Preparation of Pt@SnO2 Core-Shell Nanoparticles for Photocatalytic Degradation of Formaldehyde

We report the synthesis and characterization of platinum‐tin oxide core‐shell nanoparticles (Pt@SnO2) for use as a photocatalyst for formaldehyde (HCHO) degradation. We used a sol‐gel process followed by calcination to prepare the Pt@SnO2 photocatalyst. Transmission Electron Microscopy (TEM) reveale...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of the Chinese Chemical Society (Taipei) 2014-03, Vol.61 (3), p.345-349
Hauptverfasser: Chang, Ya-Chin, Yan, Cheng-Yu, Wu, Ren-Jang
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 349
container_issue 3
container_start_page 345
container_title Journal of the Chinese Chemical Society (Taipei)
container_volume 61
creator Chang, Ya-Chin
Yan, Cheng-Yu
Wu, Ren-Jang
description We report the synthesis and characterization of platinum‐tin oxide core‐shell nanoparticles (Pt@SnO2) for use as a photocatalyst for formaldehyde (HCHO) degradation. We used a sol‐gel process followed by calcination to prepare the Pt@SnO2 photocatalyst. Transmission Electron Microscopy (TEM) revealed that the average Pt core diameter was 7‐10 nm in diameter, and the SnO2 shell was approximately 2 nm thick. UV‐Visible spectroscopy displayed the peak from the Pt@SnO2 core‐shell structures is red‐shifted by 16 nm from that of the Pt nanoparticles. We determined photocatalytic activity by irradiating formaldehyde gas in the presence of nanoparticle samples with an 18 W daylight lamp for 180 min. The irradiated Pt@SnO2 nanoparticles achieved 93.2% formaldehyde degradation, while TiO2 (P25), SnO2, and 1 wt.% Pt/SnO2 achieved 70.1%, 67.5%, and 66.0% respectively. Thus, Pt@SnO2 was the most effective material for the degradation of formaldehyde, demonstrating its potential for use as a high efficiency photocatalyst for the degradation of formaldehyde. We prepared a novel nanocomposite Pt@SnO2 materials as a photocatalyst, the average Pt core diameter was 7‐10 nm in diameter, and the SnO2 shell was approximately 2 nm thick. Pt@SnO2 exhibited the greatest formaldehyde degradation efficiency of 93.2% during 18 W daylight illumination at room temperature.
doi_str_mv 10.1002/jccs.201300272
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_journals_1564763755</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>3442460671</sourcerecordid><originalsourceid>FETCH-LOGICAL-c3472-e32e4ef26b59a4028e2fba2706a0bd715e285fc433bbef10415ec69e152e5f133</originalsourceid><addsrcrecordid>eNqFkM1PwkAQxTdGExG9em7iubjfpTe1CmgQiWgkHtxs21kpFhZ3S5T_3pIa4s3TZF7e783kIXRKcIdgTM_nWeY7FBNWLxHdQy1KYhpKweN91MIYxyEXTB6iI-_nGHNGRdxCb2MHK-10VdhlYE0wri4mywcaJNZBOJlBWQYjvbS1pSqyEnxgrAvGM1vZTFe63NRqcA3vTue7iJ51C13mMNvkcIwOjC49nPzONnru3Twlg3D40L9NLodhxnhEQ2AUOBgqUxFrjmkXqEk1jbDUOM0jIoB2hck4Y2kKhmBeK5mMgQgKwhDG2uisyV05-7kGX6m5XbtlfVIRIXkkWSRE7eo0rsxZ7x0YtXLFQruNIlhtO1TbDtWuwxqIG-CrKGHzj1vdJcnkLxs2bOEr-N6x2n0oGdXvqJdRX73KwVV8_zhVU_YDQ0-FJA</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1564763755</pqid></control><display><type>article</type><title>Preparation of Pt@SnO2 Core-Shell Nanoparticles for Photocatalytic Degradation of Formaldehyde</title><source>Wiley Journals</source><creator>Chang, Ya-Chin ; Yan, Cheng-Yu ; Wu, Ren-Jang</creator><creatorcontrib>Chang, Ya-Chin ; Yan, Cheng-Yu ; Wu, Ren-Jang</creatorcontrib><description>We report the synthesis and characterization of platinum‐tin oxide core‐shell nanoparticles (Pt@SnO2) for use as a photocatalyst for formaldehyde (HCHO) degradation. We used a sol‐gel process followed by calcination to prepare the Pt@SnO2 photocatalyst. Transmission Electron Microscopy (TEM) revealed that the average Pt core diameter was 7‐10 nm in diameter, and the SnO2 shell was approximately 2 nm thick. UV‐Visible spectroscopy displayed the peak from the Pt@SnO2 core‐shell structures is red‐shifted by 16 nm from that of the Pt nanoparticles. We determined photocatalytic activity by irradiating formaldehyde gas in the presence of nanoparticle samples with an 18 W daylight lamp for 180 min. The irradiated Pt@SnO2 nanoparticles achieved 93.2% formaldehyde degradation, while TiO2 (P25), SnO2, and 1 wt.% Pt/SnO2 achieved 70.1%, 67.5%, and 66.0% respectively. Thus, Pt@SnO2 was the most effective material for the degradation of formaldehyde, demonstrating its potential for use as a high efficiency photocatalyst for the degradation of formaldehyde. We prepared a novel nanocomposite Pt@SnO2 materials as a photocatalyst, the average Pt core diameter was 7‐10 nm in diameter, and the SnO2 shell was approximately 2 nm thick. Pt@SnO2 exhibited the greatest formaldehyde degradation efficiency of 93.2% during 18 W daylight illumination at room temperature.</description><identifier>ISSN: 0009-4536</identifier><identifier>EISSN: 2192-6549</identifier><identifier>DOI: 10.1002/jccs.201300272</identifier><language>eng</language><publisher>Weinheim: WILEY-VCH Verlag</publisher><subject>Chemical synthesis ; HCHO degradation ; Nanoparticles ; Photocatalysis ; Photocatalyst ; Pt@SnO2</subject><ispartof>Journal of the Chinese Chemical Society (Taipei), 2014-03, Vol.61 (3), p.345-349</ispartof><rights>Copyright © 2014 The Chemical Society Located in Taipei &amp; Wiley‐VCH Verlag GmbH &amp; Co. KGaA, Weinheim, Germany</rights><rights>Copyright © 2014 The Chemical Society Located in Taipei &amp; Wiley-VCH Verlag GmbH &amp; Co. KGaA, Weinheim, Germany</rights><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c3472-e32e4ef26b59a4028e2fba2706a0bd715e285fc433bbef10415ec69e152e5f133</citedby><cites>FETCH-LOGICAL-c3472-e32e4ef26b59a4028e2fba2706a0bd715e285fc433bbef10415ec69e152e5f133</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktopdf>$$Uhttps://onlinelibrary.wiley.com/doi/pdf/10.1002%2Fjccs.201300272$$EPDF$$P50$$Gwiley$$H</linktopdf><linktohtml>$$Uhttps://onlinelibrary.wiley.com/doi/full/10.1002%2Fjccs.201300272$$EHTML$$P50$$Gwiley$$H</linktohtml><link.rule.ids>314,780,784,1417,27924,27925,45574,45575</link.rule.ids></links><search><creatorcontrib>Chang, Ya-Chin</creatorcontrib><creatorcontrib>Yan, Cheng-Yu</creatorcontrib><creatorcontrib>Wu, Ren-Jang</creatorcontrib><title>Preparation of Pt@SnO2 Core-Shell Nanoparticles for Photocatalytic Degradation of Formaldehyde</title><title>Journal of the Chinese Chemical Society (Taipei)</title><addtitle>Jnl Chinese Chemical Soc</addtitle><description>We report the synthesis and characterization of platinum‐tin