Effects of Plating Baths for Cu-undercoat on Thermal Peeling of Tin Plated Phosphor-bronze

To clarify the mechanism of thermally accelerated adhesion-loss of plated films of tin on phosphor-bronze and to find methods for providing protection from this phenomenon, the effects of the plating conditions of copper undercoat were examined with plating baths of copper cyanide, copper pyrophosph...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Hyōmen gijutsu 1992/01/01, Vol.43(1), pp.55-60
1. Verfasser: FUKAMACHI, Kazuhiko
Format: Artikel
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 60
container_issue 1
container_start_page 55
container_title Hyōmen gijutsu
container_volume 43
creator FUKAMACHI, Kazuhiko
description To clarify the mechanism of thermally accelerated adhesion-loss of plated films of tin on phosphor-bronze and to find methods for providing protection from this phenomenon, the effects of the plating conditions of copper undercoat were examined with plating baths of copper cyanide, copper pyrophosphate, copper sulfate and copper fluoborate. Main findings are summarized as follows. 1. Tin-coated phosphor-bronze is very insensitive to thermal peeling when copper undercoat is electroplated from copper cyanide baths, and very sensitive when the undercoat is electroplated from copper pyrophosphate baths. 2. In electroplated tin-copper systems, no effect of copper electroplating bath on diffusivity was observed. It is suggested that the susceptibility of thermal peeling of tin-coated phosphor-bronze to plating conditions of copper undercoat is due not to any acceleration of diffusion by the undercoat but to the interaction of vacancies induced in the undercoat by diffusion with the matrix.
doi_str_mv 10.4139/sfj.43.55
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_journals_1491091395</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>3180639001</sourcerecordid><originalsourceid>FETCH-LOGICAL-c2425-a745d7ab7a86091fb9d84dc02480705a43ced9408e04623dc8bc1c858208869d3</originalsourceid><addsrcrecordid>eNo9kD1PwzAQhi0EEqUw8A8swcKQYsd2Yo9QlQ-pEh3KwmI5jt0kSuNiJwP8ehxSdTkP97zPnQ-AW4wWFBPxGGyzoGTB2BmYYc5pQigS52CGBGYJ5pm4BFchNAgRwrJ8Br5W1hrdB-gs3LSqr7sdfFZ9FaB1Hi6HZOhK47VTPXQd3FbG71ULN8a0IxlD27r7D5oSbioXDpXzSeFd92uuwYVVbTA3x3cOPl9W2-Vbsv54fV8-rROd0pQlKqeszFWRK57FLW0hSk5LjVLKUY6YokSbUlDEDaJZSkrNC401ZzxFPP6nJHNwN3kP3n0PJvSycYPv4kiJqcDRSQSL1MNEae9C8MbKg6_3yv9IjOR4OhlPJymRbGTvj0YVtGqtV52uwynAGM4ylEbsecKa0KudOfWV72vdmlGIBRejFE-FsVNTV8pL05E_zieEOg</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1491091395</pqid></control><display><type>article</type><title>Effects of Plating Baths for Cu-undercoat on Thermal Peeling of Tin Plated Phosphor-bronze</title><source>J-STAGE Free</source><source>Elektronische Zeitschriftenbibliothek - Frei zugängliche E-Journals</source><creator>FUKAMACHI, Kazuhiko</creator><creatorcontrib>FUKAMACHI, Kazuhiko</creatorcontrib><description>To clarify the mechanism of thermally accelerated adhesion-loss of plated films of tin on phosphor-bronze and to find methods for providing protection from this phenomenon, the effects of the plating conditions of copper undercoat were examined with plating baths of copper cyanide, copper pyrophosphate, copper sulfate and copper fluoborate. Main findings are summarized as follows. 1. Tin-coated phosphor-bronze is very insensitive to thermal peeling when copper undercoat is electroplated from copper cyanide baths, and very sensitive when the undercoat is electroplated from copper pyrophosphate baths. 