Seeded Stage III glass dissolution behavior of a statistically designed glass matrix

The glass dissolution rate of some glasses accelerates after prolonged time spent at a slow, residual glass dissolution rate. This phenomenon is referred to as Stage III behavior. Here, the acceleration in glass dissolution rate linked to Stage III behavior is significant and may be the most impactf...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of the American Ceramic Society 2021-03, Vol.104 (8)
Hauptverfasser: Crum, Jarrod V., Reiser, Joelle T. G., Parruzot, Benjamin P., Neeway, James J., Bonnett, Jeff F., Kerisit, Sebastien N., Cooley, Scott K., Ryan, Joseph V., Smith, Gary L., Asmussen, Robert Matthew
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue 8
container_start_page
container_title Journal of the American Ceramic Society
container_volume 104
creator Crum, Jarrod V.
Reiser, Joelle T. G.
Parruzot, Benjamin P.
Neeway, James J.
Bonnett, Jeff F.
Kerisit, Sebastien N.
Cooley, Scott K.
Ryan, Joseph V.
Smith, Gary L.
Asmussen, Robert Matthew
description The glass dissolution rate of some glasses accelerates after prolonged time spent at a slow, residual glass dissolution rate. This phenomenon is referred to as Stage III behavior. Here, the acceleration in glass dissolution rate linked to Stage III behavior is significant and may be the most impactful to long-term performance of glass in a repository. This work is aimed at understanding the effect of glass composition on Stage III behavior to add a level of technical defensibility to glass disposal. To this end, a set of twenty-four glass compositions were statistically designed, where eight glass components (SiO2, B2O3, Al2O3, CaO, Na2O, SnO2, ZrO2, and Others) have been independently varied in order to study the individual effects of each. These glasses have been subjected to static dissolution tests at 90 °C in deionized water and then seeded with zeolite Na-P2 28 days into the testing to induce Stage III behavior. The response of the glasses to the zeolite seeds fell into four primary types: 1) no response to seeds; 2) an immediate linear sustained acceleration in the rate; 3) an immediate linear acceleration in the rate followed by a decrease; and, 4) a progressive acceleration in the rate that is concurrent with the addition of the seeds. The main glass components observed to influence these behaviors were CaO, Al2O3, B2O3, and ZrO2, where: 1) CaO influenced which glasses showed a Stage III response to seeds (high CaO: Types 2, 3, and 4) or did not respond to seeds (low CaO: Type 1), 2) Al2O3 and B2O3 influenced which glasses showed a sustainable Stage III response (high Al2O3: Types 2 and 4) versus transitory response (low Al2O3 and high B2O3: Type 3), and 3) ZrO2 concentration influenced whether glasses showed a linear (high ZrO2: Type 2) versus progressive (low ZrO2: Type 4) response to seeds.
format Article
fullrecord <record><control><sourceid>osti</sourceid><recordid>TN_cdi_osti_scitechconnect_1787838</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>1787838</sourcerecordid><originalsourceid>FETCH-osti_scitechconnect_17878383</originalsourceid><addsrcrecordid>eNqNjMsKwjAQRYMoWB__MLgvJK216VoUu273JSbTNhIb6ETRv7egH-DqcuCcO2ORyDIRJ4U4zFnEOU_iXCZ8yVZEtwlFIfcRqytEgwaqoDqEsiyhc4oIjCXy7hGsH-CKvXpaP4JvQQEFFSwFq5VzbzBIthumg292V2G0rw1btMoRbn-7ZrvzqT5eYj91DWkbUPfaDwPq0Ihc5jKV6V_SB_APQco</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Seeded Stage III glass dissolution behavior of a statistically designed glass matrix</title><source>Wiley-Blackwell Journals</source><creator>Crum, Jarrod V. ; Reiser, Joelle T. G. ; Parruzot, Benjamin P. ; Neeway, James J. ; Bonnett, Jeff F. ; Kerisit, Sebastien N. ; Cooley, Scott K. ; Ryan, Joseph V. ; Smith, Gary L. ; Asmussen, Robert Matthew</creator><creatorcontrib>Crum, Jarrod V. ; Reiser, Joelle T. G. ; Parruzot, Benjamin P. ; Neeway, James J. ; Bonnett, Jeff F. ; Kerisit, Sebastien N. ; Cooley, Scott K. ; Ryan, Joseph V. ; Smith, Gary