Response of Fiber Diameter with the Continuously Changing of Draw Ratio

The fiber with gradually changing diameter was fabricated by changing the draw ratio continuously, that is, by changing the take-up speed of melt spinning, laser drawing, and heater drawing processes. The diameter profiles of resultant fibers were monitored and compared each other. As the results, t...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Senʾi Gakkaishi 2014-08, Vol.70 (8), p.167-173
Hauptverfasser: Matoba, Munekazu, Ito, Akiyoshi, Ikaga, Toshifumi, Ohkoshi, Yutaka
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 173
container_issue 8
container_start_page 167
container_title Senʾi Gakkaishi
container_volume 70
creator Matoba, Munekazu
Ito, Akiyoshi
Ikaga, Toshifumi
Ohkoshi, Yutaka
description The fiber with gradually changing diameter was fabricated by changing the draw ratio continuously, that is, by changing the take-up speed of melt spinning, laser drawing, and heater drawing processes. The diameter profiles of resultant fibers were monitored and compared each other. As the results, the laser drawing shows the best diameter responsiveness among the three. For the case, the diameter changing rate increased with the increase of fiber acceleration rate up to 6.0 m/s2. Moreover, it can make the fiber whose diameter gradually changed about 40% within 8 cm range for the minimum case. The diameter profile was determinded by not only the draw ratio profile but also the start/end draw ratios. The lower drawing stress change tends to improve the responsiveness, and the minimum response length for laser drawing was obtained for the draw ratio decreasing case.
doi_str_mv 10.2115/fiber.70.167
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_journals_1560322101</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>3423960991</sourcerecordid><originalsourceid>FETCH-LOGICAL-c1467-1c4511be0af0c17095f8e117599f474e77f6f4cfddcb250e36fccab628a8d0893</originalsourceid><addsrcrecordid>eNotkF1LwzAUhoMoOKd3_oCAt3aekzZNeimdm8JAGHod0izZMrZmJi1j_97OeXXeA-8HPIQ8IkwYIn9xvrFxImCCpbgiI5SyyBjj1TUZAeQiq6Tgt-Qupe3w5lzwEZkvbTqENlkaHJ2d83Tq9d52gzj6bkO7jaV1aDvf9qFPuxOtN7pd-3Z9DkyjPtKl7ny4JzdO75J9-L9j8j17-6rfs8Xn_KN-XWQGi1JkaAqO2FjQDgwKqLiTFlHwqnKFKKwQrnSFcauVaRgHm5fOGN2UTGq5AlnlY_J06T3E8NPb1Klt6GM7TCrkJeSMIeDger64TAwpRevUIfq9jieFoM6o1B8qJUANqPJfp9xcRA</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1560322101</pqid></control><display><type>article</type><title>Response of Fiber Diameter with the Continuously Changing of Draw Ratio</title><source>EZB-FREE-00999 freely available EZB journals</source><creator>Matoba, Munekazu ; Ito, Akiyoshi ; Ikaga, Toshifumi ; Ohkoshi, Yutaka</creator><creatorcontrib>Matoba, Munekazu ; Ito, Akiyoshi ; Ikaga, Toshifumi ; Ohkoshi, Yutaka</creatorcontrib><description>The fiber with gradually changing diameter was fabricated by changing the draw ratio continuously, that is, by changing the take-up speed of melt spinning, laser drawing, and heater drawing processes. The diameter profiles of resultant fibers were monitored and compared each other. As the results, the laser drawing shows the best diameter responsiveness among the three. For the case, the diameter changing rate increased with the increase of fiber acceleration rate up to 6.0 m/s2. Moreover, it can make the fiber whose diameter gradually changed about 40% within 8 cm range for the minimum case. The diameter profile was determinded by not only the draw ratio profile but also the start/end draw ratios. The lower drawing stress change tends to improve the responsiveness, and the minimum response length for laser drawing was obtained for the draw ratio decreasing case.</description><identifier>ISSN: 0037-9875</identifier><identifier>EISSN: 1884-2259</identifier><identifier>DOI: 10.2115/fiber.70.167</identifier><language>eng</language><publisher>Tokyo: Japan Science and Technology Agency</publisher><ispartof>Senʾi Gakkaishi, 2014-08, Vol.70 (8), p.167-173</ispartof><rights>Copyright Japan Science and Technology Agency 2014</rights><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c1467-1c4511be0af0c17095f8e117599f474e77f6f4cfddcb250e36fccab628a8d0893</citedby></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,776,780,27901,27902</link.rule.ids></links><search><creatorcontrib>Matoba, Munekazu</creatorcontrib><creatorcontrib>Ito, Akiyoshi</creatorcontrib><creatorcontrib>Ikaga, Toshifumi</creatorcontrib><creatorcontrib>Ohkoshi, Yutaka</creatorcontrib><title>Response of Fiber Diameter with the Continuously Changing of Draw Ratio</title><title>Senʾi Gakkaishi</title><description>The fiber with gradually changing diameter was fabricated by changing the draw ratio continuously, that