oxide core‐shell nanoparticles (Pt@SnO2) for use as a photocatalyst for formaldehyde (HCHO) degradation. We used a sol‐gel process followed by calcination to prepare the Pt@SnO2 photocatalyst. Transmission Electron Microscopy (TEM) revealed that the average Pt core diameter was 7‐10 nm in diameter, and the SnO2 shell was approximately 2 nm thick. UV‐Visible spectroscopy displayed the peak from the Pt@SnO2 core‐shell structures is red‐shifted by 16 nm from that of the Pt nanoparticles. We determined photocatalytic activity by irradiating formaldehyde gas in the presence of nanoparticle samples with an 18 W daylight lamp for 180 min. The irradiated Pt@SnO2 nanoparticles achieved 93.2% formaldehyde degradation, while TiO2 (P25), SnO2, and 1 wt.% Pt/SnO2 achieved 70.1%, 67.5%, and 66.0% respectively. Thus, Pt@SnO2 was the most effective material for the degradation of formaldehyde, demonstrating its potential for use as a high efficiency photocatalyst for the degradation of formaldehyde. We prepared a novel nanocomposite Pt@SnO2 materials as a photocatalyst, the average Pt core diameter was 7‐10 nm in diameter, and the SnO2 shell was approximately 2 nm thick. Pt@SnO2 exhibited the greatest formaldehyde degradation efficiency of 93.2% during 18 W daylight illumination at room temperature.</description><subject>Chemical synthesis</subject><subject>HCHO degradation</subject><subject>Nanoparticles</subject><subject>Photocatalysis</subject><subject>Photocatalyst</subject><subject>Pt@SnO2</subject><issn>0009-4536</issn><issn>2192-6549</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2014</creationdate><recordtype>article</recordtype><recordid>eNqFkM1PwkAQxTdGExG9em7iubjfpTe1CmgQiWgkHtxs21kpFhZ3S5T_3pIa4s3TZF7e783kIXRKcIdgTM_nWeY7FBNWLxHdQy1KYhpKweN91MIYxyEXTB6iI-_nGHNGRdxCb2MHK-10VdhlYE0wri4mywcaJNZBOJlBWQYjvbS1pSqyEnxgrAvGM1vZTFe63NRqcA3vTue7iJ51C13mMNvkcIwOjC49nPzONnru3Twlg3D40L9NLodhxnhEQ2AUOBgqUxFrjmkXqEk1jbDUOM0jIoB2hck4Y2kKhmBeK5mMgQgKwhDG2uisyV05-7kGX6m5XbtlfVIRIXkkWSRE7eo0rsxZ7x0YtXLFQruNIlhtO1TbDtWuwxqIG-CrKGHzj1vdJcnkLxs2bOEr-N6x2n0oGdXvqJdRX73KwVV8_zhVU_YDQ0-FJA</recordid><startdate>201403</startdate><enddate>201403</enddate><creator>Chang, Ya-Chin</creator><creator>Yan, Cheng-Yu</creator><creator>Wu, Ren-Jang</creator><general>WILEY-VCH Verlag</general><general>WILEY‐VCH Verlag</general><general>Wiley Subscription Services, Inc</general><scope>BSCLL</scope><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>201403</creationdate><title>Preparation of Pt@SnO2 Core-Shell Nanoparticles for Photocatalytic Degradation of Formaldehyde</title><author>Chang, Ya-Chin ; Yan, Cheng-Yu ; Wu, Ren-Jang</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c3472-e32e4ef26b59a4028e2fba2706a0bd715e285fc433bbef10415ec69e152e5f133</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2014</creationdate><topic>Chemical synthesis</topic><topic>HCHO degradation</topic><topic>Nanoparticles</topic><topic>Photocatalysis</topic><topic>Photocatalyst</topic><topic>Pt@SnO2</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Chang, Ya-Chin</creatorcontrib><creatorcontrib>Yan, Cheng-Yu</creatorcontrib><creatorcontrib>Wu, Ren-Jang</creatorcontrib><collection>Istex</collection><collection>CrossRef</collection><jtitle>Journal