L. ; Asmussen, Robert Matthew ; Pacific Northwest National Lab. (PNNL), Richland, WA (United States)</creatorcontrib><description>The glass dissolution rate of some glasses accelerates after prolonged time spent at a slow, residual glass dissolution rate. This phenomenon is referred to as Stage III behavior. Here, the acceleration in glass dissolution rate linked to Stage III behavior is significant and may be the most impactful to long-term performance of glass in a repository. This work is aimed at understanding the effect of glass composition on Stage III behavior to add a level of technical defensibility to glass disposal. To this end, a set of twenty-four glass compositions were statistically designed, where eight glass components (SiO2, B2O3, Al2O3, CaO, Na2O, SnO2, ZrO2, and Others) have been independently varied in order to study the individual effects of each. These glasses have been subjected to static dissolution tests at 90 °C in deionized water and then seeded with zeolite Na-P2 28 days into the testing to induce Stage III behavior. The response of the glasses to the zeolite seeds fell into four primary types: 1) no response to seeds; 2) an immediate linear sustained acceleration in the rate; 3) an immediate linear acceleration in the rate followed by a decrease; and, 4) a progressive acceleration in the rate that is concurrent with the addition of the seeds. The main glass components observed to influence these behaviors were CaO, Al2O3, B2O3, and ZrO2, where: 1) CaO influenced which glasses showed a Stage III response to seeds (high CaO: Types 2, 3, and 4) or did not respond to seeds (low CaO: Type 1), 2) Al2O3 and B2O3 influenced which glasses showed a sustainable Stage III response (high Al2O3: Types 2 and 4) versus transitory response (low Al2O3 and high B2O3: Type 3), and 3) ZrO2 concentration influenced whether glasses showed a linear (high ZrO2: Type 2) versus progressive (low ZrO2: Type 4) response to seeds.</description><identifier>ISSN: 0002-7820</identifier><identifier>EISSN: 1551-2916</identifier><language>eng</language><publisher>United States: American Ceramic Society</publisher><subject>MATERIALS SCIENCE</subject><ispartof>Journal of the American Ceramic Society, 2021-03, Vol.104 (8)</ispartof><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><orcidid>0000000228416660 ; 0000000159777728 ; 0000000274709181 ; 0000000226381580 ; 000000022549660X ; 0000000170468408 ; 0000000191970878</orcidid></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>230,314,780,784,885</link.rule.ids><backlink>$$Uhttps://www.osti.gov/servlets/purl/1787838$$D View this record in Osti.gov$$Hfree_for_read</backlink></links><search><creatorcontrib>Crum, Jarrod V.</creatorcontrib><creatorcontrib>Reiser, Joelle T. G.</creatorcontrib><creatorcontrib>Parruzot, Benjamin P.</creatorcontrib><creatorcontrib>Neeway, James J.</creatorcontrib><creatorcontrib>Bonnett, Jeff F.</creatorcontrib><creatorcontrib>Kerisit, Sebastien N.</creatorcontrib><creatorcontrib>Cooley, Scott K.</creatorcontrib><creatorcontrib>Ryan, Joseph V.</creatorcontrib><creatorcontrib>Smith, Gary L.</creatorcontrib><creatorcontrib>Asmussen, Robert Matthew</creatorcontrib><creatorcontrib>Pacific Northwest National Lab. (PNNL), Richland, WA (United States)</creatorcontrib><title>Seeded Stage III glass dissolution behavior of a statistically designed glass matrix</title><title>Journal of the American Ceramic Society</title><description>The glass dissolution rate of some glasses accelerates after prolonged time spent at a slow, residual glass dissolution rate. This phenomenon is referred to as Stage III behavior. Here, the acceleration in glass dissolution rate linked to Stage III behavior is significant and may be the most impactful to long-term performance of glass in a repository. This work is aimed at understanding the effect of glass composition on Stage III behavior to add a level of technical defensibility to glass disposal. To this end, a set of