High-Temperature Mechanical Behavior of Extruded Mg-Y-Zn Alloy Containing LPSO Phases

The high-temperature mechanical behavior of extruded Mg 97−3 x Y 2 x Zn x (at. pct) alloys is evaluated from 473 K to 673 K (200 °C to 400 °C). The microstructure of the extruded alloys is characterized by Long Period Stacking Ordered structure (LPSO) elongated particles within the magnesium matrix....

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Metallurgical and materials transactions. A, Physical metallurgy and materials science Physical metallurgy and materials science, 2013-06, Vol.44 (6), p.2869-2883
Hauptverfasser: Oñorbe, Elvira, Garcés, Gerardo, Dobes, Ferdinand, Pérez, Pablo, Adeva, Paloma
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The high-temperature mechanical behavior of extruded Mg 97−3 x Y 2 x Zn x (at. pct) alloys is evaluated from 473 K to 673 K (200 °C to 400 °C). The microstructure of the extruded alloys is characterized by Long Period Stacking Ordered structure (LPSO) elongated particles within the magnesium matrix. At low temperature and high strain rates, their creep behavior shows a high stress exponent ( n  = 11) and high activation energy. Alloys behave as a metal matrix composite where the magnesium matrix transfers part of its load to the LPSO phase. At high-temperature and/or low stresses, creep is controlled by nonbasal dislocation slip. At intermediate and high strain rates at 673 K (400 °C) and at intermediate strain rates between 623 K and 673 K (350 °C and 400 °C), the extruded alloys show superplastic deformation with elongations to failure higher than 200 pct. Cracking of coarse LPSO second-phase particles and their subsequent distribution in the magnesium matrix take place during superplastic deformation, preventing magnesium grain growth.
ISSN:1073-5623
1543-1940
DOI:10.1007/s11661-013-1628-8