Research on Properties Improvement of Composite Aluminum Alloy Foil Based on Cold-Rolling Cladding
The cold-rolling cladding process of composite aluminum alloy foil for automobile heat exchanger was investigated, as well as the effects of percentage reduction of first pass, clad sheet thickness and final annealing schedule on the microstructure and properties of the foil. The results showed that...
Gespeichert in:
Veröffentlicht in: | Applied Mechanics and Materials 2012-07, Vol.189, p.162-166 |
---|---|
1. Verfasser: | |
Format: | Artikel |
Sprache: | eng |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | 166 |
---|---|
container_issue | |
container_start_page | 162 |
container_title | Applied Mechanics and Materials |
container_volume | 189 |
creator | Tai, Qian |
description | The cold-rolling cladding process of composite aluminum alloy foil for automobile heat exchanger was investigated, as well as the effects of percentage reduction of first pass, clad sheet thickness and final annealing schedule on the microstructure and properties of the foil. The results showed that bonding the clad sheets A4045 to the core material A3003 on both sides succeeds initially when the percentage reduction is 30%~50% of first pass during cold rolling, and the thickness of both the clad sheets of the composite foil are basically the same. The best sagging resistance is available when the percentage reduction of final pass is 25%~35%. The annealing temperature should be controlled in the range from 320 to 400°C before finish rolling, and the annealing time should control within 80 minutes when annealed at 400°C. |
doi_str_mv | 10.4028/www.scientific.net/AMM.189.162 |
format | Article |
fullrecord | <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_journals_1442628326</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>3101921361</sourcerecordid><originalsourceid>FETCH-LOGICAL-c295t-da4e2ba6d6fa6d82607a1f2cc99bd09123a7e13ae3fe19e8a5bd30ebf995a4933</originalsourceid><addsrcrecordid>eNqNkNtKxDAQhoMH8PgOAcG7dnNqmtyIa_EEiiJ6HdJ2qpG2WZOui29vdAW99GZmIMP3Tz6EjinJBWFqtlqt8tg4GCfXuSYfYZrNb29zqnROJdtAu1RKlpVCsU10qEvFCS9VIQottr7fSKY5lztoL8ZXQqSgQu2i-gEi2NC8YD_i--AXECYHEV8Pi-DfYUhp2He48sPCRzcBnvfLwY3LIQ29_8AX3vX4zEZovwCV79vswfe9G59x1du2TcMB2u5sH-Hwp--jp4vzx-oqu7m7vK7mN1nDdDFlrRXAaitb2aWimCSlpR1rGq3rlmjKuC2Bcgu8A6pB2aJuOYG607qwIn1tHx2tuenytyXEybz6ZRhTpKFCMMkUZzJtnay3muBjDNCZRXCDDR-GEvPl2STP5tezSZ5N8mySZ5M8J8DpGjAFO8YJmpc_Of9DfAIPLI4e</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1442628326</pqid></control><display><type>article</type><title>Research on Properties Improvement of Composite Aluminum Alloy Foil Based on Cold-Rolling Cladding</title><source>Scientific.net Journals</source><creator>Tai, Qian</creator><creatorcontrib>Tai, Qian</creatorcontrib><description>The cold-rolling cladding process of composite aluminum alloy foil for automobile heat exchanger was investigated, as well as the effects of percentage reduction of first pass, clad sheet thickness and final annealing schedule on the microstructure and properties of the foil. The results showed that bonding the clad sheets A4045 to the core material A3003 on both sides succeeds initially when the percentage reduction is 30%~50% of first pass during cold rolling, and the thickness of both the clad sheets of the composite foil are basically the same. The best sagging resistance is available when the percentage reduction of final pass is 25%~35%. The annealing temperature should be controlled in the range from 320 to 400°C before finish rolling, and the annealing time should control within 80 minutes when annealed at 400°C.