twenty-four glass compositions were statistically designed, where eight glass components (SiO2, B2O3, Al2O3, CaO, Na2O, SnO2, ZrO2, and Others) have been independently varied in order to study the individual effects of each. These glasses have been subjected to static dissolution tests at 90 °C in deionized water and then seeded with zeolite Na-P2 28 days into the testing to induce Stage III behavior. The response of the glasses to the zeolite seeds fell into four primary types: 1) no response to seeds; 2) an immediate linear sustained acceleration in the rate; 3) an immediate linear acceleration in the rate followed by a decrease; and, 4) a progressive acceleration in the rate that is concurrent with the addition of the seeds. The main glass components observed to influence these behaviors were CaO, Al2O3, B2O3, and ZrO2, where: 1) CaO influenced which glasses showed a Stage III response to seeds (high CaO: Types 2, 3, and 4) or did not respond to seeds (low CaO: Type 1), 2) Al2O3 and B2O3 influenced which glasses showed a sustainable Stage III response (high Al2O3: Types 2 and 4) versus transitory response (low Al2O3 and high B2O3: Type 3), and 3) ZrO2 concentration influenced whether glasses showed a linear (high ZrO2: Type 2) versus progressive (low ZrO2: Type 4) response to seeds.</description><subject>MATERIALS SCIENCE</subject><issn>0002-7820</issn><issn>1551-2916</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2021</creationdate><recordtype>article</recordtype><recordid>eNqNjMsKwjAQRYMoWB__MLgvJK216VoUu273JSbTNhIb6ETRv7egH-DqcuCcO2ORyDIRJ4U4zFnEOU_iXCZ8yVZEtwlFIfcRqytEgwaqoDqEsiyhc4oIjCXy7hGsH-CKvXpaP4JvQQEFFSwFq5VzbzBIthumg292V2G0rw1btMoRbn-7ZrvzqT5eYj91DWkbUPfaDwPq0Ihc5jKV6V_SB_APQco</recordid><startdate>20210329</startdate><enddate>20210329</enddate><creator>Crum, Jarrod V.</creator><creator>Reiser, Joelle T. G.</creator><creator>Parruzot, Benjamin P.</creator><creator>Neeway, James J.</creator><creator>Bonnett, Jeff F.</creator><creator>Kerisit, Sebastien N.</creator><creator>Cooley, Scott K.</creator><creator>Ryan, Joseph V.</creator><creator>Smith, Gary L.</creator><creator>Asmussen, Robert Matthew</creator><general>American Ceramic Society</general><scope>OIOZB</scope><scope>OTOTI</scope><orcidid>https://orcid.org/0000000228416660</orcidid><orcidid>https://orcid.org/0000000159777728</orcidid><orcidid>https://orcid.org/0000000274709181</orcidid><orcidid>https://orcid.org/0000000226381580</orcidid><orcidid>https://orcid.org/000000022549660X</orcidid><orcidid>https://orcid.org/0000000170468408</orcidid><orcidid>https://orcid.org/0000000191970878</orcidid></search><sort><creationdate>20210329</creationdate><title>Seeded Stage III glass dissolution behavior of a statistically designed glass matrix</title><author>Crum, Jarrod V. ; Reiser, Joelle T. G. ; Parruzot, Benjamin P. ; Neeway, James J. ; Bonnett, Jeff F. ; Kerisit, Sebastien N. ; Cooley, Scott K. ; Ryan, Joseph V. ; Smith, Gary L. ; Asmussen, Robert Matthew</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-osti_scitechconnect_17878383</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2021</creationdate><topic>MATERIALS SCIENCE</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Crum, Jarrod V.</creatorcontrib><creatorcontrib>Reiser, Joelle T. G.</creatorcontrib><creatorcontrib>Parruzot, Benjamin P.</creatorcontrib><creatorcontrib>Neeway, James J.</creatorcontrib><creatorcontrib>Bonnett, Jeff F.</creatorcontrib><creatorcontrib>Kerisit, Sebastien N.</creatorcontrib><creatorcontrib>Cooley, Scott K.</creatorcontrib><creatorcontrib>Ryan, Joseph V.</creatorcontrib><creatorcontrib>Smith, Gary L.</creatorcontrib><creatorcontrib>Asmussen, Robert Matthew</creatorcontrib><creatorcontrib>Pacific Northwest National Lab. (PNNL), Richland, WA (United States)</creatorcontrib><collection>OSTI.GOV - Hybrid</collection><collection>OSTI.GOV</collection><jtitle>Journal of the American Ceramic Society</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Crum, Jarrod V.