>Desempeño de insertos de WC recubiertos con nanomulticapas de [TiN/TiAlN]^sub n^ en el mecanizado del acero endurecido AISI 4340/Performance of WC- inserts coated with nanometric [TiN/TiAlN]^sub n^- multilayer for the cutting processing of hardened AISI 4340 steel</title><source>Elektronische Zeitschriftenbibliothek - Frei zugängliche E-Journals</source><creator>Moreno, Luis Henry ; Caicedo, Julio Cesar ; Gaitan, Gilberto Bejarano ; Martínez, Federico ; Pulido, Pedro Prieto</creator><creatorcontrib>Moreno, Luis Henry ; Caicedo, Julio Cesar ; Gaitan, Gilberto Bejarano ; Martínez, Federico ; Pulido, Pedro Prieto</creatorcontrib><description>In this paper, wear resistance of 4 μm uncoated tungsten carbide inserts (WC) and coated with (TiN/TiAlN)n multinanolayered or with commercial TiCN-Al2O3-TiN monolayers (TINAL) are examined. Life tests, cutting area temperature analysis, surface roughness measurements on work pieces, roughness measurements on the attacked surface, contact track analysis between chip-insert and chemical composition analysis were carried out. Mechanical tests were conducted on AISI 4340 steel parts using cutting regime and applying high speed cutting. The machining results showed that for a distance of 8,000 m the inserts coated with 300 bilayers exhibited wear values of 0.117 mm, inserts coated with 200 bilayers showed values of 0.138 mm and those coated with TINAL presented wear values of 0.174 mm. Moreover, the temperature values for cutting speed at 176.6 m/mim for 300 bilayers was 522.6°C, for 200 bilayers was 721.4 °C and 1,327.6°C for inserts coated with TINAL. Lower temperatures, caused by a lower friction coefficient and cutting force, contribute to life-time increasing at WC inserts.</description><identifier>ISSN: 0120-6230</identifier><identifier>EISSN: 2422-2844</identifier><language>spa</language><publisher>Medellín: Universidad de Antioquía</publisher><ispartof>Revista Facultad de Ingeniería, 2011-03 (58), p.85</ispartof><rights>Copyright Universidad de Antioquia Mar 2011</rights><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>315,782,786</link.rule.ids></links><search><creatorcontrib>Moreno, Luis Henry</creatorcontrib><creatorcontrib>Caicedo, Julio Cesar</creatorcontrib><creatorcontrib>Gaitan, Gilberto Bejarano</creatorcontrib><creatorcontrib>Martínez, Federico</creatorcontrib><creatorcontrib>Pulido, Pedro Prieto</creatorcontrib><title>Desempeño de insertos de WC recubiertos con nanomulticapas de [TiN/TiAlN]^sub n^ en el mecanizado del acero endurecido AISI 4340/Performance of WC- inserts coated with nanometric [TiN/TiAlN]^sub n^- multilayer for the cutting processing of hardened AISI 4340 steel</title><title>Revista Facultad de Ingeniería</title><description>In this paper, wear resistance of 4 μm uncoated tungsten carbide inserts (WC) and coated with (TiN/TiAlN)n multinanolayered or with commercial TiCN-Al2O3-TiN monolayers (TINAL) are examined. Life tests, cutting area temperature analysis, surface roughness measurements on work pieces, roughness measurements on the attacked surface, contact track analysis between chip-insert and chemical composition analysis were carried out. Mechanical tests were conducted on AISI 4340 steel parts using cutting regime and applying high speed cutting. The machining results showed that for a distance of 8,000 m the inserts coated with 300 bilayers exhibited wear values of 0.117 mm, inserts coated with 200 bilayers showed values of 0.138 mm and those coated with TINAL presented wear values of 0.174 mm. Moreover, the temperature values for cutting speed at 176.6 m/mim for 300 bilayers was 522.6°C, for 200 bilayers was 721.4 °C and 1,327.6°C for inserts coated with TINAL. Lower temperatures, caused by a lower friction coefficient and cutting force, contribute to life-time increasing at WC inserts.