</description><identifier>ISSN: 1660-9336</identifier><identifier>ISSN: 1662-7482</identifier><identifier>ISBN: 9783037854594</identifier><identifier>ISBN: 3037854596</identifier><identifier>EISSN: 1662-7482</identifier><identifier>DOI: 10.4028/www.scientific.net/AMM.189.162</identifier><language>eng</language><publisher>Zurich: Trans Tech Publications Ltd</publisher><ispartof>Applied Mechanics and Materials, 2012-07, Vol.189, p.162-166</ispartof><rights>2012 Trans Tech Publications Ltd</rights><rights>Copyright Trans Tech Publications Ltd. Jul 2012</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><cites>FETCH-LOGICAL-c295t-da4e2ba6d6fa6d82607a1f2cc99bd09123a7e13ae3fe19e8a5bd30ebf995a4933</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Uhttps://www.scientific.net/Image/TitleCover/1918?width=600</thumbnail><link.rule.ids>314,776,780,27901,27902</link.rule.ids></links><search><creatorcontrib>Tai, Qian</creatorcontrib><title>Research on Properties Improvement of Composite Aluminum Alloy Foil Based on Cold-Rolling Cladding</title><title>Applied Mechanics and Materials</title><description>The cold-rolling cladding process of composite aluminum alloy foil for automobile heat exchanger was investigated, as well as the effects of percentage reduction of first pass, clad sheet thickness and final annealing schedule on the microstructure and properties of the foil. The results showed that bonding the clad sheets A4045 to the core material A3003 on both sides succeeds initially when the percentage reduction is 30%~50% of first pass during cold rolling, and the thickness of both the clad sheets of the composite foil are basically the same. The best sagging resistance is available when the percentage reduction of final pass is 25%~35%. The annealing temperature should be controlled in the range from 320 to 400°C before finish rolling, and the annealing time should control within 80 minutes when annealed at 400°C.</description><issn>1660-9336</issn><issn>1662-7482</issn><issn>1662-7482</issn><isbn>9783037854594</isbn><isbn>3037854596</isbn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2012</creationdate><recordtype>article</recordtype><sourceid>BENPR</sourceid><recordid>eNqNkNtKxDAQhoMH8PgOAcG7dnNqmtyIa_EEiiJ6HdJ2qpG2WZOui29vdAW99GZmIMP3Tz6EjinJBWFqtlqt8tg4GCfXuSYfYZrNb29zqnROJdtAu1RKlpVCsU10qEvFCS9VIQottr7fSKY5lztoL8ZXQqSgQu2i-gEi2NC8YD_i--AXECYHEV8Pi-DfYUhp2He48sPCRzcBnvfLwY3LIQ29_8AX3vX4zEZovwCV79vswfe9G59x1du2TcMB2u5sH-Hwp--jp4vzx-oqu7m7vK7mN1nDdDFlrRXAaitb2aWimCSlpR1rGq3rlmjKuC2Bcgu8A6pB2aJuOYG607qwIn1tHx2tuenytyXEybz6ZRhTpKFCMMkUZzJtnay3muBjDNCZRXCDDR-GEvPl2STP5tezSZ5N8mySZ5M8J8DpGjAFO8YJmpc_Of9DfAIPLI4e</recordid><startdate>20120701</startdate><enddate>20120701</enddate><creator>Tai, Qian</creator><general>Trans Tech Publications Ltd</general><scope>AAYXX</scope><scope>CITATION</scope><scope>7SR</scope><scope>7TB</scope><scope>8BQ</scope><scope>8FD</scope><scope>8FE</scope><scope>8FG</scope><scope>ABJCF</scope><scope>ABUWG</scope><scope>AFKRA</scope><scope>BENPR</scope><scope>BFMQW</scope><scope>BGLVJ</scope><scope>CCPQU</scope><scope>D1I</scope><scope>DWQXO</scope><scope>FR3</scope><scope>HCIFZ</scope><scope>JG9</scope><scope>KB.</scope><scope>KR7</scope><scope>L6V</scope><scope>M7S</scope><scope>PDBOC</scope><scope>PQEST</scope><scope>PQQKQ</scope><scope>PQUKI</scope><scope>PRINS</scope><scope>PTHSS</scope></search><sort><creationdate>20120701</creationdate><title>Research on Properties Improvement of Composite Aluminum Alloy Foil Based on Cold-Rolling Cladding</title><author>Tai, Qian</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c295t-da4e2ba6d6fa6d82607a1f2cc99bd09123a7e13ae3fe19e8a5bd30ebf995a4933</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2012</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Tai, Qian</creatorcontrib><collection>CrossRef</collection><collection>Engineered Materials Abstracts</collection><collection>Mechanical & Transportation Engineering Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>ProQuest SciTech