</au><au>Reiser, Joelle T. G.</au><au>Parruzot, Benjamin P.</au><au>Neeway, James J.</au><au>Bonnett, Jeff F.</au><au>Kerisit, Sebastien N.</au><au>Cooley, Scott K.</au><au>Ryan, Joseph V.</au><au>Smith, Gary L.</au><au>Asmussen, Robert Matthew</au><aucorp>Pacific Northwest National Lab. (PNNL), Richland, WA (United States)</aucorp><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Seeded Stage III glass dissolution behavior of a statistically designed glass matrix</atitle><jtitle>Journal of the American Ceramic Society</jtitle><date>2021-03-29</date><risdate>2021</risdate><volume>104</volume><issue>8</issue><issn>0002-7820</issn><eissn>1551-2916</eissn><abstract>The glass dissolution rate of some glasses accelerates after prolonged time spent at a slow, residual glass dissolution rate. This phenomenon is referred to as Stage III behavior. Here, the acceleration in glass dissolution rate linked to Stage III behavior is significant and may be the most impactful to long-term performance of glass in a repository. This work is aimed at understanding the effect of glass composition on Stage III behavior to add a level of technical defensibility to glass disposal. To this end, a set of twenty-four glass compositions were statistically designed, where eight glass components (SiO2, B2O3, Al2O3, CaO, Na2O, SnO2, ZrO2, and Others) have been independently varied in order to study the individual effects of each. These glasses have been subjected to static dissolution tests at 90 °C in deionized water and then seeded with zeolite Na-P2 28 days into the testing to induce Stage III behavior. The response of the glasses to the zeolite seeds fell into four primary types: 1) no response to seeds; 2) an immediate linear sustained acceleration in the rate; 3) an immediate linear acceleration in the rate followed by a decrease; and, 4) a progressive acceleration in the rate that is concurrent with the addition of the seeds. The main glass components observed to influence these behaviors were CaO, Al2O3, B2O3, and ZrO2, where: 1) CaO influenced which glasses showed a Stage III response to seeds (high CaO: Types 2, 3, and 4) or did not respond to seeds (low CaO: Type 1), 2) Al2O3 and B2O3 influenced which glasses showed a sustainable Stage III response (high Al2O3: Types 2 and 4) versus transitory response (low Al2O3 and high B2O3: Type 3), and 3) ZrO2 concentration influenced whether glasses showed a linear (high ZrO2: Type 2) versus progressive (low ZrO2: Type 4) response to seeds.</abstract><cop>United States</cop><pub>American Ceramic Society</pub><orcidid>https://orcid.org/0000000228416660</orcidid><orcidid>https://orcid.org/0000000159777728</orcidid><orcidid>https://orcid.org/0000000274709181</orcidid><orcidid>https://orcid.org/0000000226381580</orcidid><orcidid>https://orcid.org/000000022549660X</orcidid><orcidid>https://orcid.org/0000000170468408</orcidid><orcidid>https://orcid.org/0000000191970878</orcidid><oa>free_for_read</oa></addata></record>
fulltext fulltext
identifier ISSN: 0002-7820
ispartof Journal of the American Ceramic Society, 2021-03, Vol.104 (8)
issn 0002-7820
1551-2916
language eng
recordid cdi_osti_scitechconnect_1787838
source Wiley-Blackwell Journals
subjects MATERIALS SCIENCE
title Seeded Stage III glass dissolution behavior of a statistically designed glass matrix
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-10T13%3A59%3A39IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-osti&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Seeded%20Stage%20III%20glass%20dissolution%20behavior%20of%20a%20statistically%20designed%20glass%20matrix&rft.jtitle=Journal%20of%20the%20American%20Ceramic%20Society&rft.au=Crum,%20Jarrod%20V.&rft.aucorp=Pacific%20Northwest%20National%20Lab.%20(PNNL),%20Richland,%20WA%20(United%20States)&rft.date=2021-03-29&rft.volume=104&rft.issue=8&rft.issn=0002-7820&rft.eissn=1551-2916&rft_id=info:doi/&rft_dat=%3Costi%3E1787838%3C/osti%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true