</description><issn>0120-6230</issn><issn>2422-2844</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2011</creationdate><recordtype>article</recordtype><sourceid>ABUWG</sourceid><sourceid>AFKRA</sourceid><sourceid>AZQEC</sourceid><sourceid>BENPR</sourceid><sourceid>CCPQU</sourceid><sourceid>DWQXO</sourceid><recordid>eNqNkE1OwzAQhQMCifBzh5FYR3UcE7KtCohuKiQisUC0cp0JceXYwT9CcCvOwMVw2ooVC1Yzmjfzvac5TFLKKM1oxdhRkpKckqykBTlJTp3bEHJVlaRKD9IbdNgP-P1loEGQ2qH1xo390wwsirCWu4kwGjTXpg_KS8EHvl16ruViUsupWrwsXViDXgJqQAU9Cq7lJ29GrgIu0JooNSEyZRxO549zYAUjkwe0rbE91wLBtNE228cYPbnHBt6l73be6K0Uf5hmsI2l-AdaiDTwHYII3kv9CoM1Ap0b28jvuG1QR-pvAnAeUZ0nxy1XDi_29Sy5vLutZ_dZPH8L6PxqY4LVUVrlZR5_e51TWvxv6wdiboCY</recordid><startdate>20110301</startdate><enddate>20110301</enddate><creator>Moreno, Luis Henry</creator><creator>Caicedo, Julio Cesar</creator><creator>Gaitan, Gilberto Bejarano</creator><creator>Martínez, Federico</creator><creator>Pulido, Pedro Prieto</creator><general>Universidad de Antioquía</general><scope>7TB</scope><scope>8FD</scope><scope>8FE</scope><scope>8FG</scope><scope>ABJCF</scope><scope>ABUWG</scope><scope>AFKRA</scope><scope>AZQEC</scope><scope>BENPR</scope><scope>BGLVJ</scope><scope>CCPQU</scope><scope>CLZPN</scope><scope>DWQXO</scope><scope>FR3</scope><scope>HCIFZ</scope><scope>KR7</scope><scope>L6V</scope><scope>M7S</scope><scope>PIMPY</scope><scope>PQEST</scope><scope>PQQKQ</scope><scope>PQUKI</scope><scope>PTHSS</scope></search><sort><creationdate>20110301</creationdate><title>Desempeño de insertos de WC recubiertos con nanomulticapas de [TiN/TiAlN]^sub n^ en el mecanizado del acero endurecido AISI 4340/Performance of WC- inserts coated with nanometric [TiN/TiAlN]^sub n^- multilayer for the cutting processing of hardened AISI 4340 steel</title><author>Moreno, Luis Henry ; Caicedo, Julio Cesar ; Gaitan, Gilberto Bejarano ; Martínez, Federico ; Pulido, Pedro Prieto</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-proquest_journals_16124271223</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>spa</language><creationdate>2011</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Moreno, Luis Henry</creatorcontrib><creatorcontrib>Caicedo, Julio Cesar</creatorcontrib><creatorcontrib>Gaitan, Gilberto Bejarano</creatorcontrib><creatorcontrib>Martínez, Federico</creatorcontrib><creatorcontrib>Pulido, Pedro Prieto</creatorcontrib><collection>Mechanical & Transportation Engineering Abstracts</collection><collection>Technology Research Database</collection><collection>ProQuest SciTech Collection</collection><collection>ProQuest Technology Collection</collection><collection>Materials Science & Engineering Collection</collection><collection>ProQuest Central (Alumni Edition)</collection><collection>ProQuest Central UK/Ireland</collection><collection>ProQuest Central Essentials</collection><collection>ProQuest Central</collection><collection>Technology Collection</collection><collection>ProQuest One Community College</collection><collection>Latin America & Iberia Database</collection><collection>ProQuest Central Korea</collection><collection>Engineering Research Database</collection><collection>SciTech Premium Collection</collection><collection>Civil Engineering Abstracts</collection><collection>ProQuest Engineering Collection</collection><collection>Engineering Database</collection><collection>Access via