of the Chinese Chemical Society (Taipei)</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Chang, Ya-Chin</au><au>Yan, Cheng-Yu</au><au>Wu, Ren-Jang</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Preparation of Pt@SnO2 Core-Shell Nanoparticles for Photocatalytic Degradation of Formaldehyde</atitle><jtitle>Journal of the Chinese Chemical Society (Taipei)</jtitle><addtitle>Jnl Chinese Chemical Soc</addtitle><date>2014-03</date><risdate>2014</risdate><volume>61</volume><issue>3</issue><spage>345</spage><epage>349</epage><pages>345-349</pages><issn>0009-4536</issn><eissn>2192-6549</eissn><abstract>We report the synthesis and characterization of platinum‐tin oxide core‐shell nanoparticles (Pt@SnO2) for use as a photocatalyst for formaldehyde (HCHO) degradation. We used a sol‐gel process followed by calcination to prepare the Pt@SnO2 photocatalyst. Transmission Electron Microscopy (TEM) revealed that the average Pt core diameter was 7‐10 nm in diameter, and the SnO2 shell was approximately 2 nm thick. UV‐Visible spectroscopy displayed the peak from the Pt@SnO2 core‐shell structures is red‐shifted by 16 nm from that of the Pt nanoparticles. We determined photocatalytic activity by irradiating formaldehyde gas in the presence of nanoparticle samples with an 18 W daylight lamp for 180 min. The irradiated Pt@SnO2 nanoparticles achieved 93.2% formaldehyde degradation, while TiO2 (P25), SnO2, and 1 wt.% Pt/SnO2 achieved 70.1%, 67.5%, and 66.0% respectively. Thus, Pt@SnO2 was the most effective material for the degradation of formaldehyde, demonstrating its potential for use as a high efficiency photocatalyst for the degradation of formaldehyde. We prepared a novel nanocomposite Pt@SnO2 materials as a photocatalyst, the average Pt core diameter was 7‐10 nm in diameter, and the SnO2 shell was approximately 2 nm thick. Pt@SnO2 exhibited the greatest formaldehyde degradation efficiency of 93.2% during 18 W daylight illumination at room temperature.</abstract><cop>Weinheim</cop><pub>WILEY-VCH Verlag</pub><doi>10.1002/jccs.201300272</doi><tpages>5</tpages><oa>free_for_read</oa></addata></record>
fulltext fulltext
identifier ISSN: 0009-4536
ispartof Journal of the Chinese Chemical Society (Taipei), 2014-03, Vol.61 (3), p.345-349
issn 0009-4536
2192-6549
language eng
recordid cdi_proquest_journals_1564763755
source Wiley Journals
subjects Chemical synthesis
HCHO degradation
Nanoparticles
Photocatalysis
Photocatalyst
Pt@SnO2
title Preparation of Pt@SnO2 Core-Shell Nanoparticles for Photocatalytic Degradation of Formaldehyde
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-04T12%3A53%3A30IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Preparation%20of%20Pt@SnO2%20Core-Shell%20Nanoparticles%20for%20Photocatalytic%20Degradation%20of%20Formaldehyde&rft.jtitle=Journal%20of%20the%20Chinese%20Chemical%20Society%20(Taipei)&rft.au=Chang,%20Ya-Chin&rft.date=2014-03&rft.volume=61&rft.issue=3&rft.spage=345&rft.epage=349&rft.pages=345-349&rft.issn=0009-4536&rft.eissn=2192-6549&rft_id=info:doi/10.1002/jccs.201300272&rft_dat=%3Cproquest_cross%3E3442460671%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=1564763755&rft_id=info:pmid/&rfr_iscdi=true