Collection</collection><collection>ProQuest Technology Collection</collection><collection>Materials Science & Engineering Collection</collection><collection>ProQuest Central (Alumni Edition)</collection><collection>ProQuest Central UK/Ireland</collection><collection>ProQuest Central</collection><collection>Continental Europe Database</collection><collection>Technology Collection</collection><collection>ProQuest One Community College</collection><collection>ProQuest Materials Science Collection</collection><collection>ProQuest Central Korea</collection><collection>Engineering Research Database</collection><collection>SciTech Premium Collection</collection><collection>Materials Research Database</collection><collection>Materials Science Database</collection><collection>Civil Engineering Abstracts</collection><collection>ProQuest Engineering Collection</collection><collection>Engineering Database</collection><collection>Materials Science Collection</collection><collection>ProQuest One Academic Eastern Edition (DO NOT USE)</collection><collection>ProQuest One Academic</collection><collection>ProQuest One Academic UKI Edition</collection><collection>ProQuest Central China</collection><collection>Engineering Collection</collection><jtitle>Applied Mechanics and Materials</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Tai, Qian</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Research on Properties Improvement of Composite Aluminum Alloy Foil Based on Cold-Rolling Cladding</atitle><jtitle>Applied Mechanics and Materials</jtitle><date>2012-07-01</date><risdate>2012</risdate><volume>189</volume><spage>162</spage><epage>166</epage><pages>162-166</pages><issn>1660-9336</issn><issn>1662-7482</issn><eissn>1662-7482</eissn><isbn>9783037854594</isbn><isbn>3037854596</isbn><abstract>The cold-rolling cladding process of composite aluminum alloy foil for automobile heat exchanger was investigated, as well as the effects of percentage reduction of first pass, clad sheet thickness and final annealing schedule on the microstructure and properties of the foil. The results showed that bonding the clad sheets A4045 to the core material A3003 on both sides succeeds initially when the percentage reduction is 30%~50% of first pass during cold rolling, and the thickness of both the clad sheets of the composite foil are basically the same. The best sagging resistance is available when the percentage reduction of final pass is 25%~35%. The annealing temperature should be controlled in the range from 320 to 400°C before finish rolling, and the annealing time should control within 80 minutes when annealed at 400°C.</abstract><cop>Zurich</cop><pub>Trans Tech Publications Ltd</pub><doi>10.4028/www.scientific.net/AMM.189.162</doi><tpages>5</tpages></addata></record> |
fulltext | fulltext |
identifier | ISSN: 1660-9336 |
ispartof | Applied Mechanics and Materials, 2012-07, Vol.189, p.162-166 |
issn | 1660-9336 1662-7482 1662-7482 |
language | eng |
recordid | cdi_proquest_journals_1442628326 |
source | Scientific.net Journals |
title | Research on Properties Improvement of Composite Aluminum Alloy Foil Based on Cold-Rolling Cladding |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-12T16%3A46%3A20IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Research%20on%20Properties%20Improvement%20of%20Composite%20Aluminum%20Alloy%20Foil%20Based%20on%20Cold-Rolling%20Cladding&rft.jtitle=Applied%20Mechanics%20and%20Materials&rft.au=Tai,%20Qian&rft.date=2012-07-01&rft.volume=189&rft.spage=162&rft.epage=166&rft.pages=162-166&rft.issn=1660-9336&rft.eissn=1662-7482&rft.isbn=9783037854594&rft.isbn_list=3037854596&rft_id=info:doi/10.4028/www.scientific.net/AMM.189.162&rft_dat=%3Cproquest_cross%3E3101921361%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=1442628326&rft_id=info:pmid/&rfr_iscdi=true |