ProQuest (Open Access)</collection><collection>ProQuest One Academic Eastern Edition (DO NOT USE)</collection><collection>ProQuest One Academic</collection><collection>ProQuest One Academic UKI Edition</collection><collection>Engineering Collection</collection><jtitle>Revista Facultad de Ingeniería</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Moreno, Luis Henry</au><au>Caicedo, Julio Cesar</au><au>Gaitan, Gilberto Bejarano</au><au>Martínez, Federico</au><au>Pulido, Pedro Prieto</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Desempeño de insertos de WC recubiertos con nanomulticapas de [TiN/TiAlN]^sub n^ en el mecanizado del acero endurecido AISI 4340/Performance of WC- inserts coated with nanometric [TiN/TiAlN]^sub n^- multilayer for the cutting processing of hardened AISI 4340 steel</atitle><jtitle>Revista Facultad de Ingeniería</jtitle><date>2011-03-01</date><risdate>2011</risdate><issue>58</issue><spage>85</spage><pages>85-</pages><issn>0120-6230</issn><eissn>2422-2844</eissn><abstract>In this paper, wear resistance of 4 μm uncoated tungsten carbide inserts (WC) and coated with (TiN/TiAlN)n multinanolayered or with commercial TiCN-Al2O3-TiN monolayers (TINAL) are examined. Life tests, cutting area temperature analysis, surface roughness measurements on work pieces, roughness measurements on the attacked surface, contact track analysis between chip-insert and chemical composition analysis were carried out. Mechanical tests were conducted on AISI 4340 steel parts using cutting regime and applying high speed cutting. The machining results showed that for a distance of 8,000 m the inserts coated with 300 bilayers exhibited wear values of 0.117 mm, inserts coated with 200 bilayers showed values of 0.138 mm and those coated with TINAL presented wear values of 0.174 mm. Moreover, the temperature values for cutting speed at 176.6 m/mim for 300 bilayers was 522.6°C, for 200 bilayers was 721.4 °C and 1,327.6°C for inserts coated with TINAL. Lower temperatures, caused by a lower friction coefficient and cutting force, contribute to life-time increasing at WC inserts.</abstract><cop>Medellín</cop><pub>Universidad de Antioquía</pub><oa>free_for_read</oa></addata></record> |
fulltext | fulltext |
identifier | ISSN: 0120-6230 |
ispartof | Revista Facultad de Ingeniería, 2011-03 (58), p.85 |
issn | 0120-6230 2422-2844 |
language | spa |
recordid | cdi_proquest_journals_1612427122 |
source | Elektronische Zeitschriftenbibliothek - Frei zugängliche E-Journals |
title | Desempeño de insertos de WC recubiertos con nanomulticapas de [TiN/TiAlN]^sub n^ en el mecanizado del acero endurecido AISI 4340/Performance of WC- inserts coated with nanometric [TiN/TiAlN]^sub n^- multilayer for the cutting processing of hardened AISI 4340 steel |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-04T11%3A26%3A30IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Desempe%C3%B1o%20de%20insertos%20de%20WC%20recubiertos%20con%20nanomulticapas%20de%20%5BTiN/TiAlN%5D%5Esub%20n%5E%20en%20el%20mecanizado%20del%20acero%20endurecido%20AISI%204340/Performance%20of%20WC-%20inserts%20coated%20with%20nanometric%20%5BTiN/TiAlN%5D%5Esub%20n%5E-%20multilayer%20for%20the%20cutting%20processing%20of%20hardened%20AISI%204340%20steel&rft.jtitle=Revista%20Facultad%20de%20Ingenier%C3%ADa&rft.au=Moreno,%20Luis%20Henry&rft.date=2011-03-01&rft.issue=58&rft.spage=85&rft.pages=85-&rft.issn=0120-6230&rft.eissn=2422-2844&rft_id=info:doi/&rft_dat=%3Cproquest%3E3462537421%3C/proquest%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=1612427122&rft_id=info:pmid/&rfr_iscdi=true |