Improving tensile properties of dilute Mg-0.27Al-0.13Ca-0.21Mn (at.%) alloy by low temperature high speed extrusion

As-cast Mg-0.27Al-0.13Ca-0.21Mn (at.%) alloy was extruded at temperatures from 350 °C to 500 °C. We examined the microstructural changes during extrusion at different temperatures to clarify dynamic recrystallization mechanisms during extrusion, and also investigated the effect of extrusion temperat...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of alloys and compounds 2015-11, Vol.648 (C), p.428-437
Hauptverfasser: Nakata, T., Mezaki, T., Xu, C., Oh-ishi, K., Shimizu, K., Hanaki, S., Kamado, S.