2. In electroplated tin-copper systems, no effect of copper electroplating bath on diffusivity was observed. It is suggested that the susceptibility of thermal peeling of tin-coated phosphor-bronze to plating conditions of copper undercoat is due not to any acceleration of diffusion by the undercoat but to the interaction of vacancies induced in the undercoat by diffusion with the matrix.</description><identifier>ISSN: 0915-1869</identifier><identifier>EISSN: 1884-3409</identifier><identifier>DOI: 10.4139/sfj.43.55</identifier><language>eng ; jpn</language><publisher>Tokyo: The Surface Finishing Society of Japan</publisher><subject>Copper Undercoat ; Phosphor-bronze ; Thermal Peeling ; Tin Plating</subject><ispartof>Journal of The Surface Finishing Society of Japan, 1992/01/01, Vol.43(1), pp.55-60</ispartof><rights>The Surface Finishing Society of Japan</rights><rights>1992 INIST-CNRS</rights><rights>Copyright Japan Science and Technology Agency 1992</rights><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,776,780,4010,27900,27901,27902</link.rule.ids><backlink>$$Uhttp://pascal-francis.inist.fr/vibad/index.php?action=getRecordDetail&amp;idt=5516602$$DView record in Pascal Francis$$Hfree_for_read</backlink></links><search><creatorcontrib>FUKAMACHI, Kazuhiko</creatorcontrib><title>Effects of Plating Baths for Cu-undercoat on Thermal Peeling of Tin Plated Phosphor-bronze</title><title>Hyōmen gijutsu</title><addtitle>Journal of The Surface Finishing Society of Japan</addtitle><description>To clarify the mechanism of thermally accelerated adhesion-loss of plated films of tin on phosphor-bronze and to find methods for providing protection from this phenomenon, the effects of the plating conditions of copper undercoat were examined with plating baths of copper cyanide, copper pyrophosphate, copper sulfate and copper fluoborate. Main findings are summarized as follows. 1. Tin-coated phosphor-bronze is very insensitive to thermal peeling when copper undercoat is electroplated from copper cyanide baths, and very sensitive when the undercoat is electroplated from copper pyrophosphate baths. 2. In electroplated tin-copper systems, no effect of copper electroplating bath on diffusivity was observed. It is suggested that the susceptibility of thermal peeling of tin-coated phosphor-bronze to plating conditions of copper undercoat is due not to any acceleration of diffusion by the undercoat but to the interaction of vacancies induced in the undercoat by diffusion with the matrix.</description><subject>Copper Undercoat</subject><subject>Phosphor-bronze</subject><subject>Thermal Peeling</subject><subject>Tin Plating</subject><issn>0915-1869</issn><issn>1884-3409</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>1992</creationdate><recordtype>article</recordtype><recordid>eNo9kD1PwzAQhi0EEqUw8A8swcKQYsd2Yo9QlQ-pEh3KwmI5jt0kSuNiJwP8ehxSdTkP97zPnQ-AW4wWFBPxGGyzoGTB2BmYYc5pQigS52CGBGYJ5pm4BFchNAgRwrJ8Br5W1hrdB-gs3LSqr7sdfFZ9FaB1Hi6HZOhK47VTPXQd3FbG71ULN8a0IxlD27r7D5oSbioXDpXzSeFd92uuwYVVbTA3x3cOPl9W2-Vbsv54fV8-rROd0pQlKqeszFWRK57FLW0hSk5LjVLKUY6YokSbUlDEDaJZSkrNC401ZzxFPP6nJHNwN3kP3n0PJvSycYPv4kiJqcDRSQSL1MNEae9C8MbKg6_3yv9IjOR4OhlPJymRbGTvj0YVtGqtV52uwynAGM4ylEbsecKa0KudOfWV72vdmlGIBRejFE-FsVNTV8pL05E_zieEOg</recordid><startdate>19920101</startdate><enddate>19920101</enddate><creator>FUKAMACHI, Kazuhiko</creator><general>The Surface Finishing Society of Japan</general><general>Hyomen Gijutsu Kyokai</general><general>Japan Science and Technology Agency</general><scope>IQODW</scope><scope>AAYXX</scope><scope>CITATION</scope><scope>7SR</scope><scope>8BQ</scope><scope>8FD</scope><scope>JG9</scope></search><sort><creationdate>19920101</creationdate><title>Effects