Head-Disk Interface Materials Issues in Heat-Assisted Magnetic Recording

In this paper, some issues concerning the reliability of heat-assisted magnetic recording (HAMR) media are highlighted. The large roughness of the grain structure originates from a surface energy mismatch between the FePt grains and the graphene-like segregant material. A simple roughness model, bas...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:IEEE transactions on magnetics 2014-03, Vol.50 (3), p.137-143
Hauptverfasser: Marchon, Bruno, Xing-Cai Guo, Pathem, Bala Krishna, Rose, Franck, Qing Dai, Feliss, Norbert, Schreck, Erhard, Reiner, James, Mosendz, Oleksandr, Takano, Kentaro, Hoa Do, Burns, John, Saito, Yoko
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:In this paper, some issues concerning the reliability of heat-assisted magnetic recording (HAMR) media are highlighted. The large roughness of the grain structure originates from a surface energy mismatch between the FePt grains and the graphene-like segregant material. A simple roughness model, based on interfacial energies, is proposed that can quantitatively predict media grain structure and roughness. The thermal behavior of the disk lubricant is reviewed both experimentally as well as theoretically using molecular dynamics (MD) and density functional theory (DFT). The lubricant film can be subjected to evaporation and oxidation, both of which follow an Arrhenius reaction rate. MD also predicts that the disk carbon overcoat can undergo structural changes under thermal transient exposure in the nanosecond time frame, and Raman imaging performed on a disk zone that was HAMR written shows small but unequivocal changes, consistent with an increase in carbon sp 2 cluster size.
ISSN:0018-9464
1941-0069
DOI:10.1109/TMAG.2013.2283068