is, by changing the take-up speed of melt spinning, laser drawing, and heater drawing processes. The diameter profiles of resultant fibers were monitored and compared each other. As the results, the laser drawing shows the best diameter responsiveness among the three. For the case, the diameter changing rate increased with the increase of fiber acceleration rate up to 6.0 m/s2. Moreover, it can make the fiber whose diameter gradually changed about 40% within 8 cm range for the minimum case. The diameter profile was determinded by not only the draw ratio profile but also the start/end draw ratios. The lower drawing stress change tends to improve the responsiveness, and the minimum response length for laser drawing was obtained for the draw ratio decreasing case.</description><issn>0037-9875</issn><issn>1884-2259</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2014</creationdate><recordtype>article</recordtype><recordid>eNotkF1LwzAUhoMoOKd3_oCAt3aekzZNeimdm8JAGHod0izZMrZmJi1j_97OeXXeA-8HPIQ8IkwYIn9xvrFxImCCpbgiI5SyyBjj1TUZAeQiq6Tgt-Qupe3w5lzwEZkvbTqENlkaHJ2d83Tq9d52gzj6bkO7jaV1aDvf9qFPuxOtN7pd-3Z9DkyjPtKl7ny4JzdO75J9-L9j8j17-6rfs8Xn_KN-XWQGi1JkaAqO2FjQDgwKqLiTFlHwqnKFKKwQrnSFcauVaRgHm5fOGN2UTGq5AlnlY_J06T3E8NPb1Klt6GM7TCrkJeSMIeDger64TAwpRevUIfq9jieFoM6o1B8qJUANqPJfp9xcRA</recordid><startdate>20140801</startdate><enddate>20140801</enddate><creator>Matoba, Munekazu</creator><creator>Ito, Akiyoshi</creator><creator>Ikaga, Toshifumi</creator><creator>Ohkoshi, Yutaka</creator><general>Japan Science and Technology Agency</general><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>20140801</creationdate><title>Response of Fiber Diameter with the Continuously Changing of Draw Ratio</title><author>Matoba, Munekazu ; Ito, Akiyoshi ; Ikaga, Toshifumi ; Ohkoshi, Yutaka</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c1467-1c4511be0af0c17095f8e117599f474e77f6f4cfddcb250e36fccab628a8d0893</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2014</creationdate><toplevel>online_resources</toplevel><creatorcontrib>Matoba, Munekazu</creatorcontrib><creatorcontrib>Ito, Akiyoshi</creatorcontrib><creatorcontrib>Ikaga, Toshifumi</creatorcontrib><creatorcontrib>Ohkoshi, Yutaka</creatorcontrib><collection>CrossRef</collection><jtitle>Senʾi Gakkaishi</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Matoba, Munekazu</au><au>Ito, Akiyoshi</au><au>Ikaga, Toshifumi</au><au>Ohkoshi, Yutaka</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Response of Fiber Diameter with the Continuously Changing of Draw Ratio</atitle><jtitle>Senʾi Gakkaishi</jtitle><date>2014-08-01</date><risdate>2014</risdate><volume>70</volume><issue>8</issue><spage>167</spage><epage>173</epage><pages>167-173</pages><issn>0037-9875</issn><eissn>1884-2259</eissn><abstract>The fiber with gradually changing diameter was fabricated by changing the draw ratio continuously, that is, by changing the take-up speed of melt spinning, laser drawing, and heater drawing processes. The diameter profiles of resultant fibers were monitored and compared each other. As the results, the laser drawing shows the best diameter responsiveness among the three. For the case, the diameter changing rate increased with the increase of fiber acceleration rate up to 6.0 m/s2. Moreover, it can make the fiber whose diameter gradually changed about 40% within 8 cm range for the minimum case. The diameter profile was determinded by not only the draw ratio profile but also the start/end draw ratios. The lower drawing stress change tends to improve the responsiveness, and the minimum response length for laser drawing was obtained for the draw ratio decreasing case.</abstract><cop>Tokyo</cop><pub>Japan Science and Technology Agency</pub><doi>10.2115/fiber.70.167</doi><tpages>7</tpages><oa>free_for_read</oa></addata></record>
fulltext fulltext
identifier ISSN: 0037-9875
ispartof Senʾi Gakkaishi, 2014-08, Vol.70 (8), p.167-173
issn 0037-9875
1884-2259
language eng
recordid cdi_proquest_journals_1560322101
source EZB-FREE-00999 freely available EZB journals
title Response of Fiber Diameter with the Continuously Changing of Draw Ratio
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-08T17%3A57%3A47IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Response%20of%20Fiber%20Diameter%20with%20the%20Continuously%20Changing%20of%20Draw%20Ratio&rft.jtitle=Sen%CA%BEi%20Gakkaishi&rft.au=Matoba,%20Munekazu&rft.date=2014-08-01&rft.volume=70&rft.issue=8&rft.spage=167&rft.epage=173&rft.pages=167-173&rft.issn=0037-9875&rft.eissn=1884-2259&rft_id=info:doi/10.2115/fiber.70.167&rft_dat=%3Cproquest_cross%3E3423960991%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=1560322101&rft_id=info:pmid/&rfr_iscdi=true