of Plating Baths for Cu-undercoat on Thermal Peeling of Tin Plated Phosphor-bronze</title><author>FUKAMACHI, Kazuhiko</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c2425-a745d7ab7a86091fb9d84dc02480705a43ced9408e04623dc8bc1c858208869d3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng ; jpn</language><creationdate>1992</creationdate><topic>Copper Undercoat</topic><topic>Phosphor-bronze</topic><topic>Thermal Peeling</topic><topic>Tin Plating</topic><toplevel>online_resources</toplevel><creatorcontrib>FUKAMACHI, Kazuhiko</creatorcontrib><collection>Pascal-Francis</collection><collection>CrossRef</collection><collection>Engineered Materials Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><jtitle>Hyōmen gijutsu</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>FUKAMACHI, Kazuhiko</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Effects of Plating Baths for Cu-undercoat on Thermal Peeling of Tin Plated Phosphor-bronze</atitle><jtitle>Hyōmen gijutsu</jtitle><addtitle>Journal of The Surface Finishing Society of Japan</addtitle><date>1992-01-01</date><risdate>1992</risdate><volume>43</volume><issue>1</issue><spage>55</spage><epage>60</epage><pages>55-60</pages><issn>0915-1869</issn><eissn>1884-3409</eissn><abstract>To clarify the mechanism of thermally accelerated adhesion-loss of plated films of tin on phosphor-bronze and to find methods for providing protection from this phenomenon, the effects of the plating conditions of copper undercoat were examined with plating baths of copper cyanide, copper pyrophosphate, copper sulfate and copper fluoborate. Main findings are summarized as follows. 1. Tin-coated phosphor-bronze is very insensitive to thermal peeling when copper undercoat is electroplated from copper cyanide baths, and very sensitive when the undercoat is electroplated from copper pyrophosphate baths. 2. In electroplated tin-copper systems, no effect of copper electroplating bath on diffusivity was observed. It is suggested that the susceptibility of thermal peeling of tin-coated phosphor-bronze to plating conditions of copper undercoat is due not to any acceleration of diffusion by the undercoat but to the interaction of vacancies induced in the undercoat by diffusion with the matrix.</abstract><cop>Tokyo</cop><pub>The Surface Finishing Society of Japan</pub><doi>10.4139/sfj.43.55</doi><tpages>6</tpages><oa>free_for_read</oa></addata></record>
fulltext fulltext
identifier ISSN: 0915-1869
ispartof Journal of The Surface Finishing Society of Japan, 1992/01/01, Vol.43(1), pp.55-60
issn 0915-1869
1884-3409
language eng ; jpn
recordid cdi_proquest_journals_1491091395
source J-STAGE Free; Elektronische Zeitschriftenbibliothek - Frei zugängliche E-Journals
subjects Copper Undercoat
Phosphor-bronze
Thermal Peeling
Tin Plating
title Effects of Plating Baths for Cu-undercoat on Thermal Peeling of Tin Plated Phosphor-bronze
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-04T08%3A17%3A10IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Effects%20of%20Plating%20Baths%20for%20Cu-undercoat%20on%20Thermal%20Peeling%20of%20Tin%20Plated%20Phosphor-bronze&rft.jtitle=Hy%C5%8Dmen%20gijutsu&rft.au=FUKAMACHI,%20Kazuhiko&rft.date=1992-01-01&rft.volume=43&rft.issue=1&rft.spage=55&rft.epage=60&rft.pages=55-60&rft.issn=0915-1869&rft.eissn=1884-3409&rft_id=info:doi/10.4139/sfj.43.55&rft_dat=%3Cproquest_cross%3E3180639001%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=1491091395&rft_id=info:pmid